Microstructure of brazed joints between mechanically metallized Si3N4 and stainless steel
Source abstract
Abstract
Brazing has been increasingly used to join metals to advanced ceramics. Brazing covalent materials requires either the use of active filler alloys or the previous metallization of the surface. To that end, a new and simple mechanical technique has been applied to metallize advanced ceramics, thus avoiding the use of costly Ti-based active filler alloys. The mechanical metallization of Si3N4 with Ti was employed as an alternative route to deposit active metallic films prior to brazing with stainless steel using 72% Ag--28% Cu or 82% Au—18% Ni eutectic alloys. The brazing temperatures were set to 40°C or 75°C above the eutectic temperature of each filler alloy. Ti-films of average thickness 4 μm produced adequate spreading of both filler alloys onto Si3N4 substrates, which were subsequently brazed to stainless steel. The interface of Si3N4/310 stainless steel basically consisted of a reaction layer, a precipitation zone and an eutectic microconstituent. Mechanically sound and vacuum-tight joints were obtained, especially upon brazing at relatively lower temperatures. Increasing the brazing temperature resulted in thermal cracking of the Si3N4, possibly due to increased thermal stress.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. A. E. MARTINELLI, Ph.D. thesis, McGill University, 1996.
2. H. OHNABE, S. MASAKI, M. ONOZUKA, K. MIYAHARA and T. SASA, Composites Part A: Applies Science and Manufacturing 30 (1999) 489.10.1016/S1359-835X(98)00139-0 ↗
3. J. A. CHEDIAK, The American Ceramic Society Bulletin 75(1) (1996) 52.
4. M. PAULASTO and J. K. KIVILAHTI, Scripta Metallurgica et Materialia 32(8) (1995) 1209.10.1016/0956-716X(95)00127-H ↗
5. G. CHAUMAT, B. DREVET and L. VERNIER, Journal of the European Ceramic Society 17 (1997) 1925.10.1016/S0955-2219(97)00059-9 ↗
6. L. MARTENS, W. TILLMANN, E. LUGSCHEIDER, G. ZIEGLER, Journal of Materials Processing Technology 58 (1996) 13.10.1016/0924-0136(95)02103-5 ↗
7. A. RABINKIN and O. BOTSTEIN, Materials Science and Engineering A 188 (1994) 305.10.1016/0921-5093(94)90386-7 ↗
8. E. LUGSCHEIDER and W. TILLMANN, Materials & Manufacturing Processes 8(2) (1993) 219.10.1080/10426919308934826 ↗
9. G. ELSSNER and G. PETZOW, ISIJ International 30(12) (1990) 1011.10.2355/isijinternational.30.1011 ↗
10. DIN 8505 T1 “Löten; Allgemeines, Begriffe” (Mai 1979) und DIN 8505 T2, Löten; Einteilung der Verfahren, Begriffe (Mai 1979).
11. R. M. NASCIMENTO, A. E. MARTINELLI and A. J. A. BUSCHINELLI, Cerâmica 49(312) (2003) 178.10.1590/S0366-69132003000400002 ↗
12. G. KÖHLER, A. PALIEGE, R. EBERHARDT, R. PALIEGE and R. HELLMICH, in Proceedings of the Hart- und Hochtemperaturlöten: Vorträge des gleichnamigen 9. Dortmunder Hochschulkolloquiums. DVS—Berichte band. 132 (1990) 12.
13. WELDING HANDBOOK, American Welding Society, 7a Ed. Vol. 2, 1978.
14. V. A. GREENHUT, edited by P. kumar and V. A. Greenhut, The Minerals, Metals & Materials Society, 1991 p. 103.
15. R. LISON, Patent P.T, 1.1481, (1997) Germany.
16. R. M. NASCIMENTO, A. E. MARTINELLI, A. J. A. BUSCHINELLI, E. LUGSCHEIDER and E. SIGISMUND. Welding and Cutting 3(2) (2004) 96.
17. R. M. NASCIMENTO, Ph.D thesis, UFSC, 2001.
18. R. M. NASCIMENTO, A. J. A. BUSCHINELLI, A. E. MARTINELLI, E. SIGISMUND, J. REMMEL, U. REISGEN and E. LUGSCHEIDER, in Proceedings of the 6th International Conference on Joining Ceramics, Glass and Metal, Munich/Germany, Oct. 2002, p. 58.
19. ASM International, in “Phase Diagrams of Ternary Boron Nitride and Silicon Nitride Systems,” 1992 edited by P. Rogl and J. C. Schuster, p. 198.
20. J. LEMUS and R. A. L. DREW, Materials Science and Engineering A 352 (2003) 169.10.1016/S0921-5093(02)00892-4 ↗