High-strength oxide ceramics joints obtained by diffusion bonding with the use of platinum and palladium gaskets
Source abstract
Abstract
Alumina and zirconia ceramics joints were made by diffusion bonding through platinum and palladium gaskets in air at temperatures between 1300 and 1550°C. The instrumentation and the procedure for these joints manufacturing are described. The effects of temperature, pressure and exposition time on 3-pt bending strength of resulting joints were established. The maximum bending strength of the samples reached 500 MPa. During thermal resistance testing the samples withstood several hundreds of thermal cycles at temperatures up to 800°C in air.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. M. A. RUBASHEV, G. I. BERDOV, V. N. GAVRILOV, et al., “Heat-Resistant Dielectrics and Their Junctions with Metals in New Engineering” (Atomizdat, Moskow, 1980) p. 246 (Russian).
2. N. F. KAZAKOV, “Diffusion Bonding of Materials” (Engineering, Moskow, 1976) p. 312 (Russian).
3. YU. V. NAIDICH, V. A. KONDRATSKY, V. S. ZHURAVLEV, et al., Adhesiya rasplavov i paika materialov 1 (1976) 74 (Russian).
4. YU. V. NAIDICH, I. I. GAB, V. S. ZHURAVLEV, et al., Avtomaticheskaya svarka 11 (1996) 33 (Russian).
5. YU. V. NAIDICH, V. S. ZHURAVLEV and N. I. FRUMINA, Adhesiya rasplavov i paika materialov 3 (1978) 99 (Russian).
6. N. F. GRIGORENKO, A. I. STEGNY, I. E. KASICH-PILIPENKO, et al., in “HTC’94,” edited by N. Eustathopoulos (Institute of Inorganic Chemistry Slovak Academy of Science, Bratislava, 1994) p. 123.
7. R. V. ALLEN and W. E. BORBIDGE, J. Mater. Sci. 18(9) (1983) 2835.10.1007/BF00547601 ↗
8. J. CHRISTENSEN and K. GOTTHJAEIP, DVS-Ber. 148 (1992) 187.