The role of carbon and tungsten disulphide nanotubes in the fracture of polymer-interlayered ceramic composites: a microscopy study
Source abstract
Abstract
Multi-walled carbon nanotubes (MWNT) and tungsten disulphide nanotubes (WS2-INT) have been widely used to improve the strength and toughness of composite materials. The mechanisms of such improvements are extensively studied, but it is not often clear what prompts a specific reinforcement mechanism to work. In this work we prepared two similar systems reinforced with different nanofillers (MWNT and WS2-INT). Using in situ optical microscopy and post-fracture electron microscopy, we established that using different nanofillers results in a different type of fracture and a different reinforcement mechanism. When compared to non-reinforced composites both systems showed significant improvements in both strength and fracture toughness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Coleman JN, Khan U, Blau WJ, Gun’ko YK (2006) Small but strong: a review of the mechanical properties of carbon nanotube–polymer composites. Carbon 44:1624–165210.1016/j.carbon.2006.02.038 ↗
2. Tenne R, Rosentsveig R, Zak A (2013) Inorganic nanotubes and fullerene-like nanoparticles: synthesis, mechanical properties, and applications. Phys Status Solidi A 210:2253–225810.1002/pssa.201329309 ↗
3. Naskar AK, Keum JK, Boeman RG (2016) Polymer matrix nanocomposites for automotive structural components. Nat Nanotech 6:1026–103010.1038/nnano.2016.262 ↗
4. Dzenis Y (2008) Structural nanocomposites. Science 314:419–42010.1126/science.1151434 ↗
5. Yu M-F, Lourie O, Dyer MJ, Moloni K, Kelly TF, Ruoff RS (2000) Strength and breaking mechanism of multiwalled carbon nanotubes under tensile load. Science 287:637–64010.1126/science.287.5453.637 ↗
6. Kaplan-Ashiri I, Tenne R (2016) On the mechanical properties of WS2 and MoS2 nanotubes and fullerene-like nanoparticles: in situ electron microscopy measurements. JOM 68:151–16710.1007/s11837-015-1659-2 ↗
7. Barber AH, Kaplan-Ashiri I, Cohen SR, Tenne R, Wagner HD (2005) Stochastic strength of nanotubes: an appraisal of available data. Compos Sci Technol 65:2380–238410.1016/j.compscitech.2005.07.021 ↗
8. Dufresne A, Paillet M, Putaux JL, Canet R, Carmona F, Delhaes P, Cui S (2002) Processing and characterization of carbon nanotube/poly(styrene- co-butyl acrylate) nanocomposites. J Mater Sci 37:3915–3923. doi: 10.1023/A:101965962456710.1023/A:1019659624567 ↗
9. Gorga RE, Cohen RE (2004) Toughness enhancements in poly(methyl methacrylate) by addition of oriented multiwall carbon nanotubes. J Polym Sci Part B Polym Phys 42:2690–270210.1002/polb.20126 ↗
10. Zhang W, Ge S, Wang Y, Rafailovich MH, Dhez O, Winesett DA, Ade H, Shafi KVPM, Ulman A, Popovitz-Biro R, Tenne R, Sokolov J (2003) Use of functionalized WS2 nanotubes to produce new polystyrene/polymethylmethacrylate nanocomposites. Polymer 44:2109–211510.1016/S0032-3861(03)00053-3 ↗
11. Zohar E, Baruch S, Shneider M, Dodiuk H, Kenig S, Tenne R, Wagner HD (2011) The effect of WS2 nanotubes on the properties of epoxy-based nanocomposites. J Adhesion Sci Technol 25:1603–161710.1163/016942410X524138 ↗
12. Zhan GD, Kuntz JD, Wan J, Mukherjee AK (2003) Single-wall carbon nanotubes as attractive toughening agents in alumina-based nanocomposites. Nat Mater 2:38–4210.1038/nmat793 ↗
13. Wang X, Padture NP, Tanaka H (2004) Contact-damage-resistant ceramic/single-wall carbon nanotubes and ceramic/graphite composites. Nat Mater 3:539–54410.1038/nmat1161 ↗
14. Mirjalili V, Ramachandramoorthy R, Hubert P (2014) Enhancement of fracture toughness of carbon fiber laminated composites using multi wall carbon nanotubes. Carbon 79:413–42310.1016/j.carbon.2014.07.084 ↗
15. Veedu VP, Cao A, Li X, Ma K, Soldano C, Kar S, Ajayan PM, Ghasemi-Nejhad MN (2006) Multifunctional composites using reinforced laminae with carbon- nanotube forests. Nat Mater 5:457–46210.1038/nmat1650 ↗
16. Mamedov AA, Kotov NA, Prato M, Guldi DM, Wicksted JP, Hirsch A (2002) Molecular design of strong single-wall carbon nanotube/polyelectrolyte multilayer composites. Nat Mater 1:190–19410.1038/nmat747 ↗
17. Greenfeld I, Wagner HD (2015) Nanocomposite toughness, strength and stiffness: role of filler geometry. Nanocomposites 1:3–1710.1179/2055033214Y.0000000002 ↗
18. Eitan A, Fisher FT, Andrews R, Brinson LC, Schadler LS (2006) Reinforcement mechanisms in MWCNT-filled polycarbonate. Compos Sci Technol 66:1162–117310.1016/j.compscitech.2005.10.004 ↗
19. Livanov K, Yang L, Nissenbaum A, Wagner HD (2016) Interphase tuning for stronger and tougher composites. Sci Rep 6:2630510.1038/srep26305 ↗
