journal article·2004-06

Creep behavior of MoSi2 and MoSi2 + SiC composite

P. Hvizdoš, J. Dusza, W. Steinkellner, K. Kromp

Journal of Materials Science· Volume 39· Issue 12
Publisher page

Abstract

Recently, there has been an increasing need for structural materials that can withstand oxidizing environments at elevated temperatures up to 1500 ◦C. Such materials are important for modifications in energy production technologies with the aim to improve their efficiency and to reduce carbon dioxide exhaust level. Similarly, advanced aircraft engine designs require new materials that can operate at temperatures higher than those tolerable for superalloys. Materials based on MoSi2 are promising candidates for such applications thanks to their high melting point (2030 ◦C), excellent oxidation and corrosion resistance, and high temperature ductility above the brittle–ductile transition temperature in the vicinity of 1000 ◦C [1–4]. However, the main disadvantage, limiting their use, is the low fracture toughness at lower temperatures (<1000 ◦C) and the low strength and creep resistance at high temperatures. In order to improve the mentioned properties, various approaches based on incorporating of SiC, Nb, and ZrO2 particles or SiC whiskers into the matrix have been used [5–10]. MoSi2 + SiC composites were generally developed to increase the fracture toughness compared to MoSi2. However, the fracture toughness has not been improved by the addition of SiC particles because the SiC particles themselves or their clusters are the strength-degrading fracture origins. The aim of the present work was to study and compare the creep behavior of monolithic MoSi2 and MoSi2 + SiC composite and to investigate the influence of the SiC particles on the creep mechanisms in the temperature range 1100–1200 ◦C in air. The materials used in this investigation were monolithic MoSi2 and MoSi2 + 20 vol% SiC, prepared by Cesiwid, Erlangen, Germany. Specimens for bending creep tests were cut to the dimensions 3 mm × 4 mm × 45 mm and polished with 15 μm finish on their tensile surface. The creep tests were carried out in the fourpoint bending mode with inner/outer roller spans of 20/40 mm. The bending bars were tested at temperatures from 1100 to 1200 ◦C under loads from 20 to 100 MPa. The tests were realized in a creep furnace with a dead weight loading system in air. From specimen deflection data, measured by two inductive transducers between the center and the inner roller and collected by a computer data acquisition system, the outer fiber strain was calculated and recorded. The accuracy of the deflection measurement was approximately ±1 μm. The creep experiments at all stress/temperature combinations were carried out up to 1% bending strain. Samples for microstructure analysis were prepared using standard procedure and investigated using optical microscopy, as well as scanning and transmission electron microscopy (SEM and TEM). The volume fraction of individual phases (pores) was measured using an image analyzer and statistical methods. X-ray microanalysis (EDX) was used for the identification of individual phases present in the microstructure. Thin foils of the as-received materials and the tensile surfaces of the crept specimens were prepared for the microstructure and substructure observations, which were carried out using high resolution TEM (HRTEM) techniques in order to identify the high temperature deformation mechanisms. Microstructures of the studied materials are shown in Fig. 1a and b. Using SEM and EDX it was found that there were three different phases present in the microstructure of the monolithic MoSi2: matrix MoSi2 grains, SiO2, and a little of Mo5Si3 (hexagonal Nowotny phase). TEM observations of the as-received materials proved that silica (SiO2) particles were frequently present in the triple grain junctions of MoSi2 grains and occasionally were placed intragranularly, inside the MoSi2 grains. The mean grain size of MoSi2 was approximately 7 μm. The silica particles were usually spherical with diameter of the intergranular particles in the range from 1 to 5 μm and the intragranular ones with diameter from 0.2 to 2 μm. HRTEM was used to determine whether there was any amorphous phase present at the grain boundaries. It was found that the grain boundaries were clear and the SiO2 did not wet the matrix boundaries, Fig. 2. The composite material, besides the features common to monolithic material, contained SiC grains with an average size of 5 μm, clusters of grains, and a porosity of 3.2 vol%. The MoSi2 matrix grains were larger than those in the monolithic material and typically had dimensions from 10 to 15 μm. Comparison of their room-temperature mechanical properties was presented elsewhere [11]. The creep tests showed a remarkable difference between the creep behavior of both materials, as can be seen from Fig. 3. At the test condition of 1100 ◦C/100 MPa the monolithic MoSi2 exhibited a strain of 0.15% after a loading time of 2 hr, while the
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. A. K. Vasudevan and J. J. Petrovic Mater. Sci. Eng. A 155 (1995) 1.10.1016/0921-5093(92)90308-N ↗
2. L. Shaw, D. Miracle and R. Abbaschian Acta Metal. Mater. 43 (1995) 4267.10.1016/0956-7151(95)00130-N ↗
3. A. Costa E Silva and M. J. Kaufman Mater. Sci. Eng. A 195 (1995) 75.10.1016/0921-5093(94)06507-1 ↗
4. S. Maloy, A. H. Heuer, J. Lewandowski and J. J. Petrovic J. Amer. Ceram. Soc. 74 (1991) 2704.10.1111/j.1151-2916.1991.tb06829.x ↗
5. J. J. Petrovic and A. K. Vasudevan Mater. Sci. Eng. A 261 (1999) 1.10.1016/S0921-5093(98)01043-0 ↗
6. S. Jayashankar and M. J. Kaufman Scrip. Met. Mater. 26 (1992) 1245.10.1016/0956-716X(92)90571-U ↗
7. T. Yamada, K. Hirota, O. Yamaguchi, J. Asai and Y. Makayama Mater. Res. Bull. 7 (1995) 851.10.1016/0025-5408(95)00073-9 ↗
8. A. K. Bhattacharya and J. J. Petrovic J. Amer. Ceram. Soc. 75 (1992) 23.10.1111/j.1151-2916.1992.tb05436.x ↗
9. W. Soboyejo, D. Brooks and L. C. Chen ibid. 78 (1995) 1481.10.1111/j.1151-2916.1995.tb08841.x ↗
10. J. J. Petrovic Mater. Sci. Eng. A 192/193 (1995) 31.10.1016/0921-5093(94)03246-7 ↗
11. B. BallÓkovÁ, J. Dusza, W. Steinkellner and K. Kromp, in Proceedings of Fractography 97, Stará Lesná, October 1997, edited by L. Parilak (IMR SAS, Kosice, 1997) p. 448.
12. K. Sadananda, C. R. Feng, H. Jones and J. J. Petrovic Mater. Sci. Eng. A 155 (1992) 227.10.1016/0921-5093(92)90329-Y ↗
13. P. Kofstad, “High Temperature Oxidation of Metals” (Wiley, New York, 1966).
14. J. Dusza, P. HvizdoŠ, W. Steinkellner and K. Kromp Scripa Materialia 37 (1997) 471.10.1016/S1359-6462(97)00120-6 ↗