Effect of atmosphere on superplastic deformation behavior in nanocrystalline liquid-phase-sintered silicon carbide with Al2O3-Y2O3 additions

T. Nagano, H. Gu, G.-D. Zhan, M. Mitomo

Journal of Materials Science· Volume 37· Issue 20
Publisher page

Abstract

Nanocrystalline β-SiC with additions of 5.135 wt% Al2O3 and 3.867 wt% Y2O3 was subjected to tensile deformation in order to study its microstructural behavior under the dynamic process. The liquid-phase-sintered body had a relative density of >95% and an average grain size of 190 nm. Tension tests were conducted at initial strain rates range from 3 × 10−4 to 2 × 10−5 s−1, in the temperature range 1873–2048 K, in both argon and N2 atmospheres. Although grain-boundary liquids formed by the additions vaporized concurrently with the decomposition of SiC and grain growth, the maximum tensile elongation of 60% was achieved in argon. The grain-boundary amorphous phase formed a crystalline phase during testing in an N2 atmosphere and fracture occurred at <8% elongation. Grain-boundary sliding was still the dominant mechanism for deformation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. S. Prochazka, Special Ceramics 6, edited by P. Popper (British Ceramic Research Association, Stoke-on-Trent, 1975) p. 171.
2. K. Suzuki, Rep.Res.Lab., Asahi Glass Co., Ltd. 36 (1986) 25.
3. M. Omori and H. Takei, J.Amer.Ceram.Soc. 65 (1982) C-92.10.1111/j.1151-2916.1982.tb10460.x ↗
4. M. Mitomo, Y.-W. Kim and H. Hirotsuru, J.Mater. Res. 11 (1996) 1601.10.1557/JMR.1996.0200 ↗
5. T. Nagano, S. Honda, F. Wakai and M. Mitomo, in Proc. of 6th Int'l Symp. on Ceramic Materials and Components for Engines, Arita, October 1997, edited by K. Niihara, S. Hirano, S. Kanzaki, K. Komeya and K. Morinaga (Japan Fine Ceramics Association, Tokyo, 1998) p. 707.
6. Idem., in Proc. of Superplasticity & Superplastic Forming 1998, San Antonio, February 1998, edited by A. K. Ghosh and T. R. Bieler (The Minerals, Metals & Materials Society, Warrendale, 1998) p. 247.
7. T. Nagano, H. Gu, K. Kaneko, G.-D. Zhan and M. Mitomo, J.Amer.Ceram.Soc. 84 (2001) 2045.10.1111/j.1151-2916.2001.tb00956.x ↗
8. T. Nagano, H. Gu, Y. Shinoda, M. Mitomo and F. Wakai, Ceramics: Getting into The 2000's, Part D, Florence, June 1998, edited by P. Vincenzini (Techna, Faenza, 1999) p. 25.
9. T. Nagano, H. Gu, Y. Shinoda, G.-D. Zhan, M. Mitomo and F. Wakai, Mater.Sci.Forum 304/306 (1999) 507.10.4028/www.scientific.net/MSF.304-306.507 ↗
10. N. Kondo, F. Wakai, M. Yamagiwa, T. Nishioka and A. Yamakawa, Material Science and EngineeringAA206 (1996) 45.10.1016/0921-5093(95)09984-0 ↗
11. T. Nagano, K. Kaneko, G.-D. Zhan and M. Mitomo, J.Amer.Ceram.Soc. 83 (2000) 2781.10.1111/j.1151-2916.2000.tb01631.x ↗
12. H.-W. Jun, H.-W. Lee, G.-H. Kim, H. Song and B.-H. Kim, Ceram.Eng.Sci.Proc. 18 (1997) 487.10.1002/9780470294444.ch57 ↗
13. I. D. Prendergast, D. W. Budworth and N. H. Brett, Trans.Brit.Ceram.Soc. 71 (1972) 31.
14. H. Tanaka and N. Iyi, J.Ceram.Soc.Jpn. 101 (1993) 1313.10.2109/jcersj.101.1313 ↗
15. T. Nagano, K. Kaneko and H. Kodama, in Proc. of The Third Pacific Rim Int'l Conference on Advanced Materials and Processing (PRICM3), edited byM.A. Imam, R. DeNale, S. Hanada, Z. Zhong and D. N. Lee (The Minerals, Metals & Materials Society, Warrendale, 1998) p. 1897.
16. T. Grande, H. Sommerset, E. Hagen, K. Wiik and M.-A. Einarsrud, J.Amer.Ceram.Soc. 80 (1997) 1047.10.1111/j.1151-2916.1997.tb02945.x ↗
17. W.-S. Seo, C.-H. Pai, K. Koumoto and H. Yanagida, J.Ceram.Soc.Japan 99 (1991) 443.10.2109/jcersj.99.443 ↗
18. H. O. Mulfinger, J.Amer.Ceram.Soc. 49 (1966) 462.10.1111/j.1151-2916.1966.tb13300.x ↗
19. S.-L. Hwang, P. F Becher and H.-T. Lin, ibid.80 (1997) 329.10.1111/j.1151-2916.1997.tb02834.x ↗