More active PtRu/C catalyst for methanol electrooxidation by reversal of mixing sequence in catalyst preparation
Source abstract
Abstract
Abstract A carbon-supported PtRu/C catalyst (PtRu-2/C) was prepared by a simple reversal of the order of mixing in catalyst preparation: adding the metal precursor salts to a carbon slurry of NaBH 4 instead of adding NaBH 4 to a carbon slurry of the metal precursor salts (PtRu-1/C), as is more commonly done. The catalysts were characterized by thermogravimetric analysis, transmission electron microscopy and X-ray photoelectron spectroscopy. Evaluation of catalytic activities by cyclic voltammetry, CO stripping voltammetry, and chronoamperometry showed that PtRu-2/C had higher specific mass activity and greater CO tolerance in room temperature methanol electrooxidation reaction. Electrochemical impedance spectroscopy also confirmed that the impedance arising from CO adsorption was lower in the case of PtRu-2/C. The enhanced operational performance of PtRu-2/C is attributed to the presence of mixed active phases although the exact composition of the mixed phases has yet to be determined.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · CO2 Reduction Techniques and Catalysts
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Wasmus · J. Electroanal. Chem. · 1999 · 461 · 1410.1016/S0022-0728(98)00197-1 ↗
2. Rao · Coord. Chem. Rev. · 2005 · 249 · 61310.1016/j.ccr.2004.08.015 ↗
3. Zhang · Chem. Mater. · 2003 · 15 · 45110.1021/cm0203868 ↗
4. Deivaraj · J. Power Sources · 2005 · 142 · 4310.1016/j.jpowsour.2004.10.010 ↗
5. Park · J. Phys. Chem. B · 2004 · 108 · 93910.1021/jp0368031 ↗
6. Takasu · Electrochim. Acta · 2003 · 48 · 386110.1016/S0013-4686(03)00521-8 ↗
7. Park · J. Catal. · 2004 · 224 · 23610.1016/j.jcat.2004.02.010 ↗
8. Park · J. Phy. Chem. B · 2004 · 108 · 598910.1021/jp037458i ↗
9. Zeng · J. Power Sources · 2006 · 159 · 50910.1016/j.jpowsour.2005.11.049 ↗
10. Leng · J. Electroanal. Chem. · 2002 · 528 · 14510.1016/S0022-0728(02)00916-6 ↗
11. Chan · J. Mater. Chem. · 2004 · 14 · 50510.1039/b314224h ↗
12. Deivaraj · J. Mater. Chem. · 2003 · 13 · 255510.1039/b307040a ↗
13. Arico · J. Power Sources · 1995 · 55 · 15910.1016/0378-7753(94)02178-6 ↗
14. Lee · J. Electrochem. Soc. · 2002 · 149 · A129910.1149/1.1502685 ↗
15. Gurau · J. Phys. Chem. B · 1998 · 102 · 999710.1021/jp982887f ↗
16. Castro Luna · Electrochem. Commun. · 2000 · 2 · 22210.1016/S1388-2481(00)00011-4 ↗
17. Chu · J. Electrochem. Soc. · 1996 · 143 · 168510.1149/1.1836700 ↗
18. Zeng · J. Power Sources · 2004 · 140 · 26810.1016/j.jpowsour.2004.08.022 ↗
19. Venkataraman · J. Electrochem. Soc. · 2003 · 150 · A27810.1149/1.1543567 ↗
20. Xiong · Electrochim. Acta · 2004 · 49 · 416310.1016/j.electacta.2004.04.011 ↗
21. Rolison · Science · 2003 · 299 · 169810.1126/science.1082332 ↗
22. Rolison · Langmuir · 1999 · 15 · 77410.1021/la9807863 ↗
23. Chen · Electrochem. Commun. · 2005 · 7 · 59310.1016/j.elecom.2005.04.002 ↗
24. Long · J. Phys. Chem. B · 2000 · 104 · 977210.1021/jp001954e ↗