journal article·2017-12-05Open access

Effect of Cooling Rate on the Microstructure and Mechanical Properties of Fe-Mn-Al-C Light-Weight Steels

Authors not provided

Abstract

The effects of cooling after solution heat treatment on the microstructure and mechanical properties of light-weight steels were investigated using Fe-30Mn-xAl-0.9C alloys containing 9.0-12.8 wt% Al. Lab-scale specimens (thickness: 10 mm) of the alloys were cooled by different cooling rates from -337 to -0.053 /s using water, air, and furnace cooling. As the cooling rate decreased, hardness of the alloys increased due to precipitation of -carbides. However, reduction of the cooling rate induced the growth of intergranular -carbides. This resulted in the decrease of impact absorbed energy of the alloys at room temperature, and exhibited intergranular brittle fracture behavior. The 12.8 wt% Al alloy cooled at the slowest cooling rate in particular showed the formation of -Mn. To estimate the cooling rates of large-scale slabs of light-weight steels, finite element simulations were conducted. The cooling rates at the center of the slab under air and water cooling (free convection) were calculated to be -0.049 and -0.15 /s, respectively. The results indicated that water cooling could prevent the excessive formation of -carbides/-Mn during fabrication of large-scale slabs of alloys containing an Al content lower than 10.5 wt%.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.