Wear resistance of austempered pearlitic ductile iron (Letter to the Editor)

Dušan Jesić, Pavel Kováč, M. Plavšic, Ľubomír Šooš, D. Sarjanovic

Abstract

The influence of austempering temperature on tribological properties of austempered pearlitic ductile iron (ADI) was investigated. The as-cast ductile iron was subjected to heat treatments consisting of austenitization at 900 C followed by austempering at temperatures of 250, 300 and 350 C for 120 min. The austempered samples were subjected to abrasion and adhesion wear resistance tests using steel and ductile iron plates. The abrasive wear testing of the tribo-pair was undertaken with the sanding plate. The results of abrasion and adhesion wear resistance tests are presented, and the effect of austempering temperature is discussed. K e y w o r d s : austempered ductile iron, heat treatment, wear
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.