Comparative investigation of microstructure and crystallographic texture effect on Ti6Al4V alloy mechanical properties
Source abstract
Abstract
Abstract In the present work, the effect of microstructure and crystallographic texture on the mechanical properties of Ti6Al4V alloy was investigated. A rolled plate of Ti6Al4V was heat-treated to produce three different typical microstructures including equiaxed, bimodal, and fully lamellar microstructures. The results showed that the samples with equiaxed and fully lamellar microstructure have relatively strong α texture due to the presence of the α phase with an individual morphology. The main texture of equiaxed microstructure was [ 0001 ] ∥ ND with a maximum intensity of 1.42 multiples of random distribution (mrd). By contrast, the presence of two morphological features of the α phase in the sample of bimodal microstructure caused a decrease in texture intensity where the main texture was [ 10 1 ‾ 4 ] ∥ ND with a maximum intensity of 1.15 mrd. The hardness measurement showed that the equiaxed microstructure had the lowest hardness values ranging from 324 HV to 366 HV whereas the greatest hardness value was approximately equal to 400 HV obtained in samples with fully lamellar microstructure. Furthermore, the results showed that the α grain size has a greater effect on hardness values rather than texture. The hardness of equiaxed sample increased from 324 HV (for RD-TD plane with an average α grain size of 10.7 μm) to 366 HV (for RD-ND plane with an average α grain size of 9.6 μm). The hardness measurement of sample with bimodal microstructure revealed that the presence of [ 11 2 ‾ 0 ] ∥ TD led to higher hardness (398 HV) than that of [ 10 1 ‾ 0 ] ∥ RD texture (373 HV).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Microstructure and properties of Ti-Al coating and Ti-Al-Si system coatings on Ti-6Al-4V fabricated by laser surface alloying10.1016/j.surfcoat.2016.10.082 ↗
2. Donachie
3. Optimization of the electrophoretic deposition parameters for biocomposite hydroxyapatite/chitosan/collagen/h-BN coatings on Ti6Al4V biomedical implants10.1007/s11661-018-5010-8 ↗
4. Bi-lamellar microstructure in Ti–6Al–4V: microstructure evolution and mechanical properties10.1016/j.msea.2019.138077 ↗
5. Tracking microstructure, texture and boundary misorientation evolution of hot deformed and post-deformation annealed Ti-6Al-4V alloy10.1016/j.msea.2015.09.060 ↗
6. Dry sliding wear behaviour of Ti-6Al-4V alloy consisting of bimodal microstructure10.1007/s12666-013-0343-x ↗
7. Effect of different heat treatments on microstructure and mechanical properties of Ti6Al4V titanium alloy10.1016/S1875-5372(17)30109-1 ↗
8. Microstructure and corrosion behaviour of additively manufactured Ti–6Al–4V with various post-heat treatments10.1080/02670836.2018.1542052 ↗
9. Study of the electrochemical behavior of a Ti6Al4V alloy modified by heat treatments and chemical conversion10.1016/j.surfcoat.2017.01.036 ↗
10. The influence of temperature during water-quench rapid heat treatment on the microstructure, mechanical properties and biocompatibility of Ti6Al4V ELI alloy10.1016/j.jmbbm.2019.04.024 ↗
11. Ti based biomaterials, the ultimate choice for orthopaedic implants - a review10.1016/j.pmatsci.2008.06.004 ↗
12. Cytocompatibility of Cu-bearing Ti6Al4V alloys manufactured by selective laser melting10.1016/j.matchar.2017.12.003 ↗
13. Enhanced mechanical response of an ultrafine grained Ti-6Al-4V alloy produced through warm symmetric and asymmetric rolling10.1016/j.msea.2015.10.061 ↗
14. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
15. The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy10.1016/S1359-6454(03)00179-4 ↗
16. Crystallographic variant selection in Ti-6Al-4V10.1016/j.actamat.2004.07.034 ↗
17. Using heat treatments, high-pressure torsion and post-deformation annealing to optimize the properties of Ti-6Al-4V alloys10.1016/j.actamat.2017.09.018 ↗
18. A novel Ti-6Al-4V alloy microstructure with very high strength and good ductility10.1016/j.scriptamat.2015.05.008 ↗
19. Factors determining room temperature mechanical properties of bimodal microstructures in Ti-6Al-4V alloy10.1016/j.msea.2018.06.019 ↗
20. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
21. Effect of heat treatment processing on microstructure and tensile properties of Ti-6Al-4V-10Nb alloy10.1016/S1003-6326(18)64915-5 ↗
22. Froes · 2015
23. Beta to alpha transformation kinetics and microstructure of Ti-6Al-4V alloy during continuous cooling10.1016/j.matchemphys.2016.06.082 ↗
24. On the influence of the heat treatment on microstructure formation and mechanical properties of near-α Ti-Fe alloys10.1016/j.msea.2018.12.071 ↗
25. Early stages of microstructure and texture evolution during beta annealing of Ti-6Al-4V10.1007/s11661-017-4444-8 ↗
26. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
27. The effect of β grain coarsening on variant selection and texture evolution in a near-β Ti alloy10.1016/j.msea.2013.04.018 ↗
28. Evolution of microstructure during welding simulation of boron modified P91 steel10.1134/S0031918X19070056 ↗
29. Microstructures and hardness of Ti-6Al-4V alloy staging castings under centrifugal field10.1016/S1003-6326(08)60051-5 ↗
30. Effect of microstructural variation on erosion wear behavior of Ti-6Al-4V alloy10.1080/10402004.2013.767400 ↗
31. Effect of microstructural variation on dry sliding wear behavior of Ti-6Al-4V alloy10.1007/s11665-014-0987-7 ↗
32. Probing true microstructure-hardening relationship in simulated heat affected zone of P91B steels10.1007/s13632-019-00573-w ↗
33. Effect of micro shot peening on the mechanical properties and corrosion behavior of two microstructure Ti-6Al-4V alloy10.1016/j.apsusc.2015.12.019 ↗
34. Six decades of the Hall–Petch effect – a survey of grain-size strengthening studies on pure metals10.1080/09506608.2016.1191808 ↗
35. Local and global mechanical behavior and microstructure of Ti6Al4V parts built using electron beam melting technology10.1007/s11661-015-2965-6 ↗