Thermoelectric Properties of Ge-doped Higher Manganese Silicides MnSi1.72-1.73:Gem
Source abstract
Abstract
Ge-doped higher manganese silicides (HMSs) MnSi 1.72-1.73 :Ge m (m = 0.01-0.04) were prepared and their thermoelectric properties were studied. HMS powders were synthesized by solid-state reaction of raw material powders (Mn, Si, and Ge) at 1273 K for 6 h in vacuum, and hot-pressed at 1173 K for 2 h under 70 MPa. Mn 11 Si 19 or Mn 15 Si 26 was the main HMS phase; only a small quantity of Si remained. The intermetallic compound MnSi was not produced. The lattice constants increased with the substitution of Ge at Si sites. With the increase in the Ge doping concentration, the electrical conductivity increased, while the Seebeck coefficient decreased. The power factor was significantly increased by the Ge doping, owing to the increase in the electrical conductivity. The Ge doping led to phonon scattering owing to the difference in mass between Ge and Si, leading to a reduced thermal conductivity. Therefore, the dimensionless figure of merit (ZT) was remarkably enhanced by the Ge doping. For MnSi 1.72 :Ge m , the maximum ZT of 0.44 was obtained at 823 K for MnSi 1.72 :Ge 0.01 , while for MnSi 1.73 :Ge m , the maximum ZT of 0.37 was achieved at 823 K for MnSi 1.73 :Ge 0.03 .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Intermetallics and Advanced Alloy Properties · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.