Abstract

The present work investigates the effect of different solutes on the formation of primary carbides in high chromium cast irons (HCCI) through thermodynamic modeling. Growth restriction factor, Q, for the growth of primary carbide in a multicomponent HCCI is evaluated with the assistance of the CALPHAD method. Thermodynamic modeling indicates that modification of the primary carbide by growth restriction through solute addition is ineffective because commonly used solutes in ferrous alloys such as Ti, Nb, and Mn, form carbides or other intermetallic compounds in the melt prior to the formation of primary carbide and non-reactive solutes, such as Cu, Ni, Si, and Co, cannot lead to the formation of sufficient constitutional undercooling zone at the front of the growing carbide to enable the new nucleation event. Hence, it is suggested that external addition or in-situ formation of inoculants to promote heterogeneous nucleation of primary carbides is a more effective approach to refine or modify the primary carbides in HCCIs. Graphical abstract: [Figure not available: see fulltext.]
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Laird II G, Powell GLFP (1993) Solidification and solid-state transformation mechanisms in si alloyed high-chromium white cast irons. Metal Trans A 24A:981–988.10.1007/BF02656520 ↗
2. Tabrett CP, Sare IR, Ghomashchi MR (1996) Microstructure-property relationships in high chromium white iron alloys. Int Mater Rev 41:59–82. https://doi.org/10.1023/A:100475551121410.1023/A:1004755511214 ↗
3. Zhi X et al. (2008) Effect of fluctuation and modification on microstructure and impact toughness of 20 wt.% Cr hypereutectic white cast iron. Materialwissenschaft und Werkstofftechnik 39(6):391–393. https://doi.org/10.1002/mawe.200700219.10.1002/mawe.200700219 ↗
4. Laird G, Klaus Röhrig RG (2000) Abrasion-Resistant cast iron handbook. American Foundry Society, Illinois.
5. Hongsug OH, Jae-Young SL, Jung, Sangho Ahn (2001) Correlation of microstructure with the wear resistance and fracture toughness of duocast materials composed of high-chromium white cast iron and low-chromium steel. Metal Mater Trans A, 32A.10.1007/s11661-001-0068-z ↗
6. Tabrett CP, Sare IR (2000) Fracture toughness of high-chromium white irons-influence of cast structure. J Mater Sci 35:2069–2077. https://doi.org/10.1023/A:100475551121410.1023/A:1004755511214 ↗
7. Coronado JJ (2011) Effect of (Fe, Cr)7C3 carbide orientation on abrasion wear resistance and fracture toughness. Wear 270(3–4):287–293. https://doi.org/10.1016/j.wear.2010.10.07010.1016/j.wear.2010.10.070 ↗
8. Ma S et al (2015) Microstructure and crystallography of M7C3 carbide in chromium cast iron. Mater Chem Phys 161:65–73. https://doi.org/10.1016/j.matchemphys.2015.05.00810.1016/j.matchemphys.2015.05.008 ↗
9. Zhi X et al (2008) Effect of titanium on the as-cast microstructure of hypereutectic high chromium cast iron. Mater Charact 59(9):1221–1226. https://doi.org/10.1016/j.matchar.2007.10.01010.1016/j.matchar.2007.10.010 ↗
10. Zhi X et al (2008) Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron. Mater Sci Eng A 487(1–2):171–179. https://doi.org/10.1016/j.msea.2007.10.00910.1016/j.msea.2007.10.009 ↗
11. Chung RJ et al. (2009) Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe–25wt.%Cr–4wt.%C. Wear 267(1–4): 356–361. https://doi.org/10.1016/j.wear.2008.12.061.10.1016/j.wear.2008.12.061 ↗
