Investigation on (100) face of KDP crystal poisoned by MoO4 2− impurity
Source abstract
Abstract
Potassium dihydrogen phosphate (KDP) single crystals doped with molybdate (MoO4 2−) were grown via the conventional temperature cooling and rapid growth methods, respectively. MoO4 2− made KDP crystals tapering for conventional temperature cooling method. When KDP crystals were grown by rapid growth method, MoO4 2− could induce liquid inclusions and simultaneous crystals. The measurement on growth rates indicated that MoO4 2− broadened the dead zone and decreased the growth rate of (100) face of KDP crystals. The growth kinetic analysis in terms of two-dimensional nucleus and screw dislocation models implied that the energetic parameter γ/kT decreased with an increase of MoO4 2− concentration. The influence of MoO4 2− growth steps on (100) face of KDP crystal was observed through ex situ AFM technique. It gave evidence that MoO4 2− could postpone the step bunching and make the step edge curving and knaggy to reduce the edge free energy, which was in agreement with the growth kinetics calculations. Additionally, the poisoned mechanism of MoO4 2− and Fe3+ on step morphologies was detailed contrasted. The interaction process was discussed according to electro negativity analysis, which indicated MoO4 2− (actually were HMoO4 − and H2MoO4) could be absorbed onto (100) face through charge-assisted hydrogen bonds and caused more Mo element distributed in prismatic sector.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nonlinear Optical Materials Research · Crystallization and Solubility Studies · Crystallography and molecular interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Yoshida H, Jitsuno T, Fujita H et al (2000) Appl Phys B 70:19510.1007/s003400050032 ↗
2. Sasaki T, Yokotani A (1990) J Cryst Growth 99:82010.1016/S0022-0248(08)80033-4 ↗
3. Balamurugan S, Bhagavannarayana G, Ramasamy P (2008) Mater Lett 62:396310.1016/j.matlet.2008.05.047 ↗
4. Kubota N, Sasaki S, Doki N, Minamikawa N, Yokota M (2004) Cryst Growth Des 4:53310.1021/cg034254i ↗
5. Wang B, Fang CS, Wang SL, Sun X et al (2006) J Cryst Growth 297:35210.1016/j.jcrysgro.2006.09.037 ↗
6. Rashkovich LN, Kronsky NV (1997) J Cryst Growth 182:43410.1016/S0022-0248(97)00360-6 ↗
7. Kannan V, Bairava Ganesh R, Sathyalakshmi R et al (2006) Cryst Res Tech 41:67810.1002/crat.200510648 ↗
8. Fu YJ, Gao ZS, Liu JM et al (1999) J Cryst Growth 198(199):682
9. Kuznetsov VA, Okhrimenko TM, Rak Mirosława (1998) J Cryst Growth 193:16410.1016/S0022-0248(98)00489-8 ↗
10. Li GH, Li XP, Su GB et al (2005) J Cryst Growth 274:55510.1016/j.jcrysgro.2004.10.052 ↗
11. Zhang JQ, Wang SL, Fang CS et al (2005) Functional Mat 36:1505 (in Chinese)
12. Li L, Zhao X, Sun X, Sun XQ (2006) Opt Express 14:1219610.1364/OE.14.012196 ↗
13. Zhong WZ, Luo HS, Hua SK, Xu GS (2004) J Syn Cryst 33:471
14. Seif S, Chang JM, Bhat K et al (2001) Cryst Growth Des 1:35910.1021/cg010002a ↗
15. Liu B, Fang CS, Wang SL et al (2008) Cryst Res Tech 43:70010.1002/crat.200711093 ↗
16. Sangwal K (1999) J Cryst Growth 203:19710.1016/S0022-0248(99)00048-2 ↗
17. Owczarek I, Sangwal (1990) J Cryst Growth 102:57410.1016/0022-0248(90)90416-I ↗
18. Kubota N, Yokota M, Mullin JW (1997) J Cryst Growth 182:8610.1016/S0022-0248(97)00328-X ↗
19. Eremina TA, Kuznestov VA, Eremin NN et al (2005) J Cryst Growth 273:58610.1016/j.jcrysgro.2004.09.068 ↗
20. Land TA, Martin TL, Potapenko S et al (1999) Nature 399:44210.1038/20886 ↗
21. Asakuma Y, Jee L, Nishimura M et al (2008) J Mol Struc: Theochem 851:22510.1016/j.theochem.2007.11.017 ↗
22. De Vries SA, Goedtkindt P, Bennett SL et al (1998) Phys Rev Lett 80:222910.1103/PhysRevLett.80.2229 ↗
23. Braga D, Grepioni F (2007) Making crystals by design. Wiley-VCH Verlag GmbH and Co. KGaA, Weinheim, p 39