Influence of interstitial carbon on the formation of monohydride and dihydride of Ti25V35Cr40 alloys

Chia-Chieh Shen, Kwen-Chou Wu, Hsueh-Chih Li, Yuan-Pang Wu

Publisher page

Abstract

Abstract The presence of interstitial carbon atoms was found to affect the hydrogenation properties of Ti25V35Cr40Cx (x = 0, 0.1, and 0.5) alloys over the range T = 30–300 °C. Heat treatment at T = 1200 °C was used to homogenize the distribution of carbon atoms throughout the specimens. X-ray diffraction, P–C isotherm curves, and thermodynamic measurements, including van't Hoff plots and in-situ temperature-programmed desorption spectra, were used to study the destabilization of the β-phase monohydride and γ-phase dihydride in annealed Ti25V35Cr40Cx as a result of the presence of interstitial carbon atoms. The experimental results showed that the interstitial carbon atoms introduced both obstacles and carbon-induced microstrain into the structure, which significantly destabilized the γ-phase dihydrides to enhance the corresponding plateau pressures at T = 30–80 °C. On the other hand, destabilization of the β-phase monohydride was less pronounced in the presence of interstitial C atoms at T = 150–300 °C. This effect was ascribed to a lower H content in the saturated β-phase monohydrides as compared with the saturated γ-phase dihydrides, as well as microstrain relaxation at higher temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Titanium Alloys Microstructure and Properties · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Metallic hydrides III: body-centered-cubic solid-solution alloys10.1557/mrs2002.225 ↗
2. The higher hydrides of vanadium and niobium10.1021/ic50089a013 ↗
3. Effect of absorption-desorption cycles on structure and stability of protides in Ti-Cr-V alloys10.2320/matertrans.43.2748 ↗
4. Effect of interstitial boron and carbon on the hydrogenation properties of Ti25V35Cr40 alloy10.1016/j.ijhydene.2010.07.166 ↗
5. TiCrVMo alloys with high dissociation pressure for high-pressure MH tank10.1016/j.ijhydene.2008.11.061 ↗
6. C.P. Chou, C.F. Kuo, C.C. Shen, T.P. Perng, F.B. Weng, A. Su, P.H. Chou, P.H. Hsu, Fuel cell module compatible with a dry cell, U.S. Patent, 7485387B2, 2009.
7. Non-Pd BCC alloy membranes for industrial hydrogen separation10.1016/j.memsci.2010.06.068 ↗
8. Hydride formation by B.C.C. solid solution alloys10.4028/www.scientific.net/MSF.31.177 ↗
9. Hydrogenation properties of Fe-Ti-V bcc alloys10.1016/j.jallcom.2010.09.030 ↗
10. Hydrogen storage in Ti–V-based body-centered-cubic phase alloys10.1557/JMR.2003.0352 ↗
11. Effect of Fe addition on hydrogen storage characteristics of Ti0.16Zr0.05Cr0.22V0.57 alloy10.1016/S0925-8388(00)00839-2 ↗
12. Effects of desorption temperature and substitution of Fe for Cr on the hydrogen storage properties of Ti0.32Cr0.43V0.25 alloy10.1016/j.ijhydene.2007.01.012 ↗
13. Influence of Cu addition on structure and hydrogen desorption characteristics of Ti0.16Zr0.05Cr0.22V0.57 alloy10.1016/j.matchemphys.2008.06.023 ↗
14. The solubility and trapping of hydrogen in vanadium10.1016/0001-6160(73)90164-8 ↗
15. Hydrogenation properties of Ti – V – Mn alloys with a BCC structure containing high and low oxygen concentrations10.1016/j.jallcom.2010.10.059 ↗
16. Hydrogen solubility of BCC titanium alloys10.1016/S0925-8388(03)00749-7 ↗
17. Influence of carbon impurity on microstructures and electrode properties for V-based battery alloys10.1016/S0925-8388(99)00210-8 ↗
18. Effect of B addition on the hydrogen absorption-desorption property of Ti0.32Cr0.43V0.25 alloy10.1016/j.ijhydene.2007.12.008 ↗
19. Influence of interstitial oxygen and nitrogen on hydrogen solubility in vanadium10.1016/S0022-3115(97)00098-6 ↗
20. Steam reforming of methanol in a compact copper microchannel foam reactor10.1002/fuce.201300169 ↗
21. Asia Pacific Fuel Cell Technologies Ltd. http://www.apfct.com/index.php, 2014.
22. Approaches and recent development of polymer electrolyte membranes for fuel cells operating above 100 °C10.1021/cm0310519 ↗
23. Phase equilibrium of the Ti–Cr–V ternary system in the non-burning β-Ti alloy region10.1016/S0925-8388(99)00144-9 ↗
24. C.C. Shen, T.P. Perng, H.C. Li, Method for evaluating extrinsic hydrogenation degradation of hydrogen storage material, U. S. Patent, 8691590B2, 2014.
25. Unit-cell refinement from powder diffraction scans10.1107/S0021889881009618 ↗
26. Pecharsky · 2005
27. Effects of hydrogen loading and type of titanium hydride on grain refinement and mechanical properties of Ti-6Al-4V10.1016/j.jallcom.2014.02.171 ↗
28. Smith · 1989
29. Murray · 1987
30. Hydrogen absorption by Laves phase related BCC solid solution10.1016/S0966-9795(97)00088-5 ↗
31. Influence of the C14 Ti35.4V32.3Fe32.3 Laves phase on the hydrogenation properties of the body-centered cubic compound Ti24.5V59.3Fe16.210.1016/j.jallcom.2010.10.213 ↗
32. Effects of B and C on the hydrogenation properties of TiFe and Ti1.1Fe10.1016/S0360-3199(99)00107-X ↗
33. Effect of partial niobium and iron substitution on short-term cycle durability of hydrogen storage Ti-Cr-V alloys10.1016/j.ijhydene.2012.12.100 ↗