Phase stability of $$\upbeta$$ -MoSi2−x prepared by the Na flux method against thermal, oxidative, and mechanical treatments
Source abstract
Abstract
The single \(\upbeta\)-MoSi2 phase was prepared by the Na flux method and its stability against thermal, oxidative, and mechanical treatments was investigated. The X-ray diffraction results show that the single \(\upbeta\) phase is formed at 600 °C within 1 h using pre-mixed Mo and Si powders with a Si/Mo molar ratio of 2.00–2.25. By energy-dispersive X-ray spectroscopy, the produced powder is found to be Si-deficient with a Si/Mo molar ratio of 1.87–1.96. The differential thermal analysis shows that the \(\upbeta\) phase transforms into the \(\upalpha\)-MoSi2 phase at 815 °C at 10 K/min with the segregation of a small amount of Mo5Si3. The transformation heat is −5.5 kJ/mol and the activation energy calculated by the Kissinger method is 290 kJ/mol. Thermogravimetry reveals that the \(\upbeta\)-MoSi2−x powder oxidizes significantly at 400–600 °C via the pest oxidation mechanism while it is resistant to oxidation at 700 °C for 5 h similarly to the \(\upalpha\)-MoSi2 phase. At last, mechanical milling on the \(\upbeta\)-MoSi2−x powder with a planetary ball mill up to 216 h demonstrates that this powder is stable under a severe mechanical treatment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Zaitsev VK, Fedorov MI, Gurieva EA, Eremin IS, Konstantinov PP, Samunin AY, Vedernikov MV (2006) Phys Rev B 74:04520710.1103/PhysRevB.74.045207 ↗
2. Udono H, Nakamori K, Takahashi Y, Ujiie Y, Ohsugi IJ, Iida T (2011) J Electron Mater 40:116510.1007/s11664-011-1561-9 ↗
3. Homm G, Klar PJ (2011) Phys Status Solidi RRL 5:32410.1002/pssr.201105084 ↗
4. Yamada T, Yamane H (2011) Intermetallics 19:90810.1016/j.intermet.2011.02.003 ↗
5. Yamada T, Yamane H (2011) J Alloy Compd 509:L2310.1016/j.jallcom.2010.09.179 ↗
6. Doland CM, Nemanich RJ (1990) J Mater Res 5:285410.1557/JMR.1990.2854 ↗
7. Frankwicz P, Perepezko J (1998) Mater Sci Eng A 246:19910.1016/S0921-5093(97)00747-8 ↗
8. Meschter PJ (1992) Metall Mater Trans A 23:176310.1007/BF02804369 ↗
9. Yao Z, Stiglich J, Sudarshan T (1999) J Mater Eng Perform 8:29110.1361/105994999770346837 ↗
10. Schwarz R, Srinivasan S, Petrovic J, Maggiore C (1992) Mater Sci Eng A 155:7510.1016/0921-5093(92)90314-Q ↗
11. Lee C (2008) J Ceram Process Res 9:321
12. Hara KO, Yamasue E, Okumura H, Ishihara KN (2011) J Alloy Compd 509:S24310.1016/j.jallcom.2011.02.014 ↗
13. Claar TD (1970) React Technol 13:124
14. Morito H, Yamada T, Ikeda T, Yamane H (2009) J Alloy Compd 480:72310.1016/j.jallcom.2009.02.036 ↗
15. Zhang XY, Sprengel W, Staab TEM, Inui H, Schaefer HE (2004) Phys Rev Lett 92:15550210.1103/PhysRevLett.92.155502 ↗
16. Mittemeijer EJ (1992) J Mater Sci 27:3977. doi: 10.1007/BF0110509310.1007/BF01105093 ↗
17. Nava F, Riontino G, Galli E (1988) J Non-Cryst Solids 104:19510.1016/0022-3093(88)90388-2 ↗
18. Berztiss DA, Cerchiara RR, Gulbransen EA, Pettit FS, Meier GH (1992) Mater Sci Eng A 155:16510.1016/0921-5093(92)90324-T ↗
19. Berkowitz-Mattuck JB, Blackburn PE, Felten EJ (1965) Trans Met Soc AIME 233:1093
20. Ishihara KN, Yamasue E, Okumura H, Hara KO (2012) Int J Mater Res 103:113010.3139/146.110772 ↗