A constitutive and microstructural study for optimizing the Al2O3/Al composite in hot forming processes

B. M. Shi, X. Bian, Y. N. Zan, D. Wang, Q. Z. Wang, B. L. Xiao, Z. Y. Ma

Journal of Materials Science· Volume 60· Issue 32
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Metallurgy and Material Forming · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Balog M, Simancik F, Walcher M, Rajner W, Poletti C (2011) Extruded Al-Al2O3 composites formed in situ during consolidation of ultrafine Al powders: effect of the powder surface area. Mater Sci Eng A 529:131–13710.1016/j.msea.2011.09.006 ↗
2. Gokce A, Findik F (2008) Mechanical and physical properties of sintered aluminum powders. J Achiev Mater Manuf Eng 30(2):157–164.
3. Zan Y, Lei X, Zhang J, Wang D, Wang Q, Xiao B, Ma Z (2022) Superb strengthening effect of net-like distributed amorphous Al2O3 on creep resistance of (B4C+Al2O3)/Al neutron-absorbing materials. Acta Metall Sin (Engl Lett) 35(12):2007–201310.1007/s40195-022-01396-5 ↗
4. Gao D, Shen Z, Chen K, Zhou X, Liu H, Wang J, Li Y, Liu Z, Deng H, Wang W, Zeng X (2024) Review of progress in calculation and simulation of high-temperature oxidation. Prog Mater Sci 147:10134810.1016/j.pmatsci.2024.101348 ↗
5. Shen Z, Zhang J, Wu S, Luo X, Jenkins BM, Moody MP, Lozano-Perez S, Zeng X (2022) Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam. Acta Mater 226:11763410.1016/j.actamat.2022.117634 ↗
6. Chen Y, Ma S, Ju J, Chen K, Wang J, Shen Z, Zeng X (2025) Phase transformation-mediated high-temperature oxidation in an AlCrFeCoNi2.1 EHEA alloy at elevated temperature. Corros Sci 245:11267410.1016/j.corsci.2025.112674 ↗
7. Li S, Tong Z, Cheng S, Shen Z, Sun L, Gong A, Long B, Qin B, Wang Y, Lu S, Sun J (2025) Resistance to embrittlement in ferritic/martensitic steel with TaWVCr coating in oxygen-saturated lead-bismuth eutectic at 350 °C. Surf Coat Technol 497:13172910.1016/j.surfcoat.2025.131729 ↗
8. Zhou Y, Liu J, Ferreirós PA, Shang X, Chen K, Que Z, Shen Z, Yu J, Zhang L (2025) Integrated effects of non-equilibrium microstructures on stress corrosion cracking susceptibility of post-treated laser powder-bed-fusion 316 L stainless steels. Corros Sci 22:11297410.1016/j.corsci.2025.112974 ↗
9. Kubota M, Wu X, Xu W, Xia K (2010) Mechanical properties of bulk aluminium consolidated from mechanically milled particles by back pressure equal channel angular pressing. Mater Sci Eng A 527:6533–653610.1016/j.msea.2010.06.088 ↗
10. Balog M, Simancik F, Bajana O, Requena G (2009) ECAP vs. direct extrusion-techniques for consolidation of ultra-fine Al particles. Mater Sci Eng A 504:1–710.1016/j.msea.2008.12.014 ↗
11. Balog M, Krizik P, Yan M, Simancik F, Schaffer G, Qian M (2013) SAP-like ultrafine-grained Al composites dispersion strengthened with nanometric. AlN Mater Sci Eng A 588:181–18710.1016/j.msea.2013.09.027 ↗
12. Jiang L, Li Z, Fan G, Zhang D (2011) A flake powder metallurgy approach to Al2O3/Al biomimetic nanolaminated composites with enhanced ductility. Scr Mater 65:412–41510.1016/j.scriptamat.2011.05.022 ↗
13. Casati R, Fabrizi A, Timelli G, Tuissi A, Vedani M (2016) Microstructural and mechanical properties of Al-based composites reinforced with in-situ and ex-situ Al2O3 nanoparticles. Adv Eng Mater 18:550–55810.1002/adem.201500297 ↗