12. Liu Q et al (2012) Effect of heat treatment on microstructure and mechanical properties of Ti-alloyed hypereutectic high chromium cast iron. ISIJ Int 52(12):2288–2294. https://doi.org/10.2355/isijinternational.52.228810.2355/isijinternational.52.2288 ↗
13. Zhifu Huang JX, Yimin Gao, Xiaohui Zhi (2012) Effect of titanium on the as-cast microstructure and impact toughness of hypereutectic high-chromium cast iron. Int J Mater Res 103(5):609–61210.3139/146.110733 ↗
14. Liu Q, Jönsson PG, Nakajima K (2013) Estimation of the maximum carbide size in a hypereutectic high chromium cast iron alloyed with titanium. ISIJ Int 53(12):2176–2183. https://doi.org/10.2355/isijinternational.53.217610.2355/isijinternational.53.2176 ↗
15. Huang ZF et al (2014) Effect of Ti addition on morphology and size of primary M7C3type carbide in hypereutectic high chromium cast iron. Mater Sci Technol 27(1):426–430. https://doi.org/10.1179/026708309x1260195277766610.1179/026708309x12601952777666 ↗
16. He-Xing Chen Z-CC, Jin-Cai Lu, Huai-Tao Lin (1993) Effect of niobium on wear resistance of 15%Cr white cast iron. Wear 166:97–201.10.1016/0043-1648(93)90262-K ↗
17. Fiset M, Peev K, Radulovic M (1993) The influence of niobium on fracture toughness and abrasion resistance in high-chromium white cast irons. J Mater Sci Lett 12: 615–617.10.1007/BF00465569 ↗
18. Zhi X et al (2008) Effect of niobium on the as-cast microstructure of hypereutectic high chromium cast iron. Mater Lett 62(6–7):857–860. https://doi.org/10.1016/j.matlet.2007.06.08410.1016/j.matlet.2007.06.084 ↗
19. Hirose M et al (2010) Abrasion behavior of high Cr-V-Nb Cast Iron. Key Eng Mater 457:243–248. https://doi.org/10.4028/www.scientific.net/KEM.457.24310.4028/www.scientific.net/KEM.457.243 ↗
20. Chung RJ et al (2013) Microstructure refinement of hypereutectic high Cr cast irons using hard carbide-forming elements for improved wear resistance. Wear 301(1–2):695–706. https://doi.org/10.1016/j.wear.2013.01.07910.1016/j.wear.2013.01.079 ↗
21. Kusumoto K et al (2017) Abrasive wear characteristics of Fe-2C-5Cr-5Mo-5W-5Nb multi-component white cast iron. Wear 376–377:22–29. https://doi.org/10.1016/j.wear.2017.01.09610.1016/j.wear.2017.01.096 ↗
22. Zhao WM et al (2008) Effects of vanadium and rare-earth on carbides and properties of high chromium cast iron. Mater Sci Forum 575–578:1414–1419. https://doi.org/10.4028/www.scientific.net/MSF.575-578.141410.4028/www.scientific.net/MSF.575-578.1414 ↗
23. Filipovic M, Kamberovic Z, Korac M (2011) Solidification of high chromium white cast iron alloyed with vanadium. Mater Trans 52(3):386–390. https://doi.org/10.2320/matertrans.M201005910.2320/matertrans.M2010059 ↗
24. Wang YP et al (2011) Improving the wear resistance of white cast iron using a new concept—high-entropy microstructure. Wear 271(9–10):1623–1628. https://doi.org/10.1016/j.wear.2010.12.02910.1016/j.wear.2010.12.029 ↗
25. L.A. Mampuru, M.G.M., J.S. Moema, Grain refinement of 25 wt% high-chromium white cast iron by addition of vanadium. J Southern Af Inst Mining Metal, 2016. 116(10): p. 969–972. https://doi.org/10.17159/2411-9717/2016/v116n10a12.10.17159/2411-9717/2016/v116n10a12 ↗
26. Maldonado-Ruíz SI et al (2016) Wear resistance of high chromium—high carbon cast irons. Int J Cast Met Res 15(6):589–594. https://doi.org/10.1080/13640461.2003.1181954510.1080/13640461.2003.11819545 ↗
