The electrochemical potentiokinetic reactivation behavior of Alloy 600
Source abstract
Abstract
Abstract The characteristics of reactivation polarization behavior of Alloy 600 in 0.5 M H 2 SO 4 +0.005 M KSCN solution were investigated. The feasibility of single-loop electrochemical potentiokinetic reactivation (SL-EPR) test technique for the evaluation of the degree of sensitization (DOS) was also explored. The experimental results showed that both sensitized and unsensitized materials exhibited reactivation curves with two separated anodic peaks. The results of reactivation termination tests showed that the anodic peak which appeared at −50 mV (SCE) was associated with the depassivation of grain matrix, while that at +100 mV (SCE) was corresponding to the grain boundary corrosion for sensitized Alloy 600. The anodic peak at more noble potential in the EPR curve might also reflect the occurrence of pitting corrosion of Alloy 600 in the testing electrolyte.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. McMinn · Corrosion · 1988 · 44 · 23910.5006/1.3583932 ↗
2. Briant · Corrosion · 1986 · 42 · 1510.5006/1.3584874 ↗
3. Scarberry · Corrosion · 1976 · 32 · 40110.5006/0010-9312-32.10.401 ↗
4. Bandy · Corrosion · 1985 · 41 · 24210.5006/1.3581997 ↗
5. Rebak · Corrosion · 1993 · 49 · 86710.5006/1.3316012 ↗
6. V. Cihal, et al., in: Proceedings of the Fifth European Corrosion Congress, Paris, September 24–28, 1973.10.1002/maco.19730240707 ↗
7. Annual Book of ASTM Standards, Designation G 108, ASTM, Philadelphia, PA, 1994, p. 450.
8. Clarke · Mater. Perform. · 1980 · 19 · 16
9. Roelandt · Corrosion · 1986 · 42 · 28910.5006/1.3584906 ↗
10. Mignone · Corrosion · 1982 · 38 · 39010.5006/1.3581901 ↗
11. Edgemon · Corrosion · 1994 · 50 · 91210.5006/1.3293482 ↗
12. Maday · Corros. Sci. · 1988 · 28 · 88710.1016/0010-938X(88)90037-6 ↗