Strong correlation between crack initiation and high cycle fatigue behavior of Ti6Al4V ELI alloy with bimodal microstructure

Xiaohui Shi, Zirui Chen, Yuqi Qiao, Zhen Jing, Junwei Qiao

Journal of Materials Science· Volume 60· Issue 16
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Fatigue and fracture mechanics · Titanium Alloys Microstructure and Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Luo XK, Dang N, Wang X (2021) The effect of laser shock peening, shot peening and their combination on the microstructure and fatigue properties of Ti–6Al–4V titanium alloy. Int J Fatigue 153:106465. https://doi.org/10.1016/j.ijfatigue.2021.10646510.1016/j.ijfatigue.2021.106465 ↗
2. Sołtysiak R, Małecka J (2018) The analysis of cyclic properties of Ti–6Al–4V titanium alloy at room and liquid nitrogen temperature. Mater Sci Eng A 734:476–484. https://doi.org/10.1016/j.msea.2018.07.07610.1016/j.msea.2018.07.076 ↗
3. Yu FL, Zhang Y, Kong C, Yu HL (2022) High strength and toughness of Ti–6Al–4V sheets via cryorolling and short-period annealing. Mater Sci Eng A 854:143766. https://doi.org/10.1016/j.msea.2022.14376610.1016/j.msea.2022.143766 ↗
4. Lavogiez C, Dureau C, Nadot Y, Villechaise P, Hémery S (2023) Crack initiation mechanisms in Ti–6Al–4V subjected to cold dwell-fatigue, low-cycle fatigue and high-cycle fatigue loadings. Acta Mater 244:118560. https://doi.org/10.1016/j.actamat.2022.11856010.1016/j.actamat.2022.118560 ↗
5. Gao T, Xue HQ, Sun ZD (2021) Effect of transformed β phase on fish-eye ductile crack initiation of a Ti–6Al–4V alloy in very high cycle fatigue regime. Mater Lett 287:129283. https://doi.org/10.1016/j.matlet.2020.12928310.1016/j.matlet.2020.129283 ↗
6. Gao T, Zhao X, Xue HQ, Sun ZD (2022) Characteristics and micromechanisms of fish-eye crack initiation of a Ti–6Al–4V alloy in very high cycle fatigue regime. J Mater Res Technol 21:3140–3153. https://doi.org/10.1016/j.jmrt.2022.10.12510.1016/j.jmrt.2022.10.125 ↗
7. Briffod F, Shiraiwa T, Enoki M, Emura S (2022) Effect of macrozones on fatigue crack initiation and propagation mechanisms in a forged ti-6Al–4V alloy under fully-reversed condition. Materialia 22:101401. https://doi.org/10.1016/j.mtla.2022.10140110.1016/j.mtla.2022.101401 ↗
8. Sun CQ, Chi WQ, Wang WJ, Duan Y (2021) Characteristic and mechanism of crack initiation and early growth of an additively manufactured Ti-6Al-4V in very high cycle fatigue regime. Int J Mech Sci 205:106591. https://doi.org/10.1016/j.ijmecsci.2021.10659110.1016/j.ijmecsci.2021.106591 ↗
9. Azgomi N, Tetteh F, Duntu SH, Yiadom SB (2021) Effect of heat treatment on the microstructural evolution and properties of 3D-printed and conventionally produced medical-grade Ti6Al4V ELI alloy. Metall Mater Trans A 52:3382–3400. https://doi.org/10.1007/s11661-021-06310-910.1007/s11661-021-06310-9 ↗
10. du Preez WB (2019) Towards qualification of additively manufactured Ti6Al4V (ELI) medical implants. JOM 71:655–661. https://doi.org/10.1007/s11837-018-3266-510.1007/s11837-018-3266-5 ↗
11. Chang C, Huang J, Yan XC, Li Q, Liu M, Deng SH, Gardan J, Bolot R, Chemkhi M, Liao HL (2020) Microstructure and mechanical deformation behavior of selective laser melted Ti6Al4V ELI alloy porous structures. Mater Lett 277:128366. https://doi.org/10.1016/j.matlet.2020.12836610.1016/j.matlet.2020.128366 ↗
12. Sorgente D, Palumbo G, Piccininni A, Guglielmi P, Tricarico L (2017) Modelling the superplastic behaviour of the Ti6Al4V-ELI by means of a numerical/experimental approach. Int J Adv Des Manuf Technol 90:1–10. https://doi.org/10.1007/s00170-016-9235-710.1007/s00170-016-9235-7 ↗
13. Gao YF, Wu CD, Peng K, Song XL, Fu YH, Chen QY, Zhang MB, Wang GL, Liu J (2021) Towards superior fatigue crack growth resistance of TC4-DT alloy by in-situ rolled wire-arc additive manufacturing. J Mater Res Technol 15:1395–1407. https://doi.org/10.1016/j.jmrt.2021.08.15210.1016/j.jmrt.2021.08.152 ↗
14. Guo P, Zhao YQ, Zeng WD, Liu JL (2015) Effect of microstructure on the fatigue crack propagation behavior of TC4-DT titanium alloy. J Mater Eng Perform 24:1865–1870. https://doi.org/10.1007/s11665-015-1465-610.1007/s11665-015-1465-6 ↗
15. Zhao YX, Yu PS, Wu LS, Zhang X, Wei PY, Zhao JH (2023) Corrosion-induced deceleration-to-acceleration of fatigue crack growth for deep-sea Ti6Al4V ELI titanium alloy. Eng Fract Mech 281:109160. https://doi.org/10.1016/j.engfracmech.2023.10916010.1016/j.engfracmech.2023.109160 ↗
