Synthesis and characterization of strontium and magnesium substituted lanthanum gallate–nickel cermet anode for solid oxide fuel cells
Source abstract
Abstract
Abstract La 0.90 Sr 0.10 Ga 0.85 Mg 0.15 O 3− δ (LSGM) was prepared by solid state synthesis and mixed with various amounts of Ni and NiO, respectively. The optimum sintering temperature of the material was identified by dilatometric studies to be above 1300 °C. The interaction between LSGM and NiO was studied by X-ray diffraction after sintering at 1300 and 1400 °C in air as well as after reduction in hydrogen atmosphere at 800 and 1000 °C. The LaSrGa 3 O 7 compound was detected after sintering, whereas, LaSrGaO 4 was found after reduction treatment of the material. Diffusion of Ni into LSGM was thought to be the reason for the presence of the above mentioned phases. After the treatment, LSGM contained 2.3 at% of Ni determined by energy dispersive X-ray analysis (EDX). The thermal expansion coefficient of LSGM with varying contents of Ni was observed to increase with increasing the Ni content.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Ishihara · J. Am. Chem. Soc. · 1994 · 116 · 380110.1021/ja00088a016 ↗
2. Feng · Eur. J. Solid State Inorg. Chem. · 1994 · 31 · 663
3. de Haart · J. Power Sources · 1998 · 71 · 30210.1016/S0378-7753(97)02725-0 ↗
4. Simwonis · J. Mater. Res. · 1997 · 12 · 150810.1557/JMR.1997.0207 ↗
5. Möbius · J. Solid State Electrochem. · 1997 · 1 · 210.1007/s100080050018 ↗
6. Brandon · Annu. Rev. Mater. Res. · 2003 · 33 · 18310.1146/annurev.matsci.33.022802.094122 ↗
7. Simwonis · Solid State Ionics · 2000 · 132 · 24110.1016/S0167-2738(00)00650-0 ↗
8. Zhu · Mater. Sci. Eng., A · 2003 · 362 · 22810.1016/S0921-5093(03)00620-8 ↗
9. Huang · J. Electrochem. Soc. · 1997 · 144 · 362010.1149/1.1838058 ↗
10. Huang · J. Am. Ceram. Soc. · 1999 · 82 · 240210.1111/j.1151-2916.1999.tb02096.x ↗
11. Schulz · Phys. Chem. Chem. Phys. · 2003 · 5 · 230810.1039/B301882M ↗
12. Taylor · Z. MetaIlkd. · 1990 · 81 · 345
13. Shannon · Acta Crystallogr., A · 1976 · 32 · 75110.1107/S0567739476001551 ↗
14. Huang · J. Electrochem. Soc. · 2001 · 148 · A78810.1149/1.1378289 ↗
15. Majewski · J. Am. Ceram. Soc. · 2001 · 84 · 109310.1111/j.1151-2916.2001.tb00795.x ↗
16. Majewski · J. Alloys Compd. · 2001 · 329 · 25310.1016/S0925-8388(01)01583-3 ↗
17. Rozumek · J. Am. Ceram. Soc. · 2004 · 87 · 65610.1111/j.1551-2916.2004.00656.x ↗
18. Matraszek · Solid State Ionics · 2004 · 166 · 34310.1016/j.ssi.2003.11.016 ↗
19. Höfer · J. Electrochem. Soc. · 1993 · 140 · 288910.1149/1.2220928 ↗
20. Nakamura · Mater. Res. Bull. · 1979 · 14 · 64910.1016/0025-5408(79)90048-5 ↗