Abstract

The second phases in Ti40 (Ti25V-15Cr-0.2Si) burn resistant titanium alloy are studied. The higher solution temperature, the more second phases in Ti40 alloy. There are not second phases if the solution temperature is below 850°C, while there are rod-like α and little Ti5Si3 phases if temperature is over 850°C. α, Ti5Si3 and oblique α′′ phases emerge after Ti40 solution at 910°C followed by aging at 600°C, while only Ti5Si3 phases emerge after solution at 860°C followed by aging at 600°C. The effect of the second phases on properties at RT are not obvious. There are different shapes of α and Ti5Si3 precipitates after Ti40 alloy exposure at 540°C for 100 h, which decreases the thermal stability.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. S. R. Seagle, Mater. Sci. Eng. A213 (1996) 1.10.1016/0921-5093(96)10245-8 ↗
2. R. R. Boyer, ibid. A213 (1996) 103.10.1016/0921-5093(96)10233-1 ↗
3. Lockheed Martin, Advanced Mater. Proc. 59 (1998) 23.
4. UK Patent Application, 2 238057 (1987).
5. Y. Q. Zhao, X. M. Zhao and K. Y. Zhu, Rare Metal Mater. Eng. 5 (1996) 1.
6. Y. G. Li, P. A. Blenkinsop and M. H. Loretto, Mater. Sci. Technol. 14 (1998) 732.10.1179/mst.1998.14.8.732 ↗
7. Idem., Acta Mater. 16 (1998) 5777.
8. Idem., in Proc. 9th World Conference on Titanium, Russia (2000), p. 141.
9. Y. Q. Zhao, K. Y. Zhu and M. X. Zhao, Chinese Patent Application, 97 1 12303.9 (1997).
10. Y. Q. Zhao, L. Zhou and J. Deng, Rare Metal Mater. Eng. 2 (1999) 77.
11. Idem., Mater. Sci. Eng. A267 (1999) 167.10.1016/S0921-5093(99)00109-4 ↗
12. Idem., J. Alloys Compounds 284 (1999) 190.10.1016/S0925-8388(98)00926-8 ↗
13. Y. Q. Zhao, K. Y. Zhu and H. L. Qu, Mater. Sci. Eng. A 316 (2001) 211.10.1016/S0921-5093(01)01238-2 ↗
14. K. Y. Zhu, Y. Q. Zhao and H. L. Qu, J. Mater. Sci. 35 (2000) 5609.10.1023/A:1004873501005 ↗
15. Y. Q. Zhao, K. Y. Zhu and M. X. Zhao, Chinese Patent Application, 97 1 12302.0 (1997).
16. Y. Q. Zhao, Research on Burn Resistant Titanium Alloys-Final Research Report, Northwest Institute for Nonferrous Metal Research, 1996.
17. D. W. Anderson and A. F. Condliff, in Proc. of the 10th Annual International Titanium Association Application Conference & Exhibition, 1994, USA, p. 91.
18. A. Vassel, in “Beta Titanium Alloys in the 1990's” edited by D. Eylon, R. R. Boyer and D. A. Koss (TMS, 1993) p. 173.