Fabrication and Mechanical Properties of WC Alloy Hard Materials by a Pulsed Current Activated Sintering Method
Source abstract
Abstract
In this study, planetary ball milled WC-5 wt%Co powders were sintered using the pulsed current activated sintering (PCAS) process. With this process, fully densified hard materials were obtained in a shorter time than conventional processes such as a HP and HIP. The particle sizes of the planetary ball milled WC and Co were 0.114 m and 0.154 m, respectively. The PCAS process was performed at temperatures up to 1300 with 60 MPa and electric current for 13 min without any significant change in the grain size. The WC-5 wt% Co hard materials were fully densified with a relative density of up to 99.8%. The density of WC-5 wt% Co hard materials increased with increasing shrinkage ratio. In addition, the Co particles penetrated into the WC particles by dissolving and re-precipitation, and finally hard materials were completely densified. The average grain size of the WC-5 wt%Co was 0.25 m, and the hardness and fracture toughness were 2,386 kg/mm 2 and 6.0 MPam 1/2
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.