journal article·2002-08

Oxidation behavior and thermal stability of Si-C-O fibers (Nicalon) in carbon dioxide

T. Shimoo, T. Morita, K. Okamura

Journal of Materials Science· Volume 37· Issue 15
Publisher page

Abstract

The oxidation behavior and thermal stability of Si-C-O fibers (Nicalon) in CO2 gas were examined at 1273 to 1773 K through mass change determination, XRD analysis, resistivity measurement, SEM observation and tensile test. Large mass gains and SiO2 film formation show that Nicalon fibers are passively oxidized in CO2, as well as Si-C fibers (Hi-Nicalon). The grain growth of β-SiC, the drop of resistivity and the crystallization of SiO2 film were observed above 1573 K. On being oxidized at high temperature, the thermal decomposition of SiC X O Y and the formation of imperfections in SiO2 film caused the degradation of the room-temperature tensile strength of both the as-oxidized fibers and unoxidized cores. It became evident that the oxygen partial pressure for the active-to-passive oxidation transition of Nicalon fibers is between 1.00 × 102 and 1.78 × 102 Pa at 1773 K.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. T. MAH, N. L. HECHT, D. E. McCULLUM, J. R. HOENIGMAN, H. M. KIM, A. P. KATS and H. A. LIPSITT, J. Mater. Sci. 19 (1984) 1191.10.1007/BF01120029 ↗
2. Y. MANIETTE and A. OBERLIN, ibid. 24 (1989) 3361.10.1007/BF01139066 ↗
3. M. H. JASKOWIAK and J. A. DI. CARLO, J. Amer. Ceram. Soc. 74 (1991) 192.
4. H.-E. KIM and A. J. MOORHEAD, ibid. 74 (1991) 666.10.1111/j.1151-2916.1991.tb04079.x ↗
5. T. SHIMOO, H. CHEN and K. OKAMURA, J. Ceram. Soc. Jpn. 100 (1992) 929.10.2109/jcersj.100.929 ↗
6. T. SHIMOO, T. HAYATSU, M. TAKEDA, H. ICHIKAWA and K. OKAMURA, ibid. 102 (1994) 617.10.2109/jcersj.102.617 ↗
7. M. H. BERGER, N. HOCHET and A. R. BUNSELL, J. Microsc. 177 (1995) 230.10.1111/j.1365-2818.1995.tb03554.x ↗
8. P. LE. COUSTUMER, M. MONTHIOUX and A. OBERLIN, Br. Ceram. Trans. 94 (1995) 177.
9. C. VIX-GUTERL and P. EHRBURGER, J. Mater. Sci. 31 (1996) 5363.10.1007/BF01159305 ↗
10. G. CHOLLON, R. E. PAILLER, R. NASLAIN, F. LAANANI, M. MONTHIOUX and P. OLRY, ibid. 32 (1997) 327.10.1023/A:1018541030308 ↗
11. G. CHOLLON, M. CZERNIAK, R. PAILLER, X. BOURRA, R. NASLAIN, J. P. PILLOT and R. CANNET, ibid. 32 (1997) 893.10.1023/A:1018597432067 ↗
12. M. H. BERGER, N. HOCHET and A. R. BUNSELL, J. Microsc. 185 (1997) 243.10.1046/j.1365-2818.1997.d01-620.x ↗
13. T. SHIMOO, F. TOYODA and K. OKAMURA, J. Ceram. Soc. Jpn. 106 (1998) 447.10.2109/jcersj.106.447 ↗
14. Y. T. ZHU, S. T. TAYLOR, M. G. STOUT, D. P. BUTT and C. LOWE, J. Amer. Ceram. Soc. 81 (1998) 655.10.1111/j.1151-2916.1998.tb02386.x ↗
15. M. TAKEDA, J. SAKAMOTO, Y. IMAI and H. ICHIKAWA, Composites Sci. and Tech. 59 (1999) 813.10.1016/S0266-3538(99)00012-3 ↗
16. T. SHIMOO, F. TOYODA and K. OKAMURA, J. Mater. Sci. 35 (2000) 3301.10.1023/A:1004883607913 ↗
17. T. SHIMOO, H. TAKEUCHI and K. OKAMURA, J. Ceram. Soc. Jpn. 108 (2000) 1096.10.2109/jcersj.108.1264_1096 ↗
18. T. SHIMOO, Y. MORISADA and K. OKAMURA, J. Amer. Ceram. Soc. 83 (2000) 3049.10.1111/j.1151-2916.2000.tb01681.x ↗
19. T. SHIMOO, H. TAKEUCHI and K. OKAMURA, ibid. 84 (2001) 566.10.1111/j.1151-2916.2001.tb00699.x ↗
20. T. SHIMOO, Y. MORISADA and K. OKAMURA, J. Mater. Sci. 37 (2002) 1793.10.1023/A:1014945823031 ↗
21. T. SHIMOO, T. MORITA and K. OKAMURA, J. Amer. Ceram. Soc. 84 (2001) 2975.10.1111/j.1151-2916.2001.tb01123.x ↗
22. E. J. OPILA, ibid. 81 (1998) 1949.10.1111/j.1151-2916.1998.tb02573.x ↗
23. E. T. TURKDOGAN, in “Physical Chemistry of High Temperature Technology” (Academic Publishers, New York, 1980) p. 1.
24. M. J. H. BALAT, J. Europ. Ceram. Soc. 16 (1996) 55.10.1016/0955-2219(95)00104-2 ↗
25. B. SCHNEIDER, A. GUETTE, R. NASLAIN, M. CATALDI and A. COSTECALDE, J. Mater. Sci. 33 (1998) 535.10.1023/A:1004313022769 ↗
26. T. SHIMOO, F. TOYODA and K. OKAMURA, J. Amer. Ceram. Soc. 83 (2000) 1450.10.1111/j.1151-2916.2000.tb01409.x ↗