Strong and tough Al2O3–MgO–C refractories with dispersed aluminosilicate reinforcement
Source abstract
Abstract
Abstract Resin–bonded Al2O3–MgO–C refractories were fabricated with dispersed aluminosilicate reinforcement. The reinforced systems were strong and tough to thermal shock failures over the standard components without reinforcement. MOR measurements showed that the shocked refractories with reinforcement were failed with a maximum strength of 20 MPa, indicating 200% increase of their load bearing capacity. Toughness and fracture surface energy improvements predicted that the shocked systems reinforced with aluminosilicate particulates exhibit three times enhanced resistance to mutual crack growth over the standard. All these beneficial properties indicate a satisfactory thermal shock performance, which is credited to the effective operation of dispersion strengthening\viscoelastic bridging effects offered by a flaw–tolerant microstructure formed in all parts of the refractory oxidized layer fortified with dispersed aluminosilicate reinforcement. Additionally, implications of these results to microstructure design of various classes of carbon containing refractories in MgO–C\Al2O3–C systems formulated with carbon\ceramic reinforcements are proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Oxidation resistance, residual strength, and microstructural evolution in Al2O3-MgO–C refractory composites with YAG nanopowder10.1016/j.jeurceramsoc.2021.01.021 ↗
2. Investigation of thermal shock in a high‐temperature refractory ceramic: a fracture mechanics approach10.1111/j.1151-2916.2001.tb00834.x ↗
3. Structural properties of Al2O3–MgO–C refractory composites improved with YAG nanoparticle hybridized expandable graphite
4. Refractories and Failures
5. Biswas · 2020 · 339
6. FEM simulation of the thermo-mechanical behaviour and failure of refractories—a case study
7. Unique opportunities for microstructural engineering with duplex and laminar ceramic composites10.1111/j.1151-2916.1992.tb07188.x ↗
8. Microstructural design of toughened ceramics10.1111/j.1151-2916.1991.tb06872.x ↗
9. Microstructures and mechanical properties of Al2O3–C refractories with addition of multi-walled carbon nanotubes10.1016/j.msea.2012.04.001 ↗
10. Microstructure and mechanical properties of MgO–C refractories containing graphite oxide nanosheets (GONs)10.1016/j.ceramint.2012.09.080 ↗
11. Effect of nanocarbon sources on microstructure and mechanical properties of MgO‐C refractories10.1016/j.ceramint.2013.08.101 ↗
12. Catalytic formation of one-dimensional nanocarbon and MgO whiskers in low carbon MgO-C refractories10.1016/j.ceramint.2014.11.017 ↗
13. Enhanced mechanical properties of Al2O3-C refractories with silicon hybridized expandable graphite10.1016/j.msea.2017.10.046 ↗
14. Improved thermal shock performance of Al2O3–C refractories due to nano-scaled additives10.1016/j.ceramint.2011.08.011 ↗
15. Elucidating the role of Ti3AlC2 in low carbon MgO-C refractories: antioxidant or alternative carbon source?10.1016/j.jeurceramsoc.2018.03.035 ↗
16. Creep resistant refractory with controlled optical emission
17. Strong, tough and stiff bioinspired ceramics from brittle constituents10.1038/nmat3915 ↗
18. The conflicts between strength and toughness10.1038/nmat3115 ↗
19. Viscoelastic toughening of aluminosilicate refractory ceramics10.1016/j.actamat.2006.02.009 ↗
20. Reaction and sintering mechanisms of mullite in the systems cristobalite/α-Al2O3 and amorphous SiO2/α-Al2O310.1016/0955-2219(96)00023-4 ↗
21. Sintering of α-Al2O3—amorphous silica compacts10.1016/0272-8842(82)90015-3 ↗
22. A novel approach to lightweight alumina‐carbon refractories for flow control of molten steel10.1111/jace.17137 ↗
23. Behavior of silicon carbide/cordierite composite material after cyclic thermal shock10.1016/j.ceramint.2008.04.029 ↗
24. Determination of thermal shock resistance in refractory materials by ultrasonic pulse velocity measurement10.1016/j.jeurceramsoc.2006.05.070 ↗
25. Correlation of damage after first cycle with overall fatigue resistance of refractory castable concrete10.1016/j.conbuildmat.2019.02.069 ↗
26. Assessment of viscoelastic crack bridging toughening in refractory materials10.1016/j.jeurceramsoc.2008.01.021 ↗