14. Balog M, Hu T, Krizik P et al (2015) On the thermal stability of ultrafine-grained Al stabilized by in-situ amorphous Al2O3 network. Mater Sci Eng A 648:61–7110.1016/j.msea.2015.09.037 ↗
15. Balog M, Poletti C, Simancik F, Walcher M, Rajner W (2011) The effect of native Al2O3 skin disruption on properties of fine Al powder compacts. J Alloys Compd 509:S235–S23810.1016/j.jallcom.2010.12.042 ↗
16. Balog M, Simancik F, Krizik P, Nosko M, Rajner W, Walcher M, Qian M (2016) Novel ultrafine-grained aluminium metal matrix composites prepared from fine atomized Al powders. Light Met 2014:1425–1430
17. Abdous S, Derradji M, Mekhalif Z, Khiari K, Mehelli O, Cherif YB (2023) Exploring the potential of benzoxazine-based nanocomposites for lightweight neutron shielding applications. High Perform Polym 35:812–82610.1177/09540083231179114 ↗
18. Pal R, Sudhi S, Raghavan R (2019) Fabrication and evaluation of structural film adhesive using oxazolidinone modified novolac epoxy resin. J Appl Polym Sci 136:4752010.1002/app.47520 ↗
19. Vignesh S, Winowlin Jappes JT, Nagaveena S et al (2022) Development of lightweight polymer laminates for radiation shielding and electronics applications. Int J Polym Sci 2022:525252810.1155/2022/5252528 ↗
20. Feng SY, Li QL, Liu W, Shu GG, Wang X (2020) Microstructure and mechanical properties of Al-B4C composite at elevated temperature strengthened with in situ Al2O3 network. Rare Met 39:671–67910.1007/s12598-019-01279-2 ↗
21. Srivatsan TS, Lavernia EJ, Mohamed FA (1990) Strength, deformation, fracture behaviour and ductility of aluminium-lithium alloys. J Mater Sci 25:1137–1158. https://doi.org/10.1007/BF0058542010.1007/BF00585420 ↗
22. Bian X, Ma K, Liu ZY, Xiao BL, Wang QZ, Ma ZY (2024) Hot deformation behavior analysis of CNT/2009Al composite with bimodal heterostructure via constructing a new processing map. Mater Charact 212:11397910.1016/j.matchar.2024.113979 ↗
23. Ma K, Liu Z, Zhang X, Xiao B, Ma Z (2021) Fabrication of high strength carbon nanotube/7055Al composite by powder metallurgy combined with subsequent hot extrusion. Sci China Technol Sci 64:1081–109110.1007/s11431-020-1715-8 ↗
24. Xiao B, Huang Z, Ma K, Zhang X, Ma Z (2018) Research on hot deformation behaviors of discontinuously reinforced aluminum composites. Acta Metall Sin 55:59–72
25. Poletti C, Balog M, Simancik F, Degischer HP (2010) High-temperature strength of compacted sub-micrometer aluminium powder. Acta Mater 58:3781–378910.1016/j.actamat.2010.03.021 ↗
26. Liu Y, Chen W, Gu L et al (2023) Effects of hot-pressing parameters on microstructure and mechanical properties of composites synthesized by Al-TiO2 in-situ reaction. Sci China Technol Sci 66:2725–273410.1007/s11431-022-2359-5 ↗
27. Cao L, Chen B, Wan J et al (2022) Superior high-temperature tensile properties of aluminum matrix composites reinforced with carbon nanotubes. Carbon 191:403–41410.1016/j.carbon.2022.02.009 ↗
28. Kim SS, Haynes MJ, Gangloff RP (1995) Localized deformation and elevated-temperature fracture of submicron-grain aluminum with dispersoids. Mater Sci Eng A 203:256–27110.1016/0921-5093(95)09844-5 ↗
