Effect of a small amount of Al2O3 addition on the hydrothermal degradation of 3Y-TZP

Zhikai Wu, Ning Li, Yuhua Wen

Journal of Materials Science· Volume 48· Issue 3
Publisher page

Abstract

The effects of 0–5 wt% Al2O3 addition on the aging sensibility and strength degradation of 3-mol-yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) were studied in this study. X-ray diffraction and field emission scanning electron microscopy were used to study the microstructures of aged specimens. The results showed that a small amount of Al2O3 addition could effectively improve the aging resistance of 3Y-TZP. The evolution of mechanical properties with aging time is different for 3Y-TZP with and without Al2O3 addition. Compared to the flexural strength, the fracture toughness and Vickers hardness of specimen are more susceptible to aging. The grain boundary segregated Al3+ plays a key role in retarding the tetragonal-to-monoclinic phase transformation of 3Y-TZP during aging.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Dental materials and restorations · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Lange FF (1982) J Mater Sci 17:225. doi: 10.1007/BF0080905710.1007/BF00809057 ↗
2. Basu B (2005) Int Mater Rev 50:23910.1179/174328005X41113 ↗
3. Lawson S (1995) J Eur Ceram Soc 15:48510.1016/0955-2219(95)00035-S ↗
4. Swab JJ (1991) J Mater Sci 26:6706. doi: 10.1007/BF0240266410.1007/BF02402664 ↗
5. Chevalier J (2004) J Am Ceram Soc 82:215010.1111/j.1151-2916.1999.tb02055.x ↗
6. Chevalier J (2006) Biomaterials 27:53510.1016/j.biomaterials.2005.07.034 ↗
7. Sato T, Shimada M (1985) J Mater Sci 20:3988. doi: 10.1007/BF0055238910.1007/BF00552389 ↗
8. Piconi C, Maccauro G (1999) Biomaterials 20:110.1016/S0142-9612(98)00010-6 ↗
9. Lughi V, Sergo V (2010) Dent Mater 26:80710.1016/j.dental.2010.04.006 ↗
10. Kihara M, Ogata T, Nakamura K, Kobayashi K (1988) J Ceram Soc Jpn 96:64610.2109/jcersj.96.646 ↗
11. Tsukama K, Shimada M (1985) J Mater Sci 4:857. doi: 1007/BF00720523
12. Li JF, Watanabe R (1997) J Mater Sci 32:1149. doi: 10.1023/A:101856741474510.1023/A:1018567414745 ↗
13. Tsubakino H, Nozato R, Hamamoto M (1991) J Am Ceram Soc 74:44010.1111/j.1151-2916.1991.tb06905.x ↗
14. Garvie RC, Nicholson PS (1972) J Am Ceram Soc 55:30310.1111/j.1151-2916.1972.tb11290.x ↗
15. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L (1999) Dent Mater 15:42610.1016/S0109-5641(99)00070-6 ↗
16. Ross IM, Rainforth WM, McComb DW, Scott AJ, Brydson R (2001) Scripta Mater 45:65310.1016/S1359-6462(01)01076-4 ↗
17. Matsui K, Horikoshi H, Ohmichi N, Ohgai M (2003) J Am Ceram Soc 86:140110.1111/j.1151-2916.2003.tb03483.x ↗
18. Tsubakino H, Hamamoto M, Nozato R (1991) J Mater Sci 26:5521. doi: 10.1007/BF0240395310.1007/BF02403953 ↗