Surface repair of porous and damaged alumina bodies using carboxylate-alumoxane nanoparticles
Source abstract
Abstract
Aqueous solutions of acetate-functionalized alumina nanoparticles (A-alumoxane), with an average particle size of 28 nm, have been used as alumina precursors for the surface infiltration and repair of porous and/or damaged alumina surfaces. SEM and AFM measurements indicate that treatment with a 1 wt% solution results in a reduction of surface roughness from >0.6 μm to ≈100 nm for surface pores in the 100 nm to 1 μm range. The use of 6 wt% solutions gives better infiltration repair for 50 μm features, but surface cracking is observed. The surface hardness of the porous alumina substrate is increased upon infiltration. No spallation of the surface infiltration layer is observed after indentation measurements and grain dislodgment is overcome.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Anodic Oxide Films and Nanostructures · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. W. D. KINGERY, H. K. BOWEN and D. R. UHLMANN, “Introduction to Ceramics,” 2nd ed. (Wiley, New York, 1976) ch. 1.
2. D. W. RICHERSON, “Modern Ceramic Engineering” (Marcel Dekker, New York, 1992) p.373.
3. J. A. MANGELS and G. L. MESSING (eds.), “Advances in Ceramics,” Vol.9 (American Ceramic Society, Westville, OH, 1984).
4. D. VOLTZKE and H.-P. ABICHT, J. Mater. Sci. Lett. 19 (2000) 1951.10.1023/A:1006788105990 ↗
5. L.-S. CHEN, S.-L. FU and W.-K. HUANG, Jpn. J. Appl. Phys., Part 1 39 (2000) 5209.10.1143/JJAP.39.5209 ↗
6. H. F. LOPEZ and W. PHOOMIPHAKDEEPHAN, J. Mater. Sci. 35 (2000) 5995.10.1023/A:1026746927762 ↗
7. H. H. K. XU and S. JAHANMIRibid. 30 (1995) 2235.10.1007/BF01184566 ↗
8. R. L. CALLENDER, C. J. HARLAN, N. M. SHAPIRO, C. D. JONES, D. L. CALLAHAN, M. R. WIESNER, D. B. MACQUEEN, R. COOK and A. R. BARRON, Chem. Mater. 9 (1997) 2421.10.1021/cm9703684 ↗
9. D. R. GABE, “Coatings for Protection” (Institution of Production Engineers, London, 1983).
10. I. LEE, J. Mater. Sci. Lett. 20 (2001) 223.10.1023/A:1006790416275 ↗
11. I. B. INWANG, I. J. MCCOLM and A. WRONSKI, J. Mater. Sci. 36 (2001) 1823.10.1023/A:1017593129519 ↗
12. R. L. CALLENDER and A. R. BARRON, J. Mater. Res. 15 (2000) 2228.10.1557/JMR.2000.0320 ↗
13. A. R. KENNEDY, J. D. WOOD and B. M. WEAGER, J. Mater. Sci. 35 (2000) 2909.10.1023/A:1004714407371 ↗
14. C. KAWAI and J.-J. PARK, J. Mater. Sci. Lett.20 (2001) 385.10.1023/A:1006735130117 ↗
15. A. C. ADAMS and C. D. CAPIO, J. Electrochem. Soc. 128 (1981) 2630.10.1149/1.2127317 ↗
16. P. RENDTEL, F. WAGNER, R. JANSSEN and N. CLAUSSEN, Mater. Sci. Forum 308-311 (1999) 181.10.4028/www.scientific.net/MSF.308-311.181 ↗
17. A. N. MACINNES, A. R. BARRON, R. S. SOMAN and T. R. GILBERT,J. Amer. Ceram. Soc. 73 (1990) 3696.10.1111/j.1151-2916.1990.tb04278.x ↗
18. C. T. VOGELSON and A. R. BARRON, J. Non-Cryst. Solids, in press.
19. C. J. HARLAN, A. KAREIVA, D. B. MACQUEEN, R. COOK and A. R. BARRON, Adv. Mater. 9 (1997) 68.10.1002/adma.19970090116 ↗
20. R. L. CALLENDER and A. R. BARRON, J. Amer. Ceram. Soc. 83 (2000) 1777.10.1111/j.1151-2916.2000.tb01464.x ↗
21. K. A. DEFRIEND and A. R. BARRON, submitted.
22. C. D. JONES, M. FIDALGO, M. R. WIESNER and A. R. BARRON, J. Membrane Sci. 193 (2001) 175.10.1016/S0376-7388(01)00490-2 ↗
23. R. L. CALLENDER and A. R. BARRON, J. Mater. Res. 15 (2000)2228.10.1557/JMR.2000.0320 ↗
24. Idem., J. Mater. Sci. 36 (2001) 4977.10.1023/A:1011825412312 ↗
25. C. D. JONES, D. A. BAILEY, M. R. WIESNER and A. R. BARRON, in 9th CIMTEC-World Ceramics Congress, Ceramics Getting into the 2000–Part D (1999) p. 413.