Effects of Heat Treatment and Thermal Cycle Conditions on the Bonding Strength and Interfacial Characteristics of Electroplated Cr/Electroplated Ni-P Coatings
Source abstract
Abstract
The effects of heat treatment and thermal cycle conditions on the bonding strength and interfacial characteristics of electroplated Cr/electroplated Ni-P coatings were systematically evaluated. With step1 samples, heat treatment was performed at 750 o C for 6 hours after successive electroplating of Ni-P and Cr layers. With step2 samples, 1st heat treatment was performed at 500 o C for 3 hours after electroplating Ni-P, and then 2nd heat treatment was performed at 750 o C for 6 hours after electroplating Cr. The bonding strengths measured by ASTM C633 were around 54.6 MPa before thermal cycling, and decreased to 35 MPa and 29.9 MPa for the step1 and the step2, respectively, after 1,000 cycles between 150~600 o C. Increasing the number of thermal cycles led to an increasing adhesive/Cr interface delaminated mode, which seemed to be closely related to the decreaed bonding strength possibly due to severe surface Cr oxidation. Also, the higher residual stress was investigated in the step1 than step2 samples. It is thought to be responsible for the higher density of channeling cracks in the Cr layer, which led to slightly stronger bonding strength due to the mechanical interlocking effects of the adhesive inside the channeling cracks.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Electronic Packaging and Soldering Technologies · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.