27. Mousavi Anijdan SH et al (2007) Effects of tungsten on erosion–corrosion behavior of high chromium white cast iron. Mater Sci Eng A 454–455:623–628. https://doi.org/10.1016/j.msea.2006.11.12810.1016/j.msea.2006.11.128 ↗
28. Heydari D, Skandani AA, Al Haik M (2012) Effect of carbon content on carbide morphology and mechanical properties of A.R. white cast iron with 10–12% tungsten. Mater Sci Eng A 542:113–126. https://doi.org/10.1016/j.msea.2012.02.040.10.1016/j.msea.2012.02.040 ↗
29. Kopyciński D, Piasny S (2012) Influence of tungsten and titanium on the structure of chromium cast iron. Arch Foundry Eng 12(1):57–60. https://doi.org/10.2478/v10266-012-0011-310.2478/v10266-012-0011-3 ↗
30. Lv Y et al (2012) Effect of tungsten on microstructure and properties of high chromium cast iron. Mater Des 39:303–308. https://doi.org/10.1016/j.matdes.2012.02.04810.1016/j.matdes.2012.02.048 ↗
31. Yamamoto K et al (2014) Influence of Mo and W on High temperature hardness of M7C3 carbide in high chromium white cast iron. Mater Trans 55(4):684–689. https://doi.org/10.2320/matertrans.F-M201480110.2320/matertrans.F-M2014801 ↗
32. Guerra FV et al (2019) Effect of the simultaneous Ti and W addition on the microstructure and wear behavior of a high chromium white cast iron. Metal Res Technol 116(6). https://doi.org/10.1051/metal/2019031.10.1051/metal/2019031 ↗
33. Filipovic M et al (2013) Microstructure and mechanical properties of Fe–Cr–C–Nb white cast irons. Mater Des 47:41–48. https://doi.org/10.1016/j.matdes.2012.12.03410.1016/j.matdes.2012.12.034 ↗
34. Youping Ma XL, Yugao Liu, Shuyi Zhou, Xiaoming Dang (2013) Microstructure and properties of Ti–Nb–V–Mo-alloyed high chromium cast iron. Bull Mater Sci 36(5):839–84410.1007/s12034-013-0558-9 ↗
35. Yilmaz SO, Teker T (2016) Effect of TiBAl inoculation and heat treatment on microstructure and mechanical properties of hypereutectic high chromium white cast iron. J Alloy Compd 672:324–331. https://doi.org/10.1016/j.jallcom.2016.02.12510.1016/j.jallcom.2016.02.125 ↗
36. Fu H-G et al (2009) Effect of TiC particle additions on structure and properties of hypereutectic high chromium cast iron. J Mater Eng Perform 18(8):1109–1115. https://doi.org/10.1007/s11665-008-9330-510.1007/s11665-008-9330-5 ↗
37. Zhang Y et al (2020) The formation of TiC–NbC core-shell structure in hypereutectic high chromium cast iron leads to significant refinement of primary M7C3. J Alloys Compounds, 824. https://doi.org/10.1016/j.jallcom.2020.153806.10.1016/j.jallcom.2020.153806 ↗
38. Liu S et al (2017) Experiments and calculations on refining mechanism of NbC on primary M 7 C 3 carbide in hypereutectic Fe-Cr-C alloy. J Alloy Compd 713:108–118. https://doi.org/10.1016/j.jallcom.2017.04.16710.1016/j.jallcom.2017.04.167 ↗
39. Hao F et al (2011) Effect of rare earth oxides on the morphology of carbides in hardfacing metal of high chromium cast iron. J Rare Earths 29(2):168–172. https://doi.org/10.1016/s1002-0721(10)60425-510.1016/s1002-0721(10)60425-5 ↗
40. Yang J et al (2014) Microstructure and wear resistance of the hypereutectic Fe–Cr–C alloy hardfacing metals with different La2O3 additives. Appl Surf Sci 289:437–444. https://doi.org/10.1016/j.apsusc.2013.10.18610.1016/j.apsusc.2013.10.186 ↗
41. Andrzej Studnicki JJ (2012) Stereological parameters of carbides in modified wear resistant Fe-C-Cr alloys. METAL 2012—conference proceedings, 21st international conference on metallurgy and materials 2012, pp 795–802.
