Using particle-loaded inks to selectively change the material properties in binder-jetted WC–Co parts
Source abstract
Abstract
Abstract Functionally graded hardmetals offer a superior combination of fracture toughness and wear resistance and alleviate the compromise that conventional hardmetals must face between these two material properties. In tooling applications, they exhibit superior cutting performance compared to the conventionally employed hardmetals. Traditionally, graded tools are enabled by a surface treatment with nitrogen or carbon. This enables a tungsten carbide–cobalt (WC–Co) tool with a surface layer containing less cobalt (Co) than the core of the part. With this Co gradation, the wear properties can be improved due to the harder surface. If different loads act at different points in a tool and the geometric complexity of a tool increases, the requirements for a targeted positioning of the Co gradients become higher. A simple surface treatment does not allow a flexible distribution of the desired gradients. Binder jetting provides a solution to produce location-independent graded structures. In this work, the process was evaluated for the generation of Co gradients in WC–Co structures. Inks loaded with graphite particle contents of 2.5, 5, 7.5, and 10 m% were used to create differences in the carbon content in the green part. This induced a Co migration during the liquid phase sintering process. The sintering parameters were varied in time and temperature and studied regarding their effect on the microstructure and the porosity, the formation of the Co gradient, and the hardness. At low sintering times and temperatures, all carbon differences led to a Co gradient in the sintering part with a deviation of up to 10 m%. With an increase in sintering time and temperature, the Co distribution began to even out, and a deviation was observed only in the parts created with the inks containing 7.5 and 10 m% of particles. Hardness values of up to 1300 HV10 were obtained, which is comparable to conventionally produced WC–Co parts. The excess of carbon resulted in porosity in the parts leading to a reduced density. However, with inks containing 10 m% particles, densities of 94.26% were achieved at the longest sintering times and the highest temperature.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Tunneling and Rock Mechanics · Injection Molding Process and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Ren X, Miao H, Peng Z (2013) A review of cemented carbides for rock drilling: an old but still tough challenge in geo-engineering. Int J Refract Metal Hard Mater 39:61–77. https://doi.org/10.1016/j.ijrmhm.2013.01.00310.1016/j.ijrmhm.2013.01.003 ↗
2. Fang Z, Eso O (2005) Liquid phase sintering of functionally graded WC-Co composites. Scripta Mater 52:785–791. https://doi.org/10.1016/j.scriptamat.2004.12.00810.1016/j.scriptamat.2004.12.008 ↗
3. Upadhyaya GS (2001) Materials science of cemented carbides – an overview. Mater Des. 22:483–489. https://doi.org/10.1016/S0261-3069(01)00007-310.1016/S0261-3069(01)00007-3 ↗
4. Fan P, Fang ZZ, Guo J (2013) A review of liquid phase migration and methods for fabrication of functionally graded cemented tungsten carbide. Int J Refract Metal Hard Mater 36:2–9. https://doi.org/10.1016/j.ijrmhm.2012.02.00610.1016/j.ijrmhm.2012.02.006 ↗
5. Emanuelli L, Molinari A, Arrighetti G, Garoli G (2018) Effect of the sintering parameters on the liquid Co migration in WC-Co. Int J Refract Metal Hard Mater 70:202–209. https://doi.org/10.1016/j.ijrmhm.2017.10.01410.1016/j.ijrmhm.2017.10.014 ↗
6. Fan P, Guo J, Fang ZZ, Prichard P (2009) Design of cobalt gradient via controlling carbon content and WC grain size in liquid-phase-sintered WC-Co composite. Int J Refract Metal Hard Mater 27:256–260. https://doi.org/10.1016/j.ijrmhm.2008.08.00210.1016/j.ijrmhm.2008.08.002 ↗
7. Konyashin I, Zaitsev AA, Sidorenko D, Levashov EA, Ries B, Konischev SN et al (2017) Wettability of tungsten carbide by liquid binders in WC-Co cemented carbides: Is it complete for all carbon contents? Int J Refract Metal Hard Mater 62:134–148. https://doi.org/10.1016/j.ijrmhm.2016.06.00610.1016/j.ijrmhm.2016.06.006 ↗
8. Tokita M (2003) Large-Size-WC/Co Functionally Graded Materials Fabricated by Spark Plasma Sintering (SPS) Method. Mater Sci Forum 423:39–44. https://doi.org/10.4028/www.scientific.net/MSF.423-425.3910.4028/www.scientific.net/MSF.423-425.39 ↗
9. Lisovsky AF (1990) The migration of metal melts in sintered composite materials. Int J Heat Mass Transf 33:1599–1603. https://doi.org/10.1016/0017-9310(90)90016-N10.1016/0017-9310(90)90016-N ↗
10. Colin C, Durant L, Favrot N, Besson J, Barbier G, Delannay F (1993) Processing of functional-gradient WC-Co cermets by powder metallurgy. Int J Refract Metal Hard Mater 12:145–152. https://doi.org/10.1016/0263-4368(93)90064-M10.1016/0263-4368(93)90064-M ↗
11. Guo J, Fang ZZ, Fan P, Wang X (2011) Kinetics of the formation of metal binder gradient in WC-Co by carbon diffusion induced liquid migration. Acta Mater 59:4719–4731. https://doi.org/10.1016/j.actamat.2011.04.01910.1016/j.actamat.2011.04.019 ↗
12. Konyashin I, Ries B, Lachmann F, Fry AT (2013) Gradient WC-Co hardmetals: Theory and practice. Int J Refract Metal Hard Mater 36:10–21. https://doi.org/10.1016/j.ijrmhm.2011.12.01010.1016/j.ijrmhm.2011.12.010 ↗
13. Eso O, Fang ZZ, Griffo A (2007) Kinetics of cobalt gradient formation during the liquid phase sintering of functionally graded WC-Co. Int J Refract Metal Hard Mater 25(4):286–292. https://doi.org/10.1016/j.ijrmhm.2006.07.00210.1016/j.ijrmhm.2006.07.002 ↗
14. Fan P, Eso OO, Fang ZZ, Sohn HY (2008) Effect of WC particle size on Co distribution in liquid-phase-sintered functionally graded WC-Co composite. Int J Refract Metal Hard Mater 26(2):98–105. https://doi.org/10.1016/j.ijrmhm.2007.02.00310.1016/j.ijrmhm.2007.02.003 ↗
15. Fischer U AJ Hartzell E.: Cemented carbide body used preferbaly for rock drilling and mineral cutting. Google Patents. US Patent 4,743,515. Available from: https://patents.google.com/patent/US4743515A/en
16. Yang Y, Zhang C, Wang D, Nie L, Wellmann D, Tian Y (2020) Additive manufacturing of WC-Co hardmetals: a review. Int J Adv Manuf Technol 108:1653–1673. https://doi.org/10.1007/s00170-020-05389-510.1007/s00170-020-05389-5 ↗
17. Berger C, Pötschke J, Abel A, Richter HJ, Scheithauer U, Weingarten S (2019) Additive Manufacturing of WC-Co Based Tools. Proceedings of 11th TOOLING 2019 conference, Aachen
18. Enneti RK, Prough KC, Wolfe TA, Klein A, Studley N, Trasorras JL (2018) Sintering of WC-12%Co processed by binder jet 3D printing (BJ3DP) technology. Int J Refract Metal Hard Mater 71:28–35. https://doi.org/10.1016/j.ijrmhm.2017.10.02310.1016/j.ijrmhm.2017.10.023 ↗
19. Mariani M, Goncharov I, Mariani D, de Gaudenzi GP, Popovich A, Lecis N et al (2021) Mechanical and microstructural characterization of WC-Co consolidated by binder jetting additive manufacturing. Int J Refract Metal Hard Mater 100:105639. https://doi.org/10.1016/j.ijrmhm.2021.10563910.1016/j.ijrmhm.2021.105639 ↗
20. Mostafaei A, Elliott AM, Barnes JE, Li F, Tan W, Cramer CL et al (2021) Binder jet 3D printing–Process parameters, materials, properties, modeling, and challenges. Prog Mater Sci 119:100707. https://doi.org/10.1016/j.pmatsci.2020.10070710.1016/j.pmatsci.2020.100707 ↗
21. Godlinski D, Morvan S (2005) Steel parts with tailored material gradients by 3D-printing using nano-particulate ink. Mater Sci Forum 492:679–684. https://doi.org/10.4028/www.scientific.net/MSF.492-493.67910.4028/www.scientific.net/MSF.492-493.679 ↗
22. Persembe E, Parra-Cabrera C, Clasen C, Ameloot R (2021) Binder-jetting 3D printer capable of voxel-based control over deposited ink volume, adaptive layer thickness, and selective multi-pass printing. Rev Sci Instrum 92:125106. https://doi.org/10.1063/5.007271510.1063/5.0072715 ↗
23. Lehmann M, Kolb CG, Klinger F, Zaeh MF (2021) Preparation, characterization, and monitoring of an aqueous graphite ink for use in binder jetting. Materials & Design. 207:109871. https://doi.org/10.1016/j.matdes.2021.10987110.1016/j.matdes.2021.109871 ↗
24. Kolb CG, Lehmann M, Lindemann JL, Bachmann A, Zaeh MF (2021) Improving the dispersion behavior of organic components in water-based electrode dispersions for inkjet printing processes. Appl Sci 11:2242. https://doi.org/10.3390/app1105224210.3390/app11052242 ↗
25. Polsakiewicz D (2018) Herstellung keramischer Komposite ueber den pulverbasierten Multi-Material-3D-Druck [Dissertation]. University of the Federal Armed Forces Hamburg
26. Traube J (1891) Über die Capillaritätsconstanten organischer Stoffe in wässerigen Lösungen. Justus Liebig’s Annalen der Chemie. 265:27–55. https://doi.org/10.1002/jlac.1891265010310.1002/jlac.18912650103 ↗
27. Schafnitzel M, Lutter-Guenther M, Schlick G (2019) Characterization of Commercially Available WC-Co Powders Used for Laser-based Powder Bed Fusion. Porceedings Euro PM2019 – HM and AM Fusion Processes, Maastricht
28. Bui HM, Fischer R, Szesni N, Tonigold M, Achterhold K, Pfeiffer F et al (2022) Development of a manufacturing process for Binder Jet 3D printed porous Al2O3 supports used in heterogeneous catalysis. Addit Manuf 50:102498. https://doi.org/10.1016/j.addma.2021.10249810.1016/j.addma.2021.102498 ↗
29. Upadhyaya GS (1998) Cemented tungsten carbides: Production, properties, and testing. Materials science and process technology series. Ceramic and other materials–processing and technology. Noyes Publications
30. Bhaumik SK, Upadhyaya GS, Vaidya ML (1996) Full density processing of complex WC-based cemented carbides. J Mater Process Technol 58(1):45–52. https://doi.org/10.1016/0924-0136(95)02106-X10.1016/0924-0136(95)02106-X ↗
31. Bounhoure V, Lay S, Coindeau S, Norgren S, Pauty E, Missiaen JM (2015) Effect of Cr addition on solid state sintering of WC-Co alloys. Int J Refract Metal Hard Mater 52:21–28. https://doi.org/10.1016/j.ijrmhm.2015.05.00210.1016/j.ijrmhm.2015.05.002 ↗
32. Nie H, Zhang T (2019) Development of manufacturing technology on WC-Co hardmetals. Tungsten. 1:198–212. https://doi.org/10.1007/s42864-019-00025-610.1007/s42864-019-00025-6 ↗
33. Enneti RK, Prough KC (2019) Effect of binder saturation and powder layer thickness on the green strength of the binder jet 3D printing (BJ3DP) WC-12%Co powders. Int J Refract Metal Hard Mater 84:104991. https://doi