journal article·2012-07-05

Effects of Coiling Temperature and Carbides Behavior on Stretch-flangeability for 980 MPa Hot-rolled Steels

Namhyun Kang, Eun-Joon Chun, Ju-Seung Lee, Hyounghyeop Do, Seong-Ju Kim, Yoon-Suk CHoi, Yong-Ho Park

Publisher page

Abstract

To analyze the factors on stretch-flangeability for 980 MPa-grade hot-rolled steels, two types of steels (Fe-Cr and Fe-Mo) were manufactured by hot-rolling. Manufactured steels at the low coiling temperature, such as 400 and 500°C, had poor stretch-flangeability due to un-uniformly distributed carbides and a large deviation of interphase hardness. However, when the coiling temperature was set at 650°C with Fe-Cr steel, 998 MPa of ultimate tensile strength, 19% of total elongation and 65% of the hole expanding ratio were achieved by microstructural constituents of polygonal ferrite (PF) and granular ferrite (GF) dispersed with fine carbides (<50 nm). Therefore, the material to attain 980 MPa with superior formability was the FeCr steel that was precipitation-hardened in polygonal ferrite and granular ferrite at the coiling temperature 650°C. (Received March 9, 2012)
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References