article·2011-01-25

Fabrication and Mechanical Properties of ultra fine WC-6wt.%Co by Spark Plasma Sintering Process

Hyun-Kuk Park, Seungmin Lee, Hee-Jun Youn, Ki-Sang Bang, Ik-Hyun Oh

Publisher page

Abstract

Using the spark plasma sintering process (SPS process), the WC-6wt.%Co hard materials were densified using an ultra fine WC-Co powder. The WC-Co was almost completely dense with a relative density of up to 100% after the simultaneous application of a pressure of 60 MPa and the DC pulse current for 3 min without any significant change in the grain size. The average grain size of WC that was produced through this experiment was about 0.2~0.8 μm. The hardness and fracture toughness were about 1816 kg/mm and 15.1 MPa·m, respectively, for 60 MPa at 1200°C. (Received September 30, 2010)
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.