Effects of Tempering Condition on the Microstructure and Mechanical Properties of 30MnB5 Hot-Stamping steel
Source abstract
Abstract
The effects of tempering condition on the microstructure and mechanical properties of 30MnB5 hot stamping steel were investigated in this study. Before the tempering, hot-stamped 30MnB5 steel was composed of only -martensite microstructure without precipitates. After the tempering at 180 o C for 120 min, nano-sized -carbides were precipitated in the -martensite laths. After tempering at 250 o C for 60 min, cementite was precipitated along the -martensite lath boundaries. The cementite was also observed in the specimens tempered at 350 o C for 30 min and 450 o C for 6 min, respectively. The globular -ferrite appeared at 350 o C-30 min tempering, and the volume fraction of -ferrite increased when the tempering temperature was increased. The yield strength increased after tempering, and it reached a peak with the tempering condition of 180 o C-120 min, due to the nano-sized precipitates in the martensite lath. After the tempering, the steel's ultimate tensile strength (UTS) was decreased due to the reduction in dislocation density and C segregation to lath boundaries. The highest elongation was observed at the 180 o C-120 min tempering condition, due to the reduction of residual stress, and the lack of precipitates along the lath boundaries. The 180 o C-120 min tempering condition was considered to have outstanding crash performance, according to toughness and anti-intrusion calculation results. In drop tower crash tests, the 30MnB5 door impact beam tempered at 180 o C for 120 min showed better crash performance compared to a 22MnB5 door impact beam.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. 10.1016/S1644-9665(12)60197-610.1016/S1644-9665(12)60197-6 ↗
2. Bouaziz · 2013 · 937
3. Lee · 2004 · 117
4. 10.3365/KJMM.2014.52.2.11310.3365/KJMM.2014.52.2.113 ↗
5. 10.1007/s11661-009-0124-710.1007/s11661-009-0124-7 ↗
6. 10.1016/j.actamat.2011.12.00410.1016/j.actamat.2011.12.004 ↗
7. 10.1007/s12540-016-5631-710.1007/s12540-016-5631-7 ↗
8. 10.1007/BF0258615710.1007/BF02586157 ↗
9. Kang · 2012 · 883
10. 10.1016/j.ijmecsci.2009.09.03010.1016/j.ijmecsci.2009.09.030 ↗
11. 10.1016/j.jmatprotec.2010.07.01910.1016/j.jmatprotec.2010.07.019 ↗
12. 10.1016/j.msea.2012.01.01810.1016/j.msea.2012.01.018 ↗
13. 10.3365/KJMM.2016.54.1.0810.3365/KJMM.2016.54.1.08 ↗
14. 10.1007/s11661-012-1316-010.1007/s11661-012-1316-0 ↗
15. Wang · 2016 · 488
16. 10.1016/j.msea.2014.11.00510.1016/j.msea.2014.11.005 ↗
17. Crafts · 1947 · 222
18. Krauss · 1999
19. 10.1016/j.msea.2016.07.09210.1016/j.msea.2016.07.092 ↗
20. 10.1007/BF0265220810.1007/BF02652208 ↗
21. 10.1007/BF0265986010.1007/BF02659860 ↗
22. 10.1080/02670836.2017.134201810.1080/02670836.2017.1342018 ↗
23. 10.3724/SP.J.1037.2012.0045110.3724/SP.J.1037.2012.00451 ↗
24. 10.1016/j.jmatprotec.2017.08.02710.1016/j.jmatprotec.2017.08.027 ↗
25. 10.1007/s11661-012-1546-110.1007/s11661-012-1546-1 ↗
26. 10.1016/j.msea.2016.08.09610.1016/j.msea.2016.08.096 ↗
27. 10.1007/BF0264243610.1007/BF02642436 ↗
28. 10.1007/s11661-008-9756-210.1007/s11661-008-9756-2 ↗
29. 10.1007/BF0264704110.1007/BF02647041 ↗
30. 10.1007/BF0264403710.1007/BF02644037 ↗
31. 10.1016/j.msea.2011.10.05610.1016/j.msea.2011.10.056 ↗
32. 10.1016/j.msea.2009.05.04610.1016/j.msea.2009.05.046 ↗
33. 10.1016/j.actamat.2014.07.00510.1016/j.actamat.2014.07.005 ↗
34. Bhadeshia · 1995 · 72
35. 10.1016/j.matchar.2007.02.01210.1016/j.matchar.2007.02.012 ↗
36. 10.1016/S0924-0136(98)00351-310.1016/S0924-0136(98)00351-3 ↗