Abstract

Abstract A sol–gel processed mullite powder of median size 1.7 μm and woven fabrics with 270 μm thick of Si–Ti–C–O fibers (10 vol.%) were formed into laminated composites by doctor blade and hot-pressed at 1500–1750°C under a pressure of 39 MPa in a N2 atmosphere. The structures of fiber interior and interfaces between fibers and mullite matrix were characterized by analytical transmission electron microscopy. Pyrolysis of the amorphous fibers in dense mullite matrix was suppressed as compared with monolithic fibers with no mullite matrix. Partial pyrolysis of fibers during hot-pressing was accompanied by crystallization into β-SiC, diffusion of Ti element from inside the fibers to the interfaces and the formation of pores inside the fibers. The fracture resistance of the notched composite with crack extension was measured at room temperature. A main crack was deflected at the Si–Ti–C–O fabric layer under the compressive residual stress, leading to the increase of fracture resistance near the fabric layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Stable and metastable equilibria in the system SiO2–Al2O310.1111/j.1151-2916.1975.tb18770.x ↗
2. High-temperature mechanical properties of mullite under compression10.1111/j.1151-2916.1977.tb15492.x ↗
3. Creep of mullite ceramics10.2109/jcersj.97.662 ↗
4. Creep of hot-pressed SiC whisker reinforced mullite
5. Microstructure and mechanical properties of mullite prepared by the sol–gel method10.1111/j.1151-2916.1987.tb04857.x ↗
6. Sintering and mechanical properties of stoichiometric mullite10.1111/j.1151-2916.1985.tb15252.x ↗
7. Microstructure, microchemistry, and flexural strength of mullite ceramics10.1111/j.1151-2916.1991.tb04295.x ↗
8. Synthesis of whisker reinforced mullite matrix composites using colloidal processing10.2109/jcersj.100.353 ↗
9. Mechanical properties of SiC whisker-reinforced mullite composites, part 110.2109/jcersj.106.843 ↗
10. Mechanical properties of mullite-β-silicon nitride whisker composite ceramics10.2109/jcersj.99.89 ↗
11. Colloidal processing and mechanical properties of whisker-reinforced mullite matrix composites10.1111/j.1151-2916.1991.tb06781.x ↗
12. Development of SiC-whisker-reinforced ceramics
13. Mechanical properties of mullite-SiC-whisker composites10.2109/jcersj.97.895 ↗
14. S. Somiya, R.F. Davis, J.A. Pask (Eds.), Ceramic Transactions, Vol. 6, Mullite and Mullite Matrix Composites, 45 papers, American Ceramic Society, Westerville, OH, 1990.
15. I.A. Aksay, S.M. Wiederhorn (Eds.), Mullite Processing, Structure and Properties, 21 papers, J. Am. Ceram. Soc. 74 (10) (1991).10.1111/j.1151-2916.1991.tb06766.x ↗
16. Mullite powder technology and application in Japan
17. H. Schneider, N. Claussen, G.L. Messing, K. Okada, J.A. Pask, S. Somiya (Eds.), Mullite’94 (special issue), 40 papers, J. Eur. Ceram. Soc. 16 (2) (1996).
18. Processing and mechanical properties of laminated composites of mullite/woven fabrics of Si–Ti–C–O fibers10.1016/0955-2219(96)82836-6 ↗
19. Observation of interfaces of Si–Ti–C–O fibers/mullite matrix composites by analytical transmission electron microscopy10.2109/jcersj.103.1197 ↗
20. T. Fujimoto, M. Kaji, K. Koga, Y. Hirata, TEM observation of Si–Ti–C–O fiber/mullite matrix composites, in: Extended Abstracts of 10th Fall Meeting of the Ceramic Society of Japan, Nagano, Japan, October 1997, The Ceramic Society of Japan, Tokyo, 1997, p. 165 (2B06).
21. Colloidal processing for preparation of laminated composites of mullite/woven fabrics of Si–Ti–C–O fibers10.1016/0167-577X(93)90129-L ↗
22. Effect of oxygen on pyrolysis of Si–Ti–C–O fibers10.2109/jcersj.99.401 ↗
23. Pyrolysis of low oxygen SiC fiber prepared by electron-irradiation curing method10.2109/jcersj.101.1379 ↗
24. High-strength alkali-resistant sintered SiC fibre stable to 2200°C10.1038/35820 ↗
25. A tough, thermally conductive silicon carbide composite with high strength up to 1600°C in air10.1126/science.282.5392.1295 ↗
26. Y. Hirata, R. Yamashita, Crack extension of laminated SiC fabrics/mullite matrix composites, in: Extended Abstracts of Annual Meeting of the Ceramic Society of Japan, Osaka, Japan, March 1997, The Ceramic Society of Japan, Tokyo, 1997, p. 362 (2G28).
27. Y. Hirata, Crack extension and residual stress of laminated SiC fabrics/mullite matrix composites, in: Proceedings of the 16th Forum on Basic Science for High-temperature Ceramics, Shizuoka, Japan, November 1997, The Ceramic Society of Japan, Tokyo, 1997, pp. 49–53.
28. Y. Kyoden, Y. Kamino, Y. Fukushige, Y. Hirata, S. Shibuya, Processing and fracture behavior of laminated Si–Ti–C–O fibers/mullite matrix composites, in: K. Niihara, S. Hirano, S. Kanzaki, K. Komeya, K. Morinaga (Eds.), Proceedings of the Sixth International Symposium on Ceramic Materials and Components for Engines, Arita, Japan, October 1997, Japan Fine Ceramic Association, Tokyo, 1998, pp. 788–791.