journal article·2019-04-05Open access

Corrosion of Hot-dip Aluminized 9Cr-1Mo Steel in N2/0.1%H2S Gas

Muhammad Ali Abro, Junhee Hahn, Dong Bok Lee

Abstract

ASTM P91 steel (viz. 9Cr-1Mo steel) was hot-dip aluminized to form a ~70 m thick coating, and was then corroded in N 2 /0.1%H 2 S gas for 50 h at 800 and 900 C, to study the effect of aluminizing on the corrosion resistance of P91 steel in highly corrosive H 2 S environments. Before corrosion, the aluminized coating consisted of an Al-rich topcoat, an Al 13 Fe 4 upper layer, and an Al 5 Fe 2 lower layer from the surface. During corrosion, Al, oxygen, and sulfur diffused inwardly, while substrate elements diffused outwardly. Impurity oxygen in the gas reacted preferentially with Al to form -Al 2 O 3 at the surface, which increased the corrosion resistance significantly. Bare P91 steel corroded quickly, to form bi-layered, fragile, nonprotective FeS scales. The coating transformed into either a (Al 13 Fe 4 , Al 5 Fe 2 )-mixed layer, AlFe layer, AlFe 3 layer, and -Fe(Al) layer when corroded at 800 C/50 h, or into a AlFe 3 layer and -Fe(Al) layer when corroded at 900 C/ 50 h. Interdiffusion that occurred during corrosion increased the total coating thickness, and transformed (high Al)-Fe phases to (low Al)-Fe phases. The corrosion accompanied the formation of voids and microcracks in the coating.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Mathiazhagan · 2011
2. Fry
3. 10.1016/j.supflu.2012.08.01510.1016/j.supflu.2012.08.015 ↗
4. 10.1007/s11085-007-9087-510.1007/s11085-007-9087-5 ↗
5. 10.1007/BF0060619410.1007/BF00606194 ↗
6. 10.1007/BF0065989910.1007/BF00659899 ↗
7. Lai · 1990 · 201
8. Simms · 1993 · 807
9. John · 2010 · 240
10. 10.1016/j.cej.2017.05.09810.1016/j.cej.2017.05.098 ↗
11. 10.1016/S1875-9491(08)00010-010.1016/S1875-9491(08)00010-0 ↗
12. 10.1002/maco.1992043030210.1002/maco.19920430302 ↗
13. 10.5695/JKISE.2016.49.2.14710.5695/JKISE.2016.49.2.147 ↗
14. 10.1007/BF0060992610.1007/BF00609926 ↗
15. 10.1007/s12540-016-6218-z10.1007/s12540-016-6218-z ↗
16. 10.3365/KJMM.2018.56.5.35010.3365/KJMM.2018.56.5.350 ↗
17. 10.1016/S0921-5093(98)00573-510.1016/S0921-5093(98)00573-5 ↗
18. 10.1179/mst.1997.13.10.83210.1179/mst.1997.13.10.832 ↗
19. 10.1016/j.apsusc.2013.04.01510.1016/j.apsusc.2013.04.015 ↗
20. 10.1007/s12540-017-6366-910.1007/s12540-017-6366-9 ↗
21. 10.1016/j.surfcoat.2005.11.03110.1016/j.surfcoat.2005.11.031 ↗
22. Barin · 1989
23. Birks · 2006 · 145
24. Grabke · 1984 · 59
25. Kutsuna · 2004 · 83
26. 10.2320/matertrans.47.148010.2320/matertrans.47.1480 ↗