Liquid phase surface nitriding of Ti-6Al-4V pre-placed with chromium
Source abstract
Abstract
Abstract In this study, liquid phase surface nitriding of Ti-6Al-4V was carried out by pre-placing of chromium powder on the substrate and subsequent Tungsten Inert Gas (TIG) surface melting. The effect of the application of low and high heat inputs on the microstructure, microhardness and wear resistance of the treated layers were studied. Surface alloying with chromium in a nitrogen containing atmosphere resulted in the formation of hard intermetallic compounds such as TiN, Cr 2 N and TiCr 2 . Moreover, the presence of beta stabilizer chromium together with the application of high heat input during surface treatment resulted in the presence of beta phase at room temperature. However, applying low heat input could not prevent transformation of beta to martensite. The hardness of the layers fabricated at high and low heat inputs were respectively 1050 and 1200 HV 0.3 compared to average 280 HV 0.3 for the as-received material. Liquid phase surface treatment of titanium at the aforementioned conditions improved the wear resistance. The lowest weight loss belonged to the specimen with the beta phase matrix. The formation of the fairly ductile bcc-β phase hindered crack nucleation during wear. The weight loss in this condition was 7 times lower than that of the base material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Microstructure and wear behaviours of laser-clad Cr13Ni5Si2 based metal-silicide coatings on a titanium alloy10.1016/j.surfcoat.2004.05.025 ↗
2. Surface plasma chromized burn-resistant titanium alloy10.1016/j.surfcoat.2006.07.078 ↗
3. Laser nitriding of titanium alloy in the atmosphere environment10.1016/j.surfcoat.2006.07.186 ↗
4. Fatigue behavior of plasma surface modified Ti–6Al–4V alloy10.1016/j.vacuum.2005.01.007 ↗
5. Tribological and electrochemical performance of PVD TiN coatings on the femoral head of Ti–6Al–4V artificial hip joints10.1016/S0257-8972(02)00630-8 ↗
6. Niche sectors for economically competitive ion implantation treatments10.1016/S0257-8972(02)00211-6 ↗
7. Tribological behavior of plasma Mo–N surface modified Ti–6Al–4V alloy10.1016/S0257-8972(03)00855-7 ↗
8. Enhancing the microstructure and properties of titanium alloys through nitriding and other surface engineering methods10.1016/j.surfcoat.2004.07.115 ↗
9. Microstructure, mechanical and wear properties of laser processed SiC particle reinforced coatings on titanium10.1016/j.surfcoat.2011.03.027 ↗
10. In situ synthesis of TiN/Ti3Al intermetallic matrix composite coatings on Ti6Al4V alloy10.1016/j.matdes.2011.12.008 ↗
11. Correlation of microstructure with hardness and fracture properties of (TiC, SiC)/Ti–6Al–4V surface composites fabricated by high-energy electron-beam irradiation
12. Microstructure and wear assessment of TIG surface alloying of CP-titanium with silicon10.1007/s10853-008-2890-9 ↗
13. Characterization of Ti–6Al–4V alloy modified by plasma carburizing process
14. Microstructural characterization and failure mechanism of vacuum plasma sprayed Ti-6Al-4V/B4C composite10.1016/j.vacuum.2014.03.028 ↗
15. Titanium nitride layer formation by TIG surface melting in a reactive environment10.1016/j.jmatprotec.2005.02.247 ↗
16. Wang · 2007
17. In-situ synthesis and wear performance of TiC particle reinforced composite coating on alloy Ti6Al4V10.1016/S0257-8972(00)01133-6 ↗
18. Leyens · 2003
19. Matthew · 2000
20. Surface modification of Ti–6Al–4V alloy using metal arc heat source10.1179/sur.1997.13.3.257 ↗
21. Wear resistance of a laser surface alloyed Ti–6Al–4V alloy10.1016/S0257-8972(00)00680-0 ↗
22. Laser powder micro-deposition of compositional gradient Ti–Cr alloy10.1016/j.matdes.2010.02.052 ↗
23. Synthesis of TiN/Ti3Al composite coatings on Ti6Al4V alloy by plasma spraying and laser nitriding10.1016/j.surfcoat.2012.07.024 ↗
24. Wear resistance of in situ synthesized titanium compound coatings produced by laser alloying technique10.1016/j.surfcoat.2014.08.012 ↗
25. Microstructure and wear resistance of one-step in-situ synthesized TiN/Al composite coatings on Ti6Al4V alloy by a laser nitriding process10.1016/j.optlastec.2014.10.007 ↗
26. Microstructural studies and wear assessments of Ti/TiC surface composite coatings on commercial pure Ti produced by titanium cored wires and TIG process10.1016/j.matchemphys.2012.11.009 ↗
27. Microstructure and wear of in-situ Ti/(TiN+ TiB) hybrid composite layers produced using liquid phase process10.1016/j.matchemphys.2014.12.026 ↗
28. Factors affecting the room-temperature mechanical properties of TiCr2 base Laves phase alloys10.1016/S0921-5093(97)00526-1 ↗