42. Kopyciński D (2013) The inoculation of white cast iron. TMS2013 Annual Meeting Supplemental Proceedings, 2013.10.1002/9781118663547.ch75 ↗
43. Aso S et al (2016) The effect of solidification conditions on phase transformation of iron matrix of Fe-25mass%Cr-C-B alloys. Int J Cast Met Res 11(5):285–290. https://doi.org/10.1080/13640461.1999.1181928710.1080/13640461.1999.11819287 ↗
44. Scandian C et al (2009) Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: The relationship between microstructure and wear. Wear 267(1–4):401–408. https://doi.org/10.1016/j.wear.2008.12.09510.1016/j.wear.2008.12.095 ↗
45. S. Atamert, Bhadeshia HKDH (1990) Silicon modification of iron base hardfacing alloys. In: David A, Vitek JM (eds) Recent trends in welding science and technology (TWR'89), Materials Park, Ohio, pp 273–278.
46. Powel G, Randle V (1997) The effect of Si on the relationship between orientation and carbide morphology in high chromium white irons. J Mater Sci 32:561–565. https://doi.org/10.1023/A:101855892891610.1023/A:1018558928916 ↗
47. Jain A-S et al (2020) Refinement of primary carbides in hypereutectic high-chromium cast irons: a review. J Mater Sci 56(2):999–1038. https://doi.org/10.1007/s10853-020-05260-810.1007/s10853-020-05260-8 ↗
48. Liu Z (2017) Review of grain refinement of cast metals through inoculation: theories and developments. Metall Mater Trans A 48(10):4755–4776. https://doi.org/10.1007/s11661-017-4275-710.1007/s11661-017-4275-7 ↗
49. John DH, Qian M, Easton MA. Peng Cao, Zoë Hildebrand (2005) Grain refinement of magnesium alloy. Metall Mater Trans A 36A:1669–167910.1007/s11661-005-0030-6 ↗
50. AL Greer PC, Meredith MW, Schneider W, Schumacher P, Spittle JA, Tronche A (2003) Grain refinement of aluminium alloys by inoculation. Adv Eng Mater 5:81–91.10.1002/adem.200390013 ↗
51. Qian M et al (2010) An analytical model for constitutional supercooling-driven grain formation and grain size prediction. Acta Mater 58(9):3262–3270. https://doi.org/10.1016/j.actamat.2010.01.05210.1016/j.actamat.2010.01.052 ↗
52. Quested T, Dinsdale A, Greer A (2005) Thermodynamic modelling of growth-restriction effects in aluminium alloys. Acta Mater 53(5):1323–1334. https://doi.org/10.1016/j.actamat.2004.11.02410.1016/j.actamat.2004.11.024 ↗
53. Wang F et al (2013) Revisiting the role of peritectics in grain refinement of Al alloys. Acta Mater 61(1):360–370. https://doi.org/10.1016/j.actamat.2012.09.07510.1016/j.actamat.2012.09.075 ↗
54. Wang F et al (2013) The grain refinement mechanism of cast aluminium by zirconium. Acta Mater 61(15):5636–5645. https://doi.org/10.1016/j.actamat.2013.05.04410.1016/j.actamat.2013.05.044 ↗
55. Liu Y, Liu X, Xiufang B (2004) Grain refinement of Mg–Al alloys with Al4C3–SiC/Al master alloy. Mater Lett 58(7–8):1282–1287. https://doi.org/10.1016/j.matlet.2003.09.02210.1016/j.matlet.2003.09.022 ↗
56. Lu L, Dahle AK, StJohn DH (2005) Grain refinement efficiency and mechanism of aluminium carbide in Mg–Al alloys. Scripta Mater 53(5):517–522. https://doi.org/10.1016/j.scriptamat.2005.05.00810.1016/j.scriptamat.2005.05.008 ↗
