Abstract

Abstract The morphologies, crystal structures and electrochemical properties of the LiV 3 O 8 powders prepared by spray pyrolysis at various preparation temperatures are investigated. The pure crystal structures of layered LiV 3 O 8 phase are obtained after post-treatment at 400 °C irrespective of the preparation temperatures of the as-prepared powders. However, the morphologies of the post-treated LiV 3 O 8 powders are affected by the preparation temperatures of the as-prepared powders. The powders prepared at 600, 900 and 1000 °C have spherical shapes before and after post-treatment. The mean size of the LiV 3 O 8 powders obtained from the as-prepared powders obtained at 900 °C is 0.63 μm. The discharge capacities of the LiV 3 O 8 powders obtained from the as-prepared powders obtained at 900 °C decreased from 300 to 289 mAh g −1 by the 30th cycles at a current density of 0.1 C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Transition Metal Oxide Nanomaterials · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Wadsley · Acta Crystallogr. · 1957 · 10 · 26110.1107/S0365110X57000821 ↗
2. Nassau · J. Non-Cryst. Solids · 1981 · 44 · 29710.1016/0022-3093(81)90032-6 ↗
3. Pistoia · J. Electrochem. Soc. · 1990 · 137 · 236510.1149/1.2086945 ↗
4. Wang · J. Power Sources · 2004 · 133 · 22910.1016/j.jpowsour.2004.01.048 ↗
5. Lanz · J. Electrochem. Soc. · 2000 · 147 · 399710.1149/1.1394009 ↗
6. Kannan · J. Power Sources · 2006 · 159 · 140510.1016/j.jpowsour.2005.12.026 ↗
7. Panero · J. Electrochem. Soc. · 1983 · 130 · 122510.1149/1.2119923 ↗
8. Liu · Mater. Chem. Phys. · 2009 · 114 · 91510.1016/j.matchemphys.2008.10.064 ↗
9. Yang · J. Mater. Process. Technol. · 2008 · 207 · 26510.1016/j.jmatprotec.2007.12.122 ↗
10. Xie · Mater. Lett. · 2003 · 57 · 268210.1016/S0167-577X(02)01356-3 ↗
11. Zhou · Solid State Ionics · 2008 · 179 · 176310.1016/j.ssi.2008.03.025 ↗
12. Liu · J. Alloys Compd. · 2009 · 471 · 35210.1016/j.jallcom.2008.03.096 ↗
13. Xu · Electrochim. Acta · 2004 · 49 · 34910.1016/j.electacta.2003.08.017 ↗
14. Liu · Electrochim. Acta · 2002 · 47 · 323910.1016/S0013-4686(02)00174-3 ↗
15. Bakenov · Solid State Ionics · 2005 · 176 · 102710.1016/j.ssi.2005.02.004 ↗
16. Park · Electrochim. Acta · 2004 · 49 · 55710.1016/j.electacta.2003.09.009 ↗
17. Taniguchi · J. Power Sources · 2002 · 109 · 33310.1016/S0378-7753(02)00076-9 ↗
18. Taniguchi · Solid State Ionics · 2002 · 146 · 23910.1016/S0167-2738(01)01016-5 ↗
19. Ju · Ceram. Int. · 2009 · 35 · 120510.1016/j.ceramint.2008.06.007 ↗
20. Oh · Solid State Ionics · 2004 · 171 · 16710.1016/j.ssi.2004.04.012 ↗
21. Ju · Electrochim. Acta · 2010 · 55 · 608810.1016/j.electacta.2010.05.071 ↗
22. Ko · J. Alloys Compd. · 2010 · 502 · 15810.1016/j.jallcom.2010.04.133 ↗