Abstract

Abstract The oxidation resistance of Ti-50Al intermetallics has been improved by pre-oxidizing at 800°C×48 h in air and subsequently polishing the outer TiO 2 layer of the oxide scale. The cyclic oxidation resistance’s at 800°C of the per-oxidized and polished specimens are substantially improved and the oxidation kinetics follow the parabolic rate law. This means that the outermost alumina-rich layer of the pre-oxidized and polished specimens is protective against oxidation at 800°C in air. This characteristic is attributed to the compressive stress relief associated with the removal of the outer TiO 2 layer. The stress relief will alleviate cracking or rupture of the scales and simultaneously reduce the stress-assisted diffusion in the scale. At the same time, the catalytic effect of outer rutile titania may also play a detrimental role in the oxidation resistance of TiAl at high temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Kim · JOM · 1989 · 41 · 3010.1007/BF03220267 ↗
2. Beddoes · Mater. Manufacturing Process. · 1992 · 7 · 52710.1080/10426919208947440 ↗
3. Huang · Metall. Trans. A · 1991 · 22A · 42710.1007/BF02656810 ↗
4. Huang · Acta Metall. Mater. · 1991 · 39 · 105310.1016/0956-7151(91)90192-4 ↗
5. Kim · JOM · 1994 · 46 · 3010.1007/BF03220745 ↗
6. Taniguchi · Mater. Sci. Eng. · 1989 · A120 · 51910.1016/0921-5093(89)90809-5 ↗
7. Kobayashi · High Temp. Tech. · 1990 · 8 · 17910.1080/02619180.1990.11753477 ↗
8. Anada · Mater. Trans. JIM · 1995 · 36 · 55310.2320/matertrans1989.36.533 ↗
9. Shida · Mater. Trans. JIM · 1993 · 34 · 23610.2320/matertrans1989.34.236 ↗
10. Rakowski · Script Met. et Mater. · 1995 · 33 · 99710.1016/0956-716X(95)00312-J ↗
11. Taniguchi · Mater. Trans. JIM · 1991 · 32 · 29910.2320/matertrans1989.32.299 ↗
12. Taniguchi · Mater. Sci. Eng. · 1995 · A198 · 8510.1016/0921-5093(95)80062-Y ↗
13. Taniguchi · Oxid. Metals · 1994 · 42 · 1710.1007/BF01061922 ↗
14. Taniguchi · Oxid. Metals · 1994 · 41 · 10310.1007/BF01196645 ↗
15. G.E. Co., US Patent 4,780,342, 25 October 1988.10.1177/875647938800400639 ↗
16. P. Kofstad, High Temperature Corrosion, Elsevier, Amsterdam, 1988, p. 164.
17. Shimizu · Mater. Sci. Eng. · 1992 · A153 · 60210.1016/0921-5093(92)90258-3 ↗
18. P. Kofstad, High Temperature Corrosion, Elsevier, Amsterdam, 1988, p. 244.
19. P.G. Shewmon, Diffusion in Solids, McGraw-Hill, New York, 1963, p. 23.
20. V.F. Kiselev, O.V. Krylov, Adsorption and Catalysis on Transition Metals and Their Oxides, Springer, New York, 1989, p. 177.10.1007/978-3-642-73887-6 ↗
21. P.W. Atkins, Physical Chemistry, Oxford University Press, New York, 1994, p. 80.
22. Taniguchi · Mater. Trans. JIM · 1991 · 32 · 15110.2320/matertrans1989.32.151 ↗
23. Jin · Script Met. et Mater. · 1993 · 29 · 74710.1016/0956-716X(93)90220-M ↗