The lack of ductility is known to be a major drawback in the mechanical properties of amorphous alloys. A temperature impact is often used, as a factor to improve the mechanical parameters of these thermally unstable materials. A thick Ni82.1Cr7.8Si4.6Fe3.1Mn0.2Al0.1Cu0.1B2 metallic glass ribbon was subjected to a series of one-hour anneals between 50 and 700 °C. Annealing at 250 °C revealed an increase in the density of the ribbon accompanied by structure rearrangement responsible for the β-relaxation process. In addition, the metallic glass demonstrated high ductility along with high tensile strength and hardness under load. Based on the analysis of transformation of excess free volume in the vicinity of the β-relaxation temperature, a mechanism explaining the attainment of ductility maximum realized in metallic glass under loading has been proposed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Ghidelli M, Orekhov A, Bassi AL, Terraneo G, Djemia P, Abadias G, Nord M, Béché A, Gauquelin N, Verbeeck J, Raskin JP, Schryvers D, Pardoen T, Idrissi H (2021) Novel class of nanostructured metallic glass films with superior and tunable mechanical properties. Acta Mater 213:11695510.1016/j.actamat.2021.116955 ↗
2. Wang Q, Yang Y, Jiang H, Liu CT, Ruan HH, Lu J (2014) Superior tensile ductility in bulk metallic glass with gradient amorphous structure. Sci Rep 4:475710.1038/srep04757 ↗
3. Xu T, Pang S, Li H, Zhang T (2015) Corrosion resistant Cr-based bulk metallic glasses with high strength and hardness. J Non-Cryst Solids 410:20–2510.1016/j.jnoncrysol.2014.12.006 ↗
4. Liu CT, Heatherly L, Easton DS, Carmichael CA, Schneibel JH, Chen CH, Wright JL, Yoo MH, Horton JA, Inoue A (1998) A Test environments and mechanical properties of Zr-base bulk amorphous alloys. Metall. Mater. Trans. A Phys. Metall. Mater. Sci. 29:1811–182010.1007/s11661-998-0004-6 ↗
5. Liu X, Kong J, Song X, Feng S, Zhang Z, Yang Y, Wang T (2021) Free volume evolution dominated by glass forming ability determining mechanical performance in ZrxTi65-xBe27.5Cu7.5 metallic glasses. Mater Sci Eng A 804:14076410.1016/j.msea.2021.140764 ↗
6. Murali P, Ramamurty U (2005) Embrittlement of a bulk metallic glass due to sub-Tg annealing. Acta Mater 53:1467–147810.1016/j.actamat.2004.11.040 ↗
7. Sarac B (2021) Influence of sub-glass transition heat-treatment on physical and structural properties of Cu46Zr44Al8Hf2 metallic glass. Res Eng Struct Mat 7(1):121–134
8. Butenko PN, Hilarov VL, Obidov BA (2022) Crystallization of Ni50Ti50 metallic glass ribbon in the concept of multifractal formalism. Phase Transit. 95(7):537–55010.1080/01411594.2022.2085572 ↗
9. Zhang K, Gao X, Dong Y, Xing Q, Wang Y (2015) Effect of annealing on the microstructure, microhardness, and corrosion resistance of Ni62Nb33Zr5 metallic glass and its composites. J Non-Cryst Solids 425:46–5110.1016/j.jnoncrysol.2015.05.027 ↗
10. Okulov I, Soldatov I, Kaban I, Sarac B, Spieckermann F, Eckert J (2020) Fabrication of metastable crystalline nanocomposites by flash annealing of Cu47.5Zr47.5Al5 metallic glass using Joule heating. Nanomaterials 10:8410.3390/nano10010084 ↗
11. Hasani S, Jaafari Z, Seifoddini A, Rezaei-Shahreza P (2021) Nucleation and growth of nano-crystallites in a new multicomponent Fe-based BMG during the partial crystallization process. J Therm Anal Calorim 145:109–11810.1007/s10973-020-09718-4 ↗
12. Okulov IV, Soldatov IV, Sarmanova MF, Kaban I, Gemming T, Edström K, Eckert J (2015) Flash Joule heating for ductilization of metallic glasses. Nat Commun 6:793210.1038/ncomms8932 ↗
13. Chen Z, Datye A, Ketkaew J, Sohn S, Zhou C, Dagdeviren OE, Schroers J, Schwarz UD (2020) Relaxation and crystallization studied by observing the surface morphology evolution of atomically flat Pt57.5Cu14.7Ni5.3P22.5 upon annealing. Scr Mater 182:32–3710.1016/j.scriptamat.2020.02.035 ↗
14. Yoo BG, Park KW, Lee JC, Ramamurty U, Jang JI (2009) Role of free volume in strain softening of as-cast and annealed bulk metallic glass. J Mater Res 24(4):1405–141610.1557/jmr.2009.0167 ↗
