journal article·2018-01-05Open access

Growth Rate of Gamma Prime Precipitates in Ni-Base Superalloy

Authors not provided

Abstract

The mechanical properties of nickel-base superalloys used in disk and blade materials for gas turbine engines can be maximized by controlling their microstructure, such as the size of precipitates. In this study, we investigated the size of gamma prime precipitates after age hardening heat treatment at 650-980 o C for 1-48 hours. As the aging temperature and time increased, the grain size of gamma prime increased. The growth constants were 0.11, 0.24, 15.5 and 167 nm 3 /sec at 650, 760, 870, and 980 o C respectively. Activation energy for the growth of the gamma prime precipitates was determined to be 26154 kJ/mol and reference studies have confirmed that Ni, Al, or Ti lattice diffusion in Ni or Ni3Al dominates the rate. The hardness increased with the decreasing size of gamma prime precipitates, and reached maximum at 24 nm, and decreased thereafter. The data on hardness vs. precipitate size followed the Hall-Petch relation over a precipitate size range from 24 nm to hundreds of nanometers. The maximum hardness at each annealing time increased with a reduction in the annealing temperature time. The optimum condition was determined to be 727 o C and 24 hours by using an approximation curve. The maximum hardness (520HV) was experimentally confirmed under this condition. The reduction in hardness with decreasing size might be due to changes in the misfit strain at the interface, decrease in the gamma prime volume fraction, or an increase in particle cutting events by dislocation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical and Alloy Processes · Intermetallics and Advanced Alloy Properties · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.