20. Alhazov D, Zussman E (2012) Study of the energy absorption capabilities of laminated glass using carbon nanotubes. Compos Sci Technol 72:681–68710.1016/j.compscitech.2012.01.016 ↗
21. Evans AG (1990) Perspective on the development of high-toughness ceramics. J Am Ceram Soc 73:187–20610.1111/j.1151-2916.1990.tb06493.x ↗
22. Bouville F, Maire E, Meille S, Van de Moortèle B, Stevenson AJ, Deville S (2014) Strong, tough and stiff bioinspired ceramics from brittle constituents. Nat Mater 13:508–51410.1038/nmat3915 ↗
23. Launey ME, Ritchie RO (2009) On the fracture toughness of advanced materials. Adv Mater 21:2103–211010.1002/adma.200803322 ↗
24. Livanov K, Jelitto H, Bar-On B, Schulte K, Schneider GA, Wagner DH (2015) Tough alumina/polymer layered composites with high ceramic content. J Am Ceram Soc 98:1285–129110.1111/jace.13413 ↗
25. Mirkhalaf M, Dastjerdi AK, Barthelat F (2014) Overcoming the brittleness of glass through bio-inspiration and micro-architecture. Nat Commun 5:316610.1038/ncomms4166 ↗
26. Behr S, Köllner A, Schneider GA (2016) Tailoring toughness and mechanical reliability by controlled defects: nature-inspired composite laminates of laser-perforated yttria-stabilized zirconia. Adv Eng Mater 18(11):1877–188310.1002/adem.201600128 ↗
27. Behr S, Jungblut L, Swain MV, Schneider GA (2016) Shear strength and interfacial toughness characterization of sapphire-epoxy interfaces for nacre-inspired composites. ACS Appl Mater Interfaces 8(40):27322–2733110.1021/acsami.6b09050 ↗
28. Ritchie RO (2011) The conflicts between strength and toughness. Nat Mater 10:817–82210.1038/nmat3115 ↗
29. Norman DA, Robertson RE (2003) The effect of fiber orientation on the toughening of short fiber-reinforced polymers. J Appl Polym Sci 90:2740–275110.1002/app.12913 ↗
30. Drzal LT, Rich MJ, Lloyd PF (1983) Adhesion of graphite fibers to epoxy matrices: I. The role of fiber surface treatment. J Adhesion 16:1–3010.1080/00218468308074901 ↗
31. Leger L, Creton C (2008) Adhesion mechanisms at soft polymer interfaces. Phil Trans R Soc A 366:1425–144210.1098/rsta.2007.2166 ↗
32. Kim JK, Ma YW (1998) Engineered interfaces in fiber reinforced composite. 1st edn, Chapter 6. Elsevier, New York, pp 239–27710.1016/B978-008042695-2/50007-5 ↗
33. Livanov K, Nissenbaum A, Wagner HD (2016) Nanocomposite thin film coatings for brittle materials. Nanocomposites 2:162–16810.1080/20550324.2016.1254926 ↗
34. Vaisman L, Wagner HD, Marom G (2006) The role of surfactants in dispersion of carbon nanotubes. Adv Colloid Interface Sci 128–130:37–4610.1016/j.cis.2006.11.007 ↗
35. Kuebler J, Blugan G, Jelitto H, Schneider GA, Dobedoe R (2007) Structural micro-layered ceramics with surfaces under tension and compression with increasing apparent fracture toughness. Key Eng Mater 336–338:2564–256810.4028/www.scientific.net/KEM.336-338.2564 ↗
36. Jelitto H, Hackbarth F, Özcoban H, Schneider GA (2013) Automated control of stable crack growth for r-curve measurements in brittle materials. Exp Mech 53:163–17010.1007/s11340-012-9622-4 ↗
37. Jelitto H, Felten F, Swain MV, Balke H, Schneider GA (2007) Measurement of the total energy release rate for cracks in PZT under combined mechanical and electrical loading. J Appl Mech 74:1197–121110.1115/1.2744027 ↗
38. Krause RF Jr (1988) Rising fracture toughness from the bending strength of indented alumina beams. J Am Ceram Soc 71:338–34310.1111/j.1151-2916.1988.tb05051.x ↗
39. Tattersall HG, Tappin G (1966) The work of fracture and its measurement in metals, ceramics and other materials. J Mater Sci 1:296–301. doi: 10.1007/BF0055017710.1007/BF00550177 ↗
40. dos Santos SF, Rodrigues JA (2003) Correlation between fracture toughness, work of fracture and fractal dimensions of alumina-mullite-zirconia composites. Mater Res 6:219–22210.1590/S1516-14392003000200017 ↗
41. Piggott M (2002) Load bearing fibre composites, 2nd edn, Chapter 6, Kluwer, p 196
42. Belenky A, Rittel D (2012) Static and dynamic flexural strength of 99.5% alumina: relation to porosity. Mech Mater 48:43–5510.1016/j.mechmat.2012.01.006 ↗
43. Asloun EM, Nardin M, Schultz J (1989) Stress transfer in single-fibre composites: effect of adhesion, elastic modulus of fibre and matrix, and polymer chain mobility. J Mater Sci 24:1835–1844. doi: 10.1007/BF0110571310.1007/BF01105713 ↗
44. Yang L, He X, Mei L, Tong L, Wanga R, Li Y (2012) Interfacial shear behavior of 3D composites reinforced with CNT-grafted carbon fibers. Compos A 43:1410–141810.1016/j.compositesa.2011.11.012 ↗
45. Yang L, Greenfeld I, Wagner HD (2016) Toughness of carbon nanotubes conforms to classic fracture mechanics. Sci Adv 2:e150096910.1126/sciadv.1500969 ↗