29. Spigarelli S, Evangelista E, Cerri E, Langdon TG (2001) Constitutive equations for hot deformation of an Al-6061/20%Al2O3 composite. Mater Sci Eng A 319:721–72510.1016/S0921-5093(01)01071-1 ↗
30. Li S, Luo T, Chao Z et al (2024) A review of dynamic mechanical behavior and the constitutive models of aluminum matrix composites. Materials 17:187910.3390/ma17081879 ↗
31. Zhou L, Cui C, Wang QZ, Li C, Xiao BL, Ma ZY (2018) Constitutive equation and model validation for a 31 vol.% B4Cp/6061Al composite during hot compression. J Mater Sci Technol 34:1730–173810.1016/j.jmst.2018.02.001 ↗
32. Jia C, Xu Z, Li Y et al (2024) Hot deformation behavior and microstructural evolution of an in situ 2 wt.% TiB2-reinforced 6061 Al matrix composite. J Mater Eng Perform 33:3309–331910.1007/s11665-023-08226-4 ↗
33. Liu P, Hao S, Xie J (2024) Hot compressive deformation characteristics of Al-9.3Zn-2.4Mg-1.1Cu Alloy. J. Wuhan Univ. Technol. Mater Sci Ed 39:754–765
34. Cho CH, Kim DO, Son K, Park HS (2023) Relationship between hot workability and texture evolution in an Al-Zn-Mg-Cu alloy under hot compressive stress mode. J Mater Sci 58:16537–16549. https://doi.org/10.1007/s10853-023-09081-310.1007/s10853-023-09081-3 ↗
35. Xue W, Chao Z, Han H et al (2024) Research on low flow stress and quantitative DRX analysis in B4C/Al composites with interfacial amorphous B2O3 layer. Compos B 272:11122610.1016/j.compositesb.2024.111226 ↗
36. Yang H, Qian Z, Sun P, Yang H, Zheng S, Li M (2024) Flow behavior and activation energy evolution of 7075–T6 Al alloy during hot deformation. Jom 76:3679–369310.1007/s11837-024-06567-6 ↗
37. Sun W, Zhang Y, Yu F et al (2024) Research on hot deformation rheological stress of Al-Mg-Si-Mn-Sc aluminium alloy. Materials 17:315910.3390/ma17133159 ↗
38. Wang Z, Wang A, Xie J, Liu P (2020) Hot Deformation behavior and strain-compensated constitutive equation of nano-sized SiC particle-reinforced Al-Si matrix composites. Materials 13:181210.3390/ma13081812 ↗
39. Wang Z, Li K, Luo T et al (2024) Hot deformation mechanism of a rapidly-solidified Al-Zn-Mg-Cu-Zr alloy. J Mater Res Technol 31:2424–243410.1016/j.jmrt.2024.06.216 ↗
40. Kim SK, Koo SH, Cho H, Ha SH (2024) Hot deformation constitutive analysis and processing maps of ultrasonic melt treated A5052 alloy. Materials 17:318210.3390/ma17133182 ↗
41. Zhang Z, Cong H, Yin Z et al (2024) Thermal deformation behavior and microstructural evolution of the rapidly-solidified Al-Zn-Mg-Cu alloy in hot isostatic pressing state. J Mater Res Technol 30:5927–593910.1016/j.jmrt.2024.04.235 ↗
42. Wang H, Yin D, Zhao MC, Tian Y, Atrens A (2023) The hot deformation characteristics and the associated microstructural evolution of an Al-Cu-Li-Zn alloy studied by constitutive equations and processing maps. J Mater Res Technol 27:401–41810.1016/j.jmrt.2023.09.222 ↗
43. Zener C, Hollomon JH (1944) Effect of strain rate upon plastic flow of steel. J Appl Phys 15:22–3210.1063/1.1707363 ↗
44. Wang H, Wang W, Lyu P, Wu S (2024) Hot deformation behavior of free-Al 2.43 wt.% Si electrical steel strip produced by twin-roll strip casting and its effect on microstructure and texture. Materials 17:315210.3390/ma17133152 ↗
45. Shiming H, Pengru L, Jingpei X (2023) Microstructure evolution and dynamic recrystallization nucleation mechanism of medium volume fraction SiCp/Al composite during hot deformation. J Mater Res Technol 23:919–93010.1016/j.jmrt.2023.01.033 ↗
46. Ma M, Zhang K, Li X, Li Y, Zhang K (2008) Hot deformation behavior of rare earth magnesium alloy without pre-homogenization treatment. Trans Nonferrous Met Soc China 18:132–13910.1016/S1003-6326(10)60189-6 ↗
47. Gurgel MAM, Leite DNF, Moreira LP et al (2024) Flow stress behavior, constitutive modeling, processing map and microstructure evolution in hot deformation of Fe-7.1Al-0.7Mn-0.4C-0.3Nb alloy. J Mater Res Technol 30:7145–715910.1016/j.jmrt.2024.05.063 ↗
48. Li W, Li H, Wang Z, Zheng Z (2011) Constitutive equations for high temperature flow stress prediction of Al–14Cu–7Ce alloy. Mater Sci Eng A 528:4098–410310.1016/j.msea.2011.01.076 ↗
49. Ruano OA, Wadsworth J, Sherby OD (2003) Deformation of fine-grained alumina by grain boundary sliding accommodated by slip. Acta Mater 51:3617–363410.1016/S1359-6454(03)00180-0 ↗
50. Sun P, Huang R, Yang H, Zhang Y, Zheng S, Li M (2024) Hot compression behavior and processing map of homogenized Al-Mg-Si alloy. J Mater Eng Perform 34:7641–765710.1007/s11665-024-09717-8 ↗
51. Zhang J, Han B, Shen G et al (2024) Hot deformation behavior and microstructural evolution of a new type of 7xxx Al alloy. Mater Today Commun 41:11021810.1016/j.mtcomm.2024.110218 ↗
52. Zhou X, Le Q, Hu C et al (2023) Study on the hot deformation behavior of a novel multi-element synergistic strengthening Mg-Al-Ca-Mn-Zn-Sn alloy. J Alloys Compd 953:17015610.1016/j.jallcom.2023.170156 ↗
53. Murty SN, Rao BN, Kashyap B (2003) On the hot working characteristics of 6061Al-SiC and 6061-Al2O3 particulate reinforced metal matrix composites. Compos Sci Technol 63:119–13510.1016/S0266-3538(02)00197-5 ↗
54. Alaneme KK, Babalola SA, Bodunrin MO, Chown LH, Okotete EA, Maledi NB (2021) Hot deformation of nickel particles reinforced aluminium based composites: flow behaviour, microstructural evolution and processing map analyses. Mater Res Express 8:01651010.1088/2053-1591/abd5a3 ↗
55. Ma Z, Shu X, Xu H et al (2024) Hot compression deformation behavior and microstructure evolution of Al-0.5Mg-0.4Si alloy. J Alloys Compd 1002:17528210.1016/j.jallcom.2024.175282 ↗
56. Hao S, Xie J, Wang A, Wang W, Li J, Sun H (2014) Hot deformation behaviors of 35% SiCp/2024Al metal matrix composites. Trans Nonferrous Met Soc China 24:2468–247410.1016/S1003-6326(14)63372-0 ↗
57. Han J, Guo F, Liu J (2017) Recrystallization induced by subgrain rotation in Pb-free BGA solder joints under thermomechanical stress. J Alloys Compd 698:706–71310.1016/j.jallcom.2016.12.281 ↗
58. Li H, Huang Y, Liu Y (2023) Dynamic recrystallization mechanisms of as-forged Al-Zn-Mg-(Cu) aluminum alloy during hot compression deformation. Mater Sci Eng, A 878:14523610.1016/j.msea.2023.145236 ↗
59. Ma K, Liu Z, Bi S, Zhang X, Xiao B, Ma Z (2021) Microstructure evolution and hot deformation behavior of carbon nanotube reinforced 2009Al composite with bimodal grain structure. J Mater Sci Technol 70:73–8210.1016/j.jmst.2020.09.003 ↗