Erosion of a reaction bonded silicon nitride
Source abstract
Abstract
Many potential applications of silicon nitride involve solid particle erosion at elevated temperatures. The typical examples of such applications are the key components in the hot section of a gas turbine engine. One variety of such silicon nitride is the reaction bonded silicon nitride. Though the mechanical properties of this material are not particularly outstanding at room temperature, they are known to be retained up to very high temperatures since this material typically does not contain a grain boundary phase that softens and degrades the properties at elevated temperatures. The temperature dependence of erosion rate has been reported for sintered and hot pressed silicon nitrides [1, 2]. The temperature increases the erosion rate of hot pressed silicon nitrides [1], whereas it decreases the erosion rate in sintered silicon nitride [2]. Thus, it is difficult to predict erosion behavior of reaction bonded silicon nitride at elevated temperatures based on these results. In addition, the hardness and fracture toughness that are known to control the erosion of ceramics are much lower for this material compared to hot pressed and sintered silicon nitrides. In this report, the effects of temperature, impact velocity and impact angle on the erosion rate of a reaction bonded silicon nitride were investigated. The target material used in this investigation is a high purity reaction bonded silicon nitride supplied in disc form with the following properties: density ρ = 2.4 g·cm−3; hardness H = 7.8 GPa; fracture toughness KIC = 2.5 MPa·m1/2. This is a porous material with density of 75% of theoretical. The discs were cut into pieces to give specimens of dimensions 20 × 20 × 5 mm3. The specimens were mechanically ground and polished successively using diamond paste up to 3 μm. After grinding and polishing, the specimens were fired at 400 ◦C for 24 hrs to remove the oil-based grinding and polishing fluids. Erosion tester used for this work consists of a screwtype particle feeder, gas heater and resistance heated furnace. The carrier gas, either air or N2, is heated to the desired temperature and passed through an acceleration tube, and then mixed with particles before reaching the 4 mm internal diameter alumina nozzle. The acceleration tube, nozzle and the specimen holder are all housed in a 3-zone furnace which is heated to test temperature. The particle velocity is controlled utilizing the gas pressure and measured using the rotating double discs [3]. Erosion tests were conducted at 22, 300, 500, 700 and 900 ◦C using 50 g of angular silicon carbide particles of mean diameter 100 μm. Air was used for accelerating these particles. After completion of the test, the specimen was furnace cooled to room temperature either in air or N2 atmosphere and then weighed to an accuracy of 10−5 g using a microbalance. Erosion rate was calculated by dividing the specimen mass loss by the total mass of erodent particles impacted. Fig. 1 shows the variation in the erosion rates of reaction bonded silicon nitride with temperature at an impact velocity of 70 ms−1 under normal impingement condition. The erosion rate of this material decreases with increasing temperature in contrast to the result of hot-pressed silicon nitride, but is consistent with that of sintered silicon nitride. The erosion rate of reaction bonded silicon nitride decreases sharply by increasing temperature to 300 ◦C, but is very little affected by temperatures between 300 and 700 ◦C. There is again a larger drop in erosion rate at 900 ◦C. The erosion rates at 300 and 900 ◦C are approximately 50 and 30% of that at room temperature, respectively. The temperature dependence of erosion rate for reaction bonded silicon nitride may be related with the variation of fracture toughness and hardness of this material with temperature as a quasi-static model predicts [4]. According to this model, the erosion rate of brittle materials follows the power-law relations, E ∝ (KIC)−4/3(H )0.11, where, KIC and H are the fracture toughness and hardness of the target material, respectively. The fracture toughness of a similar reaction bonded silicon nitride with a density of 2.32 g cm−3 (73% of theoretical) has been reported to increase up to 900 ◦C with increasing temperature [5]. The fracture toughness of the reaction bonded silicon nitride at 900 ◦C was larger by about 6% than that at room temperature. In addition, hardness of reaction bonded silicon nitride can be presumed to decrease with increasing temperature as reported in a similar purity silicon nitride [6]. This can be confirmed indirectly from the size of indentation formed during erosion at 900 ◦C, which is much larger than that at room temperature. The velocity exponents obtained from the slope of log–log plot of the erosion data are presented in Fig. 2. The exponents for normal incidence are 2.4 and 2.0 at 22 and 900 ◦C, respectively. The value of the velocity exponent is predicted to be 2.4 by quasi-static model [3] and 2.0 by grain ejection model [4]. This suggests that the temperature dependence of the erosion of this material can only be explained roughly by the quasistatic model, since the grain ejection was not observed in this material as will be described later. For the investigation of the effect of temperature on the exponent in detail, specimens eroded under normal
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Erosion and Abrasive Machining · Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. S. M. Wiederhorn and J. B. Hockey, J. Mater. Sci. 18 (1983) 766.10.1007/BF00745575 ↗
2. J. E. Ritter, S. R. Choi, K. Jakus, P. J. Whalen and R. G. Rateick, ibid. 26 (1991) 5543.10.1007/BF02403956 ↗
3. A. W. Ruff and L. K. Ives, Wear 35 (1975) 195.10.1016/0043-1648(75)90154-4 ↗
4. S. M. Wiederhorn and B. R. Lawn, J. Amer. Ceram. Soc. 62(1/2) (1979) 66.10.1111/j.1151-2916.1979.tb18808.x ↗
5. A. S. Jayatilaka and J. A. Leaks, Proc. Brit. Ceram. Soc. 25 (1975) 311.
6. K. Nihara and T. Hirai, Powder Met. Int. 6(5) (1984) 223.
7. J. K. Ritter, P. Strazepa, K. Jakus, L. Rosenfeld and K. J. Buckman, J. Amer. Ceram. Soc. 67(11) (1984) 769.10.1111/j.1151-2916.1984.tb19515.x ↗
8. L. K. Ives and A. W. Ruff, ASTM STP (1979) vol. 664, p. 5.
9. J. J. Kim, D. J. Kim and S. J. Cho, J. Mater. Sci. Lett. 20 (2001) 427.10.1023/A:1010946313262 ↗