A relation between the electrochemical behaviors and morphology of Ni–Co3O4 composites prepared by the chemical reduction method or the mechanical milling
Source abstract
Abstract
Abstract In order to improve low initial coulombic efficiency of Co 3 O 4 (69%), Ni–Co 3 O 4 composites were prepared by the chemical reduction method or by mechanical milling. Ni–Co 3 O 4 composite prepared by the mechanical milling showed an improved initial coulombic efficiency (79%), whereas the initial coulombic efficiency (71%) of Ni–Co 3 O 4 composite obtained from the chemical reduction method was almost the same as that of Co 3 O 4 . In SEM studies, when compared with Ni–Co 3 O 4 composite prepared by the mechanical milling, only a small amount of Ni particles was found on the surface of Ni–Co 3 O 4 composite made by the chemical reduction method. Supposing that Ni in Ni–Co 3 O 4 composite makes the irreversible portion of Li 2 O decompose during the first discharge, the contact area between Ni and Co 3 O 4 should be enlarged as much as possible. Hence, it could be suggested that the disparity between the mechanical milling and the precipitation method in the initial coulombic efficiency results from the difference in the contact area between Ni and Co 3 O 4 , which is closely related to the homogeneity of Ni dispersion on Co 3 O 4 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Electrodeposition and Electroless Coatings · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Sekai · J. Power Sources · 1993 · 43–44 · 24110.1016/0378-7753(93)80120-E ↗
2. Dahn · Solid State Ionics · 1990 · 44 · 8710.1016/0167-2738(90)90049-W ↗
3. Ohzuku · J. Electrochem. Soc. · 1990 · 137 · 76910.1149/1.2086552 ↗
4. Yamada · J. Power Sources · 2003 · 119–121 · 23210.1016/S0378-7753(03)00239-8 ↗
5. Sawai · Solid State Ionics · 1994 · 69 · 27310.1016/0167-2738(94)90416-2 ↗
6. Dahn · Electrochim. Acta · 1993 · 38 · 117910.1016/0013-4686(93)80048-5 ↗
7. Yazami · J. Power Sources · 1993 · 43–44 · 3910.1016/0378-7753(93)80100-4 ↗
8. Idota · Science · 1997 · 276 · 139510.1126/science.276.5317.1395 ↗
9. Tamura · J. Electrochem. Soc. · 2003 · 150 · A67910.1149/1.1568108 ↗
10. Kim · J. Electrochem. Soc. · 1999 · 146 · 440110.1149/1.1392650 ↗
11. Wan · J. Power Sources · 1998 · 75 · 910.1016/S0378-7753(98)00076-7 ↗
12. Poizot · Nature · 2000 · 407 · 49610.1038/35035045 ↗
13. Larcher · J. Electrochem. Soc. · 2002 · 149 · A23410.1149/1.1435358 ↗
14. Obrovac · J. Electrochem. Soc. · 2001 · 148 · A57610.1149/1.1370962 ↗
15. Kang · J. Electrochem. Soc. · 2003 · 150 · A153810.1149/1.1617299 ↗
16. Han · J. Alloys Compd. · 2003 · 349 · 29010.1016/S0925-8388(02)00882-4 ↗
17. Lee · J. Power Sources · 2000 · 90 · 7010.1016/S0378-7753(00)00450-X ↗