On the selection of halide activators for the formation of hybrid Ni-aluminide/Ni coatings on creep resistant ferritic steels by low temperature pack cementation process
Source abstract
Abstract
Abstract Thermochemical calculations were made and experiments were subsequently conducted to verify the thermochemical predictions in an attempt to establish a basis for selecting suitable halide activators for forming Ni-aluminide/Ni hybrid coatings on creep resistant steels by pack cementation at temperatures below 700 °C. The pack powder mixtures analysed and used in subsequent experiments consisted of Al, Al2O3 and one of chloride or fluoride salts which included NH4Cl, AlCl3 (anhydrous), NaCl, NH4F and AlF3. Pack Al content was varied from 0.5 to 16 wt% to show its effects on aluminising kinetics at constant temperature and time. The aluminised layers were analysed using XRD, SEM and EDS. It was demonstrated that the partial pressure of AlX (X = Cl and F) vapour species generated in packs can be used to measure the activating strengths of different chloride and fluoride salts. This is particularly true in the case of chloride salt activated packs in which aluminising kinetics was shown to be higher in packs activated by salts with higher activating strengths. Fluoride salts are not suitable activators in the low temperature range concerned because a solid AlF3 phase layer would deposit on the surface, which would then prematurely terminate the aluminising process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. History of power plants and progress in heat resistant steels history of power plants and progress in heat resistant steels10.2355/isijinternational.41.612 ↗
2. Materials for ultrasupercritical coal power plants – boiler materials: part 110.1361/105994901770345394 ↗
3. Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors10.1179/174328005X41140 ↗
4. The development of creep-resistant steels
5. Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
6. Effect of chromium content on the oxidation behaviour of ferritic steels for applications in steam atmospheres at high temperatures10.1007/s11085-008-9134-x ↗
7. Long-term oxidation kinetics of aluminide coatings on alloy steels by low temperature pack cementation process10.1007/s10853-006-0806-0 ↗
8. Pack aluminisation of low alloy steels at temperatures below 700 °C10.1016/j.surfcoat.2003.10.046 ↗
9. Relationship between pack chemistry and aluminide coating formation for low temperature aluminisation of alloy steels10.1016/j.actamat.2006.05.032 ↗
10. Diffusion coatings for heat exchanger materials10.1179/026708404225016472 ↗
11. Formation of aluminide coatings on ferritic–martensitic steels by a low-temperature pack cementation process10.1016/j.surfcoat.2010.02.025 ↗
12. Formation and oxidation performance of low-temperature pack aluminide coatings on ferritic–martensitic steels10.1016/j.surfcoat.2009.09.063 ↗
13. Long-term performance of aluminide coatings on Fe-base alloys10.1016/j.surfcoat.2007.06.046 ↗
14. Cyclic oxidation and mechanical behaviour of slurry aluminide coatings for steam turbine components10.1016/j.surfcoat.2006.11.033 ↗
15. Slurry coated Ni-plated Fe-base alloys: investigation of the influence of powder and substrate composition on interdiffusional and structural degradation of aluminides10.1016/j.surfcoat.2013.10.038 ↗
16. Iron aluminide coatings on ferritic steels by CVD-FBR technology10.1016/j.intermet.2005.12.010 ↗
17. Mechanisms of formation of diffusion aluminide coatings on nickel-base superalloys10.1007/BF00604047 ↗
18. Aluminide coating formation on nickel-base superalloys by pack cementation process10.1023/A:1012534220165 ↗
19. Low-temperature formation and oxidation resistance of nickel aluminide/nickel hybrid coatings on alloy steels10.1016/j.scriptamat.2008.02.034 ↗
20. A phenomenological model for lifetime design of Ni2Al3/Ni hybrid coating formed on creep resistant ferritic steels10.1007/s10853-011-5793-0 ↗
21. Steam oxidation resistance of Ni-aluminide/Fe-aluminide duplex coatings formed on creep resistant ferritic steels by low temperature pack cementation process10.1016/j.corsci.2010.09.064 ↗
22. Comparison of the dry and wet oxidation at 900 °C of η-Fe2Al5 and δ-Ni2Al3 coatings10.1016/j.corsci.2010.10.003 ↗
23. Formation of nickel aluminide/nickel hybrid coatings on alloy steels by a two step process of nickel plating and low temperature pack aluminisation10.1179/174328407X245111 ↗
24. Rare-earth modified chromium-aluminide coatings applied by pack cementation method on low-alloy steels10.1007/BF00354445 ↗
25. Modelling of aluminized coating growth on nickel10.1016/j.actamat.2007.08.025 ↗
26. Diffusion mechanisms and microstructure development in pack aluminizing of Ni-based alloy10.1016/j.surfcoat.2013.11.034 ↗
27. Kinetics of phase layer growth during aluminide coating of nickel10.1007/BF02658400 ↗
28. On the kinetics of the pack-aluminization process10.1007/BF02656589 ↗
29. Gas phase deposition of aluminum on nickel alloys10.1016/0040-6090(77)90268-1 ↗
30. Thermodynamics and kinetics of pack aluminide coating formation on IN-10010.1149/1.2401976 ↗
31. The effect on the kinetics of pack aluminisation of varying the activator10.1016/0040-6090(80)90501-5 ↗
32. Codeposited chromium and silicon diffusion coatings for Fe-base alloys via pack cementation10.1007/BF01052029 ↗