journal article·2022-08

Effects of destabilization and tempering on microstructure and mechanical properties of a hypereutectic high-chromium cast iron

Abhi-Shek Jain, Muhammad Ikhmal Mustafa, Mohd Izzat Iskandar Mohd Sazili, Haiwei Chang, Ming-Xing Zhang

Journal of Materials Science· Volume 57· Issue 32
Publisher page

Abstract

The components made out of hypereutectic high-chromium cast iron (HCCI), featured with high abrasion resistance and hardness, are usually subjected to destabilization treatment before use, to improve their hardness and wear resistance by destabilizing the retained austenite which transforms to martensite. This study investigates the effects of destabilization and tempering heat treatment on the microstructure and mechanical properties of an HCCI with and without modification of primary carbides. For the unmodified HCCI, the destabilization simultaneously increased both hardness and the transverse rupture strength (TRS). Increasing the destabilization temperature from 970 to 1090 degrees C led to a marginal decrease in hardness and slight increase in TRS. Destabilization at 1090 degrees C increased the transverse rupture strength (TRS) by 54% compared to the as-cast HCCI without reduction in wear resistance due to the coarsening of the secondary carbides. In addition, tempering within a temperature range from 200 to 280 degrees C after destabilization at 1090 degrees C led to a slight decrease in hardness, but an increase in TRS and wear resistance. Further increasing the tempering temperature to 310, 340 and 400 degrees C did not vary the properties. Tempering at 280 degrees C after destabilization at 1090 degrees C enabled more than 85% increase in TRS compared to the as-cast HCCI. The influence of destabilization temperature on the TiB2-modified HCCI is similar to the unmodified alloy. But, tempering after destabilization at 1090 degrees C decreased both hardness and TRS without significant variation of wear resistance even though a TRS peak was obtained at 310 degrees C tempering. Hence, to achieve the best performance an optimized heat treatment for the unmodified HCCI is destabilization at 1090 degrees C followed by tempering at 280 degrees C. For the TiB2-modified HCCI, tempering is not needed. Rationalizations of the mechanical properties are also discussed in terms of microstructure.[GRAPHICS].
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Gahr KHZ, Doane DV (1980) Optimizing fracture toughness and abrasion resistance in white cast irons. Metall Trans A 11(4):613–62010.1007/BF02670698 ↗
2. Gahr KHZ, Scholz WG (1980) Fracture toughness of white cast irons. J Metals 32:38–44
3. Anon, (1978) Cast Iron- A review of recent developments, Eng Mater Des 22(3), 60–65
4. Bedolla-Jacuinde A, Correa R, Quezada JG, Maldonado C (2005) Effect of titanium on the as-cast microstructure of a 16%chromium white iron. Mater Sci Eng A 398(1–2):297–30810.1016/j.msea.2005.03.072 ↗
5. Sare BKAIR (1995) The effect of heat treatment on the gouging abrasion resistance of alloy white cast irons. Metall Mater Trans A 26A:357–370
6. Dogan GLIÖN, Hawk JA (1995) Abrasion resistance of the columnar zone in high Cr white cast irons. Wear 181–183:342–34910.1016/0043-1648(94)07056-3 ↗
7. Powell JVBGLF (1996) Secondary carbide precipitation in an 18 wt %Cr-1 wt % Mo white iron. J Mater Sci 31:707–711. https://doi.org/10.1007/BF0036788910.1007/BF00367889 ↗
8. Tabrett IRSCP, Ghomashchi MR (1996) Microstructure-property relationships in high chromium white iron alloys. Int Mater Rev 41:59–8210.1179/imr.1996.41.2.59 ↗
9. Zhang MX, Kelly PM, Gates JD (2001) The effect of heat treatment on the toughness, hardness and microstructure of low carbon white cast irons. J Mater Sci 36:3865–387510.1023/A:1017949600733 ↗
10. Wang J, Li C, Liu H, Yang H, Shen B, Gao S, Huang S (2006) The precipitation and transformation of secondary carbides in a high chromium cast iron. Mater Charact 56(1):73–7810.1016/j.matchar.2005.10.002 ↗
