Crystallization of some modified fluor-miserite Kx(Ca,Ce)5−xSi8O22F2 glasses
Source abstract
Abstract
Abstract Fluorine-rich miserite glass compositions with variable K 2 O to CaO ratios, K x (Ca 5.5− x ,Ce 0.5 )Si 8 O 21.5 F 3 where x = 1, 2 or 3, have been investigated in term of crystallization path and Ce 3+ substitution. For sake of comparison a second series without ceria was also prepared: K x Ca 6.5− x Si 8 O 21.5 F 3 . Xonotlite, tokkoite, fluorite and cristobalite were developed in all crystallized glasses; however, miserite was only identified in Ce-containing samples. Increase of K 2 O/CaO ratio, in Ce-free sample, enhanced the formation of tokkoite, and reduced the contents of xonotlite and fluorite. On the other hand, in Ce-containing samples, an increase of K 2 O/CaO ratio promotes the formation of miserite crystals. Quantitative Rietveld analyses assessed the presence of Ce 3+ cations in miserite structure. The microstructure of Ce-free glass–ceramics was relatively coarse in the form of interlocked flakes and rods; however, it became unpronounced in the sample of highest K 2 O/CaO ratio. In Ce-containing glass-ceramics, irregular nanosized grains were spread in cryptocrystalline groundmass, whose fineness increased with increasing K 2 O/CaO ratio. The CTE values of the parent glasses and their glass–ceramics varied from 10.31 to 11.05 and from 7.52 to 9.84 × 10 −6 °C −1 respectively with lower values for Ce-free glass-ceramics. Density and micro hardness values were also measured.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Hőland · 2002
2. Chain silicate glass-ceramics10.1016/0022-3093(91)90092-K ↗
3. Effect of isomorphous substitutions on crystallization of fluorrichterite glasses10.4028/www.scientific.net/KEM.132-136.836 ↗
4. Hamzawy · 1996
5. Crystallization of Cu-containing K-fluor-richterite (KNaCa(Mg,Cu)5Si8O22F2) glasses
6. Substitution of boron for silicon in K-fluor-richterite glass ceramics
7. Crystallization of fluorcanasite–fluorrichterite glasses10.1016/j.ceramint.2007.10.002 ↗
8. Role of fluorine and phosphorous in the crystallization of K-richterite glass
9. Effect of magnesium content on the microstructure and crystalline phases of fluoramphibole glass-ceramics10.1002/1097-4636(2000)53:4<289::AID-JBM2>3.0.CO;2-E ↗
10. Effect of sodium content on the crystallisation behaviour of fluoramphibole glass-Ceramics10.1002/jbm.10085 ↗
11. Formation of apatite layers on modified canasite glass-ceramics in simulated body fluid10.1002/jbm.10018 ↗
12. Effect of fluorine content on crystallization of canasite glass–ceramics10.1007/BF00369661 ↗
13. Refinement of miserite crystal structure (K1.290.21)[Ca5.51M3+0.49](Si6(O,OH)15)(Si2O7)(F,OH)2·0.25H2O (M = Y, REE, Fe, Ti, Mn, Mg, Na) from the Dara-i-Pioz occurrence, Pamirs, Tajikistan
14. Gaines · 1997 · 1400
15. Strong sintered miserite glass-ceramics10.1111/j.1151-2916.1999.tb02114.x ↗
16. Effect of composition and heat treatment on the phase evolution and mechanical properties of tough miserite-based glass ceramics10.1016/j.jnoncrysol.2013.10.015 ↗
17. Synthesis of bioactive and machinable miserite glass-ceramics for dental implant applications10.1016/j.dental.2013.03.013 ↗
18. McMillan · 1979