15. Turnbull D, Cohen MH (1961) Free-volume model of the amorphous phase: glass transition. J Chem Phys 34(1):12010.1063/1.1731549 ↗
16. Spaepen F (1977) A microscopic mechanism for steady state inhomogeneous flow in metallic glasses. Acta Metall 25(4):407–41510.1016/0001-6160(77)90232-2 ↗
17. Frenkel J (1946) Kinetic theory of liquids. Clarendon Press, Oxford, p 488
18. Hasani S, Rezaei-Shahreza P, Seifoddini A (2019) Effect of Cu presence on evolution of mechanical and magnetic properties in a novel Fe-based bulk metallic glass during partial annealing process. Metall Mater Trans A 50:63–7110.1007/s11661-018-4976-6 ↗
19. Brechtl J, Agarwal S, Crespillo ML, Yang T, Bei H, Zinkle SJ (2019) Evolution of the microstructural and mechanical properties of BAM-11 bulk metallic glass during ion irradiation and annealing. J Nucl Mater 523:299–30910.1016/j.jnucmat.2019.06.010 ↗
20. Rezaei-Shahreza P, Seifoddini A, Hasani S (2018) Microstructural and phase evolutions: their dependent mechanical and magnetic properties in a Fe-based amorphous alloy during annealing process. J Alloys Compd 738:197–20510.1016/j.jallcom.2017.12.135 ↗
21. Poddar C, Ningshen S, Jayaraj J (2020) Corrosion assessment of Ni60Nb30Ta10 metallic glass and its partially crystallized alloy in concentrated nitric acid environment. J Alloy Compd 813:15217210.1016/j.jallcom.2019.152172 ↗
22. Hitit A, Şahin H, Öztürk P, Aşgın AM (2015) A new Ni-based metallic glass with high thermal stability and hardness. Metals 5:162–17110.3390/met5010162 ↗
23. Galimzyanov BN, Doronina MA, Mokshin AV (2021) Excellent glass former Ni62Nb38 crystallizing under combined shear and ultra-high pressure. J Non-Cryst Solids 572:12110210.1016/j.jnoncrysol.2021.121102 ↗
24. Inoue A, Takeuchi A (2011) Recent development and application products of bulk glassy alloys. Acta Mater 59:2243–226710.1016/j.actamat.2010.11.027 ↗
25. Li R, Li Z, Huang J, Zhang P, Zhu Y (2011) Effect of Ni-to-Fe ratio on structure and properties of Ni–Fe–B–Si–Nb coatings fabricated by laser processing. Appl Surf Sci 257:3554–355710.1016/j.apsusc.2010.11.073 ↗
26. Ishida M, Takeda H, Watanabe D, Amiya K, Nishiyama N, Kita K, Saotome Y, Inoue A (2004) Fillability and imprintability of high-strength Ni-based bulk metallic glass prepared by the precision die-casting technique. Mater Trans 45(4):1239–124410.2320/matertrans.45.1239 ↗
27. Conner RD, Dandliker RB, Johnson WL (1998) Mechanical properties of tungsten and steel fiber reinforced Zr41.25Ti13.75Cu12.5Ni10Be22.5 metallic glass matrix composites. Acta Met. 46(17):6089–610210.1016/S1359-6454(98)00275-4 ↗
28. Kündig AA, Ohnuma M, Ping DH, Ohkubo T, Hono K (2004) In situ formed two-phase metallic glass with surface fractal microstructure. Acta Mater 52(8):2441–244810.1016/j.actamat.2004.01.036 ↗
29. He J, Jiang HX, Chen S, Zhao JZ, Zhao L (2011) Liquid phase separation in immiscible Ag–Ni–Nb alloy and formation of crystalline/amorphous composite. J Non-Cryst Solids 357(21):3561–356410.1016/j.jnoncrysol.2011.07.015 ↗
30. Xi YY, He J, Sun XJ, Li W, Zhao JZ, Hao HR, Xiong T (2018) Ni-Based metallic glass composites containing Cu-rich crystalline nanospheres. Acta Metall Sin (Engl Lett) 31:1130–113610.1007/s40195-018-0756-y ↗
31. Budhani RC, Goel TC, Chopra KL (1982) Melt-spinning technique for preparation of metallic glasses. Bull Mater Sci 4(5):549–56110.1007/BF02824962 ↗
32. Betekhtin VI, Kadomtsev AG, Larionova TV, Narykova MV (2015) Effect of thermobaric treatment on the nanoporosity and properties of amorphous alloys. Met Sci Heat Treat 56(9):555–55810.1007/s11041-015-9798-1 ↗
33. McSkimin HJ (1964). In: Mason WP (Ed.), Physical acoustics, Part A. Academic Press, New York, Vol. I, p 27110.1016/B978-1-4832-2857-0.50010-1 ↗
34. Burenkov YA, Nikanorov SL, Stepanov AV (1971) Change of elastic constants of shaped crystals by electrostatic method. Izv.Akad.Nauk SSSR, Ser.Fiz. 35, 3: 525–528 (in Russian).