11. Hinckley KFDB, Wuhrer R, Yeung W, Ray A (2008) SEM investigation of heat treated high-chromium cast irons. Mater Forum 32:55–71
12. Karantzalis AE, Lekatou A, Mavros H (2008) Microstructural modifications of as-cast high-chromium white iron by heat treatment. J Mater Eng Perform 18(2):174–18110.1007/s11665-008-9285-6 ↗
13. Zhi X, Xing J, Gao Y, Fu H, Peng J, Xiao B (2008) Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron. Mater Sci Eng A 487(1–2):171–17910.1016/j.msea.2007.10.009 ↗
14. Karantzalis AE, Lekatou A, Diavati E (2009) Effect of destabilization heat treatments on the microstructure of high-chromium cast iron: a microscopy examination approach. J Mater Eng Perform 18(8):1078–108510.1007/s11665-009-9353-6 ↗
15. Liu Q, Hedström P, Zhang H, Wang Q, Jönsson P, Nakajima GK (2012) Effect of heat treatment on microstructure and mechanical properties of Ti-alloyed hypereutectic high chromium cast iron. ISIJ Int 52(12):2288–229410.2355/isijinternational.52.2288 ↗
16. Gasan H, Erturk F (2013) Effects of a destabilization heat treatment on the microstructure and abrasive wear behavior of high-chromium white cast iron investigated using different characterization techniques. Metall Mater Trans A 44(11):4993–500510.1007/s11661-013-1851-3 ↗
17. Lai JP, Pan QL, Wang ZB, Cui HR, Wang XD, Gao ZZ (2017) Effects of destabilization temperature on the microstructure and mechanical properties of high chromium cast iron. J Mater Eng Perform 26(10):4667–467510.1007/s11665-017-2943-9 ↗
18. Guitar MA, Suárez S, Prat O, Duarte Guigou M, Gari V, Pereira G, Mücklich F (2018) High chromium cast irons: destabilized-subcritical secondary carbide precipitation and its effect on hardness and wear properties. J Mater Eng Perform 27(8):3877–388510.1007/s11665-018-3347-1 ↗
19. Gelfi M, Pola A, Girelli L, Zacco A, Masotti M, La Vecchia GM (2019) Effect of heat treatment on microstructure and erosion resistance of white cast irons for slurry pumping applications. Wear 428–429:438–44810.1016/j.wear.2019.03.011 ↗
20. Sare IR, Arnold BK (1995) The influence of heat treatment on the high-stress abrasion resistance and fracture toughness of alloy white cast irons. Metall Mater Trans A 26:1785–179310.1007/BF02670766 ↗
21. Abdel-Aziz K, El-Shennawy M, Omar AA (2017) Microstructural characteristics and mechanical properties of heat treated high-Cr white cast iron alloys. Int J Appl Eng Res 12:4675–4686
22. Al-Rubaie KS, Preti O, Pohl M (2016) On the abrasion of heat-treated 2.8 C21Cr1Mo white cast iron. Int J Mater Res 107:815–82310.3139/146.111408 ↗
23. Liu H-H, Wang J, Yang H-S, Shen B-L, Gao S-J, Huang S-J (2006) Effect of cryogenic treatment on property of 14Cr2Mn2V high chromium cast iron subjected to subcritical treatment. J Iron Steel Res Int 13(6):43–4810.1016/S1006-706X(06)60108-8 ↗
24. Yilmaz SO, Teker T (2016) Effect of TiBAl inoculation and heat treatment on microstructure and mechanical properties of hypereutectic high chromium white cast iron. J Alloy Compd 672:324–33110.1016/j.jallcom.2016.02.125 ↗
25. Karantzalis AE, Lekatou A, Kapoglou A, Mavros H, Dracopoulos V (2011) Phase transformations and microstructural observations during subcritical heat treatments of a high-chromium cast iron. J Mater Eng Perform 21(6):1030–103910.1007/s11665-011-9995-z ↗
26. Guo Z-H, Xiao F-R, Lu S-L, Li H-Y, Liao B (2016) Effects of heat-treatment on the microstructure and wear resistance of a high-chromium cast iron for rolls. Adv Mater Sci Eng 2016:1–7
27. Efremenko VG, Wu KM, Chabak YG, Shimizu K, Isayev OB, Kudin VV (2018) Alternative heat treatments for complex-alloyed high-Cr cast iron before machining. Metall Mater Trans A 49(8):3430–344010.1007/s11661-018-4722-0 ↗
28. Huang JXZ, Zhang A (2006) Investigation of microstructure and impact toughness of semisolid hypereutectic high chromium cast iron prepared by slope cooling body method. J Appl Sci 6:1635–164010.3923/jas.2006.1635.1640 ↗
