journal article·2019-02

Microstructure and mechanical properties of brass/Mo composites processed via pressureless and spark plasma sintering

Ehsan Rahimi, Mohammad Ardestani, Mohammad Moazami-Goudarzi, Alireza Abbasi

Publisher page

Abstract

Abstract Brass/molybdenum composites containing 30, 70 and 85 wt% Mo were synthesized by mechanical milling and densification of the brass/Mo powder mixtures. The milled powders were separately consolidated by spark plasma and pressureless sintering processes. The pressureless sintered samples were cold compacted under 300, 450 and 600 MPa before sintering. The results showed that by increasing the cold pressure up to 600 MPa, the relative density of the sintered samples with 70 and 85 wt% Mo were increased. However, the highest relative density of the brass-30 wt% Mo composites was achieved for the samples which were cold compacted under 450 MPa before sintering. The microstructural observations by scanning electron microscopy and energy dispersive spectroscopy analyses revealed that the distribution of Mo particles within the brass matrix of brass-30 wt% Mo composites was not as fine as the other samples. According to the results, the relative density and hardness of the spark plasma sintered samples was higher than that of the pressureless sintered ones. Moreover, increasing the volume percent of molybdenum has led to decreasing the relative density of the spark plasma sintered samples. The flexural strength of the spark plasma sintered composites with 30, 70 and 85 wt% Mo were 397, 376 and 114 MPa, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Chawla · 2013
2. Balasubramanian · 2014
3. 1998
4. The effect of sintering temperature on densification of nanoscale dispersed W–20–40wt% Cu composite powders10.1016/j.ijrmhm.2009.04.004 ↗
5. The influence of the dispersion technique on the characteristics of the W–Cu powders and on the sintering behavior10.1016/S0032-5910(03)00123-2 ↗
6. Solid state and liquid phase sintering of mechanically activated W–20 wt. % Cu powder mixture10.1016/j.jallcom.2007.08.080 ↗
7. Experimental investigations on the synthesis of W–Cu nanocomposite through spark plasma sintering10.1016/j.jallcom.2015.03.183 ↗
8. Mechanochemical synthesis of W–Cu nanocomposites via in-situ Co-reduction of the oxides10.1016/j.powtec.2012.08.013 ↗
9. Fabrication and characterization of W–15Cu composite powders by a novel mechano-chemical process10.1016/j.msea.2007.11.022 ↗
10. Synthesis and densification of W–30wt%Cu composite powders using ammonium meta tungstate and copper nitrate as precursors10.1016/j.ijrmhm.2009.01.001 ↗
11. Liquid phase sintering of mechanically alloyed Mo-Cu powders10.1016/j.msea.2017.06.090 ↗
12. Cu–Mo composite powders obtained by combustion–coreduction process10.1016/j.ijrmhm.2015.09.002 ↗
13. Compressibility and solid-state sintering behavior of W-Cu composite powders10.1515/secm-2013-0159 ↗
14. Self-compacting high density tungsten–bronze composites10.1016/j.jmatprotec.2013.02.006 ↗
15. Sintering behavior and microstructure evolution of mechanically alloyed W–bronze composite powders by two-step ball milling process10.1016/j.jmst.2012.12.001 ↗
16. The effects of sintering temperature on the densification of mechanically alloyed W-brass composites10.4236/ojmetal.2015.53003 ↗
17. Synthesis and densification of tungsten-brass composite by mechanical alloying10.4236/ojmetal.2015.53004 ↗
18. Effects of sintering temperature on microstructure and mechanical properties of spark plasma sintered titanium10.1016/j.matchemphys.2017.09.069 ↗
19. Chawla · 2012
20. German · 2005
21. Lenel · 1980
22. Fabrication and consolidation behavior of Al 6061 nanocomposite powders reinforced by multi-walled carbon nanotubes10.1016/j.powtec.2014.03.039 ↗
23. Campbell · 2008