Kinetic investigation of C38 steel corrosion in concentrated perchloric acid solutions

M. Benabdellah, K.F. Khaled, B. Hammouti

Materials Chemistry and Physics· Volume 120· Issue 1
Publisher page

Abstract

The corrosion behaviour of steel at various concentrations of perchloric acid was studied by weight loss method in temperature range from 298 to 323 K. Results obtained show that corrosiveness of acid increases with its concentration and temperature. The logarithm of corrosion rate was plotted against the acid concentration and values of Hammett Ho and Strehlow Ro(H) acidity functions. The activation energies, enthalpies and entropies of the corrosion process of steel were also determined and fitted against Ro(H). © 2009 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Wang · Corros. Sci. · 2001 · 43 · 228110.1016/S0010-938X(01)00036-1 ↗
2. Khaled · J. Appl. Electrochem. · 2004 · 34 · 69710.1023/B:JACH.0000031160.88906.03 ↗
3. Mu · Mater. Chem. Phys. · 2004 · 86 · 5910.1016/j.matchemphys.2004.01.041 ↗
4. Ebenso · Mater. Chem. Phys. · 1999 · 60 · 7910.1016/S0254-0584(99)00074-7 ↗
5. Benabdellah · Appl. Surf. Sci. · 2005 · 252 · 165710.1016/j.apsusc.2005.03.191 ↗
6. Hammouti · Bull. Electrochem. · 1998 · 14 · 49
7. Elouafi · Ann. Chim. Sci. Mater. · 2001 · 26 · 7910.1016/S0151-9107(01)80086-6 ↗
8. Abed · Bull. Electrochem. · 2000 · 16 · 289
9. Garverick · 1994
10. Bradford · 1998
11. Osman · Anti-Corros. Meth. Mater. · 1998 · 45 · 17610.1108/00035599810216894 ↗
12. Tang · Corros. Sci. · 2003 · 45 · 225110.1016/S0010-938X(03)00046-5 ↗
13. Zhao · Corros. Sci. · 1999 · 41 · 193710.1016/S0010-938X(99)00029-3 ↗
14. Wahdan · Mater. Chem. Phys. · 1997 · 49 · 13510.1016/S0254-0584(96)01925-6 ↗
15. Kriaa · Corros. Sci. · 2008 · 50 · 348710.1016/j.corsci.2008.09.004 ↗
16. Hammett · J. Am. Chem. Soc. · 1932 · 54 · 272110.1021/ja01346a015 ↗
17. Hammett · Chem. Rev. · 1935 · 16 · 6710.1021/cr60053a006 ↗
18. Koepp · Z. Electrochem. · 1960 · 64 · 484
19. Strehlow · 1966 · 129
20. Strehlow · Z. Phys. Chem. · 1961 · 30 · 14110.1524/zpch.1961.30.1_2.141 ↗
21. Hammouti · Ber. Bunsenges. Phys. Chem. · 1997 · 101 · 6510.1002/bbpc.19971010108 ↗
22. Hammouti · Bull. Electrochem. · 1997 · 13 · 466
23. El Ouafi · Annales de Chimie Science des Matériaux · 2001 · 26 · 7910.1016/S0151-9107(01)80086-6 ↗
24. Hammouti · Bull. Electrochem. · 2000 · 16 · 283
25. Hammouti · Bull. Electrochem. · 2001 · 17 · 335
26. Hammouti · Trans. SAEST · 2004 · 39 · 466
27. Louis · Can. J. Chem. · 1985 · 63 · 90810.1139/v85-151 ↗
28. Janata · J. Chem. Soc. Farad. Trans. · 1972 · 1 · 165610.1039/f19726801656 ↗
29. Perez · 2004
30. I.N. Putilova, S.A. Balezin, V.P. Barannik, Metallic Corros. Inhib., Pergamon Press, Oxford, 1960, p. 27.