29. Fu H-G, Wu X-J, Li X-Y, Xing J-D, Lei Y-P, Zhi X-H (2009) Effect of TiC particle additions on structure and properties of hypereutectic high chromium cast iron. J Mater Eng Perform 18(8):1109–111510.1007/s11665-008-9330-5 ↗
30. Jain A-S, Chang H, Tang X, Hinckley B, Zhang M-X (2020) Refinement of primary carbides in hypereutectic high-chromium cast irons: a review. J Mater Sci 56(2):999–1038. https://doi.org/10.1007/s10853-020-05260-810.1007/s10853-020-05260-8 ↗
31. Jain AS, Chang H, Zhang MX (2021) Effect of TiB2 addition on microstructure and mechanical properties of a hypereutectic high chromium cast iron. J Mater Sci 56:19047–19059. https://doi.org/10.1007/s10853-021-06429-510.1007/s10853-021-06429-5 ↗
32. A. International, Standard Test Method for Transverse Rupture Strength of Powder Metallurgy (PM) Specimens, (2016)
33. Tabrett IRSCP (1998) Effect of high temperature and sub-ambient treatments on the matrix structure and abrasion resistance of a high-chromium white iron. Scripta Mater 38:1747–175310.1016/S1359-6462(98)00118-3 ↗
34. Babu SS, Bhadeshia HKDH (1995) Diffusion of carbon in substitutionally alloyed austenite. J Mater Sci Lett 14:314–31610.1007/BF00592135 ↗
35. Wiengmoon TCA, Pearce JTH (2004) A microstructural study of destabilised 30wt%Cr–2.3wt%C high chromium cast iron. ISIJ Int 44:396–40310.2355/isijinternational.44.396 ↗
36. Wiengmoon A, Chairuangsri T, Poolthong N, Pearce JTH (2008) Electron microscopy and hardness study of a semi-solid processed 27wt%Cr cast iron. Mater Sci Eng A 480(1–2):333–34110.1016/j.msea.2007.07.043 ↗
37. Wang J, Xiong J, Fan H, Yang H-S, Liu H-H, Shen B-L (2009) Effects of high temperature and cryogenic treatment on the microstructure and abrasion resistance of a high chromium cast iron. J Mater Process Technol 209(7):3236–324010.1016/j.jmatprotec.2008.07.035 ↗
38. Purba RH, Shimizu K, Kusumoto K, Gaqi Y, Todaka T (2022) Effect of boron addition on three-body abrasive wear characteristics of high chromium based multi-component white cast iron. Mater Chem Phys 275:12523210.1016/j.matchemphys.2021.125232 ↗
39. Pearce JTH (1983) Examination of M7C3 carbides in high chromium cast irons using thin foil transmission electron microscopy. J Mater Sci Lett 2:428–43210.1007/BF00723685 ↗
40. Higuera-Cobos FDDOF, Mesa-Grajales DH (2016) Improvement of abrasive wear resistance of the high chromium cast iron ASTM A-532 through thermal treatment cycles. Fac Ing 25:93–10310.19053/01211129.4141 ↗
41. Guitar MA, Nayak UP, Britz D, Mücklich F (2020) The effect of thermal processing and chemical composition on secondary carbide precipitation and hardness in high-chromium cast irons. Int J Metalcast 14(3):755–76510.1007/s40962-020-00407-4 ↗
42. Kopyciński EGD, Siekaniec D, Szczesny A (2014) Analysis of the high chromium cast iron microstructure after the heat treatment. Arch Foundry Eng 14:43–4610.2478/afe-2014-0059 ↗
43. Ortega-Cubillos P, Nannetti-Bernardini PA, Celso-Fredel M, Antonio Campos R, (2015) Wear resistance of high chromium white cast iron for coal grinding rolls, Revista Facultad de Ingeniería Universidad de Antioquia (76)10.17533/udea.redin.n76a16 ↗
44. Maratray F, Poulalion A (1982) Austenite retention in high-chromium white irons. (retroactive coverage). Trans Am Foundrymen’s Soc 90:795–804
45. Inthidech S, Sricharoenchai P, Matsubara Y (2006) Effect of alloying elements on heat treatment behavior of hypoeutectic high chromium cast iron. Mater Trans 47:72–8110.2320/matertrans.47.72 ↗
46. Biner SB (1985) The role of eutectic carbide morphology on the fracture behaviour of high-chromium cast irons-ii. martensitic alloys. Can Metall Q 24:163–16710.1179/cmq.1985.24.2.163 ↗
47. Biner SB (1985) The role of eutectic carbide morphology on the fracture behavior of high-chromium cast irons-i. austenitic alloys. Can Metall Q 24:155–16210.1179/cmq.1985.24.2.155 ↗
48. Sare IR (1979) Abrasion resistance and fracture toughness of white cast irons. Metals Technol 6:412–41910.1179/030716979803276228 ↗
49. Gahr KHZ (1987) Microstructure and wear of materials. Elsevier, Amsterdam