35. Yu H, Wang WH, Bai HY, Samwer K (2014) The β-relaxation in metallic glasses. Natl Sci Rev 1(3):429–46110.1093/nsr/nwu018 ↗
36. Goldstein M (1969) Viscous liquids and the glass transition: a potential energy barrier picture. J Chem Phys 51:3728–373910.1063/1.1672587 ↗
37. Gao M, Perepezko JH (2020) Separating β relaxation from α relaxation in fragile metallic glasses based on ultrafast flash differential scanning calorimetry. Phys Rev Mater 4:02560210.1103/PhysRevMaterials.4.025602 ↗
38. Wang J, Kaban I, Levytskyi V, Li R, Han J, Stoica M, Gumeniuk R, Nielsch K (2021) Ultra-high strength Co–Ta–B bulk metallic glasses: Glass formation, thermal stability and crystallization. J Alloy Compd 860:15839810.1016/j.jallcom.2020.158398 ↗
39. Laskovski A (2011) Biomedical engineering, trends in materials science. InTech, London, p 56410.5772/992 ↗
40. Jiang JZ, Saida J, Kato H, Inoue A (2003) Is Cu60Ti10Zr30 a bulk glass-forming alloy. Appl Phys Lett 82:4041–404210.1063/1.1581001 ↗
41. Joint Committee on Powder Diffraction Standards (JCPDS) card no. 04–0850
42. Zhu ZW, Zhang HF, Sun WS, Hu ZQ (2007) Effect of Zr addition on the glass-forming ability and mechanical properties of Ni–Nb alloy. J Mater Res 22(2):453–45910.1557/jmr.2007.0055 ↗
43. Rycroft CH, Bouchbinder E (2012) Fracture toughness of metallic glasses: annealing-induced embrittlement. Phys Rev Lett 109:19430110.1103/PhysRevLett.109.194301 ↗
44. Li J, Spaepen F, Hufnagel TC (2002) Nanometre-scale defects in shear bands in a metallic glass. Philos Mag A 82(13):2623–263010.1080/01418610208240056 ↗
45. Huang R, Suo Z, Prevost JH, Nix WD (2002) Inhomogeneous deformation in metallic glasses. J Mech Phys Solids 50:1011–102710.1016/S0022-5096(01)00115-6 ↗
46. Leamy HJ, Chen HS, Wang TT (1972) Plastic flow and fracture of metallic glass. Metall Trans 3:699–70810.1007/BF02642754 ↗
47. Lewandowski JJ, Greer AL (2006) Temperature rise at shear bands in metallic glasses. Nat Mater 5:15–1810.1038/nmat1536 ↗
48. Chen CS, Yiu P, Li CL, Chu JP, Shek CH, Hsueh CH (2014) Effects of annealing on mechanical behavior of Zr–Ti–Ni thin film metallic glasses. Mater Sci Eng A 608:258–26410.1016/j.msea.2014.03.144 ↗
49. Gu J, Song M, Ni S, Guo SF, He YH (2013) Effects of annealing on the hardness and elastic modulus of a Cu36Zr48Al8Ag8 bulk metallic glass. Mater Des 47:706–71010.1016/j.matdes.2012.12.071 ↗
50. Xing LQ, Bertrand C, Dallas JP, Cornet M (1998) Nanocrystal evolution in bulk amorphous Zr57Cu20Al10Ni8Ti5 alloy and its mechanical properties. Mater Sci Eng A 241:216–22510.1016/S0921-5093(97)00489-9 ↗
51. Wang X, Gong P, Deng L, Jin J, Wang S, Li F (2017) Sub-Tg annealing effect on the kinetics of glass transition and crystallization for a Ti-Zr-Be-Fe bulk metallic glass. J Non-Cryst Solids 473:132–14010.1016/j.jnoncrysol.2017.08.007 ↗
52. Frechen Th, Dietz G (1984) Elastic properties and structural relaxation of amorphous Co-P and Fe-P alloys. J Phys F Met Phys 14:1811–182610.1088/0305-4608/14/8/011 ↗
53. Dietz G, Hüller K, Jung K (1983) Isothermal changes of volume and Young’s modulus of amorphous Co-P. J Non-cryst Solids 57(2):265–27310.1016/0022-3093(83)90059-5 ↗
54. Yu HB, Shen X, Wang Z, Gu L, Wang WH, Bai HY (2012) Tensile plasticity in metallic glasses with pronounced β relaxations. Phys Rev Lett 108:01550410.1103/PhysRevLett.108.015504 ↗
55. Falk ML, Langer JS (1998) Dynamics of viscoplastic deformation in amorphous solids. Phys Rev E 57:7192–720510.1103/PhysRevE.57.7192 ↗
56. Yuea X, Inoueb A, Liud CT, Fan C (2017) the development of structure model in metallic glasses. Mater Res 20(2):326–33810.1590/1980-5373-mr-2016-0318 ↗