Yttria-stabilised tetragonal zirconia polycrystals (YTZP) are well recognised for the excellent combination of bending strength and transformation toughness [1]. The modest hardness however restricts their use for tribological applications. Since the discovery of transformation toughening three decades ago [2], research efforts have been put forward to incorporate non-oxide hard phases such as borides, carbides, nitrides and carbonitrides into a zirconia matrix in order to increase the hardness of Y-TZP monoliths [3–5]. Titanium diboride (TiB2), for example, has an excellent hardness, but poor fracture toughness and a moderate bending strength [6]. Therefore, TZP–TiB2 composites are considered to be promising composite materials for tribological applications. In this communication, the microstructure and properties of hot pressed yttria-stabilised tetragonal zirconia polycrystalline (Y-TZP) ceramics with 30 vol% TiB2 particles are reported. The ZrO2 starting powders were of the yttria-coated monoclinic ZrO2 type. Commercial 2.8 mol% Y2O3-coated ZrO2 powder (Tioxide grade YZ5N (Tio2.8)) and in-house processed yttria-coated zirconia starting powders (YZ grades) were used. The Tio2.8 powder is prepared by co-milling high purity yttria and plasma derived monoclinic zirconia powders [7]. The YZ grade powders were prepared by a chemical suspension coating technique [8, 9], in which a well-defined solution of Y2O3 (Aldrich Chemical Company) in HNO3 (65 vol%) is mixed with monoclinic zirconia powder (Tosoh grade TZ-O) using Y-TZP milling balls (Tosoh grade TZ-3Y) in polyethylene containers for 48 hrs. After drying in a rotary evaporator, the powder was subsequently calcined in an alumina crucible in air at 800 ◦C for 1 hr to obtain yttria-coated zirconia powders with 2.5 and 2.75 mol% stabilizer, respectively, denoted as YZ2.5 and YZ2.75. H. C. Starck TiB2 powder grade F, with an average particle size <0.9 μm, and grade E, with an average particle size of 1.5–2 μm, were used. 50–100 g of powder with a ZrO2/TiB2 volume ratio of 70/30, was mixed for 24 hrs using alumina milling balls and subsequently dried. The dry powder mixture was hot pressed (FCT-Systeme, Rauenstein, Germany) at 1450 ◦C in vacuum (≈0.1 Pa) for 1 hr at 28 MPa. The final thickness of the hot pressed sample was 5 mm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. R. H. J. Hannink, P. M. Kelly and B. C. Muddle, J. Amer. Ceram. Soc. 83(2000) 461.10.1111/j.1151-2916.2000.tb01221.x ↗
2. R. C. Garvie, R. H. Hannink and R. T. Pascoe, Nature 258(1975) 703.10.1038/258703a0 ↗
3. R. Telle and G. Petzow, Mater. Sci. Engng. A105/106(1988) 97.10.1016/0025-5416(88)90485-5 ↗
4. T. Watanabe and K. Shorbu, J. Amer. Ceram. Soc. 68(1985) C34.10.1111/j.1151-2916.1985.tb15247.x ↗
5. B. Basu, J. Vleugels and O. Van Der Biest, J. Alloys Comp. 334(1-2) (2002) 200.10.1016/S0925-8388(01)01742-X ↗
6. R. A. Cutler, "Engineering Properties of Borides, Engineered Materials Handbook", Vol. 4, Ceramics and Glasses, ASM International (The Materials Information Society, USA, 1991) p. 787.
7. R. Singh, C. Gill, S. Lawson and G. P. Dransfield, J. Mater. Sci. 31(1996) 6055.10.1007/BF01152158 ↗
8. Z. X. Yuan, J. Vleugels and O. Van Der Biest, J. Mater. Sci. Lett. 19(2000) 359.10.1023/A:1006714032131 ↗
9. J. Vleugels, Z. X. Yuan and O. Van Der Biest, J. Europ Ceram. Soc. 22(6) (2002) 873.10.1016/S0955-2219(01)00389-2 ↗
10. G. R. Anstis, P. Chantikul, B. R. Lawn and D. B. Marshall, J. Amer. Ceram. Soc. 64(1981) 533.10.1111/j.1151-2916.1981.tb10320.x ↗
11. J. Vleugels and O. Van Der Biest, ibid. 82(1999) 2717.10.1111/j.1151-2916.1999.tb02147.x ↗
12. B. Basu, J. Vleugels and O. Van Der Biest, J. Eur. Ceram. Soc. 24(7) (2004) 2031.10.1016/S0955-2219(03)00355-8 ↗
13. K. T. Faber and A. G. Evans, Acta Metall. 31(1983) 565.10.1016/0001-6160(83)90046-9 ↗
14. M. Johnsson and L. Eriksson, Z. Metallkd. 89(1998) 478.
15. H. Schubert, J. Amer. Ceram. Soc. 69(1986) 270.10.1111/j.1151-2916.1986.tb07424.x ↗
16. M. Taya, S. Hayashi, A. S. Kobayashi and H. S. Yon, ibid. 73(1990) 1382.10.1111/j.1151-2916.1990.tb05209.x ↗