57. StJohn DH et al (2011) The interdependence theory: the relationship between grain formation and nucleant selection. Acta Mater 59(12):4907–4921. https://doi.org/10.1016/j.actamat.2011.04.03510.1016/j.actamat.2011.04.035 ↗
58. John DH, Easton MA (2001) A model of grain refinement incorporating alloy constitution and potency of heterogenous nucleant particles. Acta Mater 49:1867–1878.10.1016/S1359-6454(00)00368-2 ↗
59. Desnain P, Fautrelle Y, Meyer J-L, Riquet J-P, Durand F (1990) Prediction of equiaxed grain density in multicomponent alloys, stirred electromagnetically. Acta Metall Mater 38:1513–1523.10.1016/0956-7151(90)90119-2 ↗
60. Schmid-Fetzer R, Kozlov A (2011) Thermodynamic aspects of grain growth restriction in multicomponent alloy solidification. Acta Mater 59(15):6133–6144. https://doi.org/10.1016/j.actamat.2011.06.02610.1016/j.actamat.2011.06.026 ↗
61. Andersson J-O, Lars Höglund TH, Pingfang Shi, Bo Sundman (2002) Thermo-Calc and DICTRA, Computational Tools for Materials Science. Calphad 26(2):273–312.10.1016/S0364-5916(02)00037-8 ↗
62. Mason P, Nicholas Grundy A, Rettig R, Kjellqvist L, Jeppsson J, Bratberg J (2020) The application of an effective equilibrium reaction zone model based on CALPHAD thermodynamics to steel making. In: Peng Z. et al. (eds) 11th international symposium on high-temperature metallurgical processing. The minerals, metals & materials series. Springer, Cham. https://doi.org/10.1007/978-3-030-36540-0_10.10.1007/978-3-030-36540-0_10 ↗
63. TCFE7 Steels/Fe-alloys Database Version 7.0. Thermo-Calc Software.
64. Mark Easton DS (1999) Grain refinement of aluminum alloys—part II. confirmation of, and a mechanism for, the solute paradigm. Metall Mater Trans A 30A:1625–1633.10.1007/s11661-999-0099-4 ↗
65. Ali Y et al (2016) Grain coarsening of cast magnesium alloys at high cooling rate: a new observation. Metall Mater Trans A 48(1):474–481. https://doi.org/10.1007/s11661-016-3852-510.1007/s11661-016-3852-5 ↗
66. Hinckley B, Dolman KF, Wuhrer R, Yeung W, Ray A (2008) SEM investigation of heat treated high-chromium cast irons. Mater Forum 32:55–71.
67. Nikolaenko MR, Grinberg NA (1973) Influence of boron, vanadium and nickel on the structure and properties of high chromium cast irons deposited with powder-filled strip. Welding Prod 20(4):56–60.
68. Li P et al (2020) Mechanical behavior and microstructure of hypereutectic high chromium cast iron: the combined effects of tungsten, manganese and molybdenum additions. J Market Res 9(3):5735–5748. https://doi.org/10.1016/j.jmrt.2020.03.09810.1016/j.jmrt.2020.03.098 ↗
69. Nofal A et al (2010) Structural refinement of 15%Cr-2%Mo White Irons. Key Eng Mater 457:231–236. https://doi.org/10.4028/www.scientific.net/KEM.457.23110.4028/www.scientific.net/KEM.457.231 ↗
70. Wu X et al (2007) Effect of titanium on the morphology of primary M7C3 carbides in hypereutectic high chromium white iron. Mater Sci Eng A 457(1–2):180–185. https://doi.org/10.1016/j.msea.2006.12.00610.1016/j.msea.2006.12.006 ↗