journal article·2018-12-05Open access

Sulfur Poisoning of Ni Anode as a Function of Operating Conditions in Solid Oxide Fuel Cells

Ho Seong Lee, Hyun Mi Lee, Hyung-Tae Lim

Abstract

In the present study, we investigated the sulfur poisoning of the Ni anode in solid oxide fuel cells (SOFCs) as a function of operating conditions. Anode supported cells were fabricated, and sulfur poising tests were conducted as a function of current density, H 2 S concentration and humidity in the anode gas. The voltage drop was significant under the higher current density (~ 714 mA/cm 2 ) condition, while it was much reduced under the lower current density (~ 389 mA/cm 2 ) condition, at 100 ppm of H 2 S. A secondary voltage drop, which occurred only at the high current density, was attributed to Ni oxidation in the anode. Thus, operation at high current density with high H 2 S concentration may lead to permanent deterioration in the anode. The effect of water content (10%) on the sulfur poisoning was also investigated through a constant current test (~ 500 mA/cm 2 ) at 10 ppm of H 2 S. The cell operating with 10% wet anode gas showed a much smaller initial voltage drop, in comparison with a dry anode gas. The present study indicates that operating conditions, such as gas humidity and current density, should be carefully taken into account, especially when fuel cells are operated with H 2 S containing fuel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Singhal · 2003
2. 10.3365/KJMM.2017.55.5.33510.3365/KJMM.2017.55.5.335 ↗
3. 10.1016/j.ssi.2005.05.00810.1016/j.ssi.2005.05.008 ↗
4. 10.1016/j.jpowsour.2008.05.00210.1016/j.jpowsour.2008.05.002 ↗
5. 10.1007/s12540-017-6401-x10.1007/s12540-017-6401-x ↗
6. 10.1016/j.jpowsour.2011.02.05310.1016/j.jpowsour.2011.02.053 ↗
7. 10.1016/j.ssi.2008.02.06210.1016/j.ssi.2008.02.062 ↗
8. 10.1039/c1ee01758f10.1039/c1ee01758f ↗
9. 10.1016/j.jpowsour.2018.01.06710.1016/j.jpowsour.2018.01.067 ↗
10. 10.1149/07801.1285ecst10.1149/07801.1285ecst ↗
11. 10.1016/j.ijhydene.2016.06.01410.1016/j.ijhydene.2016.06.014 ↗
12. 10.1016/j.ijhydene.2017.12.13410.1016/j.ijhydene.2017.12.134 ↗
13. 10.1016/j.jallcom.2017.11.38110.1016/j.jallcom.2017.11.381 ↗
14. 10.1016/j.jpowsour.2009.02.00110.1016/j.jpowsour.2009.02.001 ↗
15. 10.1149/2.032211jes10.1149/2.032211jes ↗
16. 10.1016/j.ijhydene.2007.11.03310.1016/j.ijhydene.2007.11.033 ↗
17. Cheng · 2008
18. Waldbillig · 2005 · 237
19. 10.1149/1.272917410.1149/1.2729174 ↗
20. 10.1039/c0ee00386g10.1039/c0ee00386g ↗
21. 10.1016/j.ssi.2007.04.00410.1016/j.ssi.2007.04.004 ↗
22. 10.1016/j.cej.2015.08.09110.1016/j.cej.2015.08.091 ↗
23. 10.1149/2.080406jes10.1149/2.080406jes ↗
24. 10.1016/j.ceramint.2015.09.00610.1016/j.ceramint.2015.09.006 ↗
25. 10.1016/j.jpowsour.2010.09.08910.1016/j.jpowsour.2010.09.089 ↗
26. 10.1002/fuce.20140007010.1002/fuce.201400070 ↗
27. 10.1016/j.ssi.2012.03.02310.1016/j.ssi.2012.03.023 ↗
28. Hansen · 2008
29. 10.1149/1.272907410.1149/1.2729074 ↗