journal article·2013-01

Shear bond strength and characterization of interfaces between electroformed gold substrates and porcelain

Y.S. Al Jabbari, X. Barbagadaki, K.A. Al Wazzan, E.A. El-Danaf, G. Eliades, S. Zinelis

Materials Chemistry and Physics· Volume 137· Issue 3
Publisher page

Abstract

Abstract This study aimed to determine the effects of two different sandblasting conditions on the shear bond strength between electroformed Au substrates and porcelain, and characterize the interface between the Au substrate and porcelain. Electroformed Au specimens, 0.3 mm thick with a cap-like shape were prepared. The prepared specimens were then divided into two different groups and each group was sandblasted with a different size of alumina grains (100 or 250 μm) prior to dental porcelain application. Bonded specimens from each group were subjected to shear testing. After debonding, the fracture mode was analyzed by optical microscopy and SEM-EDX. One intact bonded specimen from each group was metallographically prepared to characterize the interfacial bonding by SEM-EDX and area scan analysis. The shear bond strength values (MPa) and standard deviations were 8.2 ± 1.8 and 9.1 ± 2.7 for the samples blasted with 100 and 250 μm alumina particles, respectively. No statistically significant difference was found between the two groups. In addition, no differences in fracture mode were found between the two groups. Qualitative analysis showed that, surprisingly, the Au substrate contained O, N, and P which might be related to the Au–sulfite electrolyte used in electroforming. As expected, the retained porcelain comprised Si, O, Al, Ca, Na and K. Mutual diffusion of Au, P, Si, Na, K and O without concentration gradients was found at the interface. Mutual ionic diffusion at the interface between ceramics and electroformed Au substrates (as opposed to mechanical interlocking) seems to be the most possible factor contributing to Au–ceramic bonding.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Advanced Sensor and Energy Harvesting Materials · Dental materials and restorations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Gold electroforming system: GES restorations
2. Electroforming technique
3. Electroforming technology for galvanoceramic restorations10.1016/S0022-3913(97)70170-7 ↗
4. Comparison of marginal fit of 3 different metal-ceramic systems: an in vitro study
5. Marginal fit of electroformed ceramometal crowns10.1111/j.1532-849X.1996.tb00284.x ↗
6. The marginal fit of cemented galvanoceramic crowns
7. Gold in dentistry: alloys, uses and performance10.1007/BF03215496 ↗
8. Development of the G.E.S. electroforming technique: biocompatible, corrosion-free production of telescopic crowns
9. Clinical marginal gap of porcelain fused to electro-formed gold coping crowns
10. Galvano- vs. metal-ceramic crowns: up to 5-year results of a randomised split-mouth study10.1007/s00784-010-0429-3 ↗
11. Long-term clinical results of galvano-ceramic and glass-ceramic individual crowns10.1016/S0022-3913(00)70010-2 ↗
12. Six-year follow-up of titanium and high-gold porcelain-fused-to-metal fixed partial dentures10.1046/j.1365-2842.1999.00373.x ↗
13. Metal-ceramic failure in noble metal crowns: 7-year results of a prospective clinical trial in private practices
14. A 10-year longitudinal study of fixed prosthodontics: clinical characteristics and outcome of single-unit metal-ceramic crowns
15. ISO 9693 · 1999
16. Comparative microstructural study of the diffusion zone between NiCr alloy and different dental ceramics10.1177/154405910208100509 ↗
17. Oxidation kinetics of some Ni-Cr alloys10.1177/00220345830620011101 ↗
18. Solution of Ni-Cr alloy oxides in an alkali alumino-silicate glass10.1016/S0109-5641(88)80049-6 ↗
19. X-ray diffraction characterization of dental gold alloy-ceramic interfaces10.1023/A:1008906930748 ↗
20. Effect of interfacial variables on metal-porcelain bonding10.1002/jbm.820270414 ↗
21. Microprobe analyses of gold-porcelain bonding10.1177/00220345690480061901 ↗
22. Adherence controlling elements in ceramic-metal systems. I. Precious alloys10.1177/00220345770560090301 ↗
23. Effect of aluminium oxide sandblasting on cast commercially pure titanium surfaces
24. Effects of surface treatments on bond strength between porcelain and electroformed gold substrates
25. Bonding agents of low fusing cpTi porcelains: elemental and morphological characterization10.1016/j.jpor.2009.03.003 ↗
26. Bond strength and surface characterization of a Ni-Cr-Be alloy10.1016/S0109-5641(96)80065-0 ↗
27. An investigation of gold/ceramic and gold/glass interfaces10.1007/BF03214853 ↗
28. The relationship between oxide adherence and porcelain-metal bonding10.1177/00220345880670020801 ↗
29. Comparative evaluation of ceramic-metal bond tests using finite element stress analysis10.1177/00220345800590030901 ↗
30. Designs of bond strength tests for metal-ceramic complexes: review of the literature10.1016/S0022-3913(96)90244-9 ↗
31. Effects of sandblasting media and steam cleaning on bond strength of titanium-porcelain10.4012/dmj.2009-119 ↗
32. Surface analysis of porcelain fused to metal systems10.1016/j.dental.2005.05.003 ↗
33. Fundamentals of glass-to-metal bonding: VIII, nature of wetting and adherence10.1111/j.1151-2916.1962.tb11067.x ↗
34. In situ stress measurements of gold films on glass substrates during thermal cycling10.1063/1.349753 ↗
35. Bonding, structure, and properties of metal/ceramic interfaces: part 1 chemical bonding, chemical reaction, and interfacial structure10.1179/imr.1993.38.5.233 ↗