16. Peng XN, Guo HZ, Wang T, Yao ZK (2012) Effects of treatments on microstructures and mechanical properties of TC4-DT titanium alloy. Mater Sci Eng A 533:55–63. https://doi.org/10.1016/j.msea.2011.11.03310.1016/j.msea.2011.11.033 ↗
17. Peng XN, Guo HZ, Shi ZF, Qin C, Zhao ZL (2013) Constitutive equations for high temperature flow stress of TC4-DT alloy incorporating strain, strain rate and temperature. Mater Des 50:198–206. https://doi.org/10.1016/j.matdes.2013.03.00910.1016/j.matdes.2013.03.009 ↗
18. Lu W, Shi YW, Li XY, Lei YP (2013) Correlation between tensile strength and hardness of electron beam welded TC4-DT joints. J Mater Eng Perform 22:1694–1700. https://doi.org/10.1007/s11665-012-0469-810.1007/s11665-012-0469-8 ↗
19. Chafino JA, Yamanaka K, Mercier F, Rivory P, Balvay S, Hartmann DJ, Chiba A, Fabregue D (2019) The influence of temperature during water-quench rapid heat treatment on the microstructure, mechanical properties and biocompatibility of Ti6Al4V ELI alloy. J Mech Behav Biomed Mater 96:144–151. https://doi.org/10.1016/j.jmbbm.2019.04.02410.1016/j.jmbbm.2019.04.024 ↗
20. Fu PF, Mao ZY, Zuo CJ, Wang YJ, Wang CM (2014) Microstructures and fatigue properties of electron beam welds with beam oscillation for heavy section TC4-DT alloy. Chin J Aeronaut 27:1015–1021. https://doi.org/10.1016/j.cja.2014.03.02010.1016/j.cja.2014.03.020 ↗
21. Sun PF, Qu SG, Duan CF, Zhong H, Li FL, Liang L, Li XQ, Zhang ZF (2024) Strategy and mechanism to improve the fatigue properties of Ti6Al4V ELI alloy by microstructure modulation combined with surface strengthening process. Mater Sci Eng A 892:146005. https://doi.org/10.1016/j.msea.2023.14600510.1016/j.msea.2023.146005 ↗
22. Sun PF, Qu SG, Duan CF, Hu XF, Li XQ (2024) Improving the high cycle fatigue property of Ti6Al4V ELI alloy by optimizing the surface integrity through electric pulse combined with ultrasonic surface rolling process. J Mater Sci Technol 170:103–121. https://doi.org/10.1016/j.jmst.2023.06.02910.1016/j.jmst.2023.06.029 ↗
23. Hall JA (1997) Fatigue crack initiation in alpha-beta titanium alloys. Int J Fatigue 19:23–37. https://doi.org/10.1016/S0142-1123(97)00047-910.1016/S0142-1123(97)00047-9 ↗
24. Irwin GR (1962) Crack extension force for a part-through crack in a plate. J Appl Mech 29:651–654. https://doi.org/10.1115/1.364064910.1115/1.3640649 ↗
25. Shah RC, Kobayashi AS (1973) Stress intensity factors for an elliptical crack approaching the surface of a semi-infinite solid. Int J Fract 9:133–146. https://doi.org/10.1007/BF0004185510.1007/BF00041855 ↗
26. Hong YS, Zhao AG, Qian GA, Zhou CG (2012) Fatigue strength and crack initiation mechanism of very-high-cycle fatigue for low alloy steels. Metall Mater Trans A 43A:2753–2762. https://doi.org/10.1007/s11661-011-0816-710.1007/s11661-011-0816-7 ↗
27. Shiozawa K, Lu L, Ishihara S (2001) S-N curve characteristics and subsurface crack initiation behaviour in ultra-long life fatigue of a high carbon-chromium bearing steel. Fatigue Fract Engng Mater Struct 24:781–790. https://doi.org/10.1046/j.1460-2695.2001.00459.x10.1046/j.1460-2695.2001.00459.x ↗
28. Marines I, Bin X, Bathias C (2003) An understanding of very high cycle fatigue of metals. Int J Fatigue 25:1101–1107. https://doi.org/10.1016/S0142-1123(03)00147-610.1016/S0142-1123(03)00147-6 ↗
29. Szczepanski CJ, Jha SK, Larsen JM, Jones JW (2008) Microstructural influences on very-high-cycle fatigue-crack initiation in Ti-6246. Metall Mater Trans A 39:2841–2851. https://doi.org/10.1007/s11661-008-9633-z10.1007/s11661-008-9633-z ↗
30. Campbell FC (2012) Fatigue and fracture: understanding the basics. ASM International, Materials Park, pp 171–17210.31399/asm.tb.ffub.9781627083034 ↗
31. Hagiwara M, Kitashima T, Emura S (2018) Relationship between microstructures, facet morphologies at the high-cycle fatigue (HCF) crack initiation site, and HCF strength in Ti-6242S. Mater Sci Eng A 727:43–50. https://doi.org/10.1016/j.msea.2018.04.04310.1016/j.msea.2018.04.043 ↗
32. Wu ZH, Kou HC, Chen NN, Qiang FM, Fan JK, Tang B, Li JS (2023) Crack initiation mechanism in a high-strength Ti–5Al–75V alloy subjected to high cycle fatigue loading. Eng. Failure Anal. 148:107201. https://doi.org/10.1016/j.engfailanal.2023.10720110.1016/j.engfailanal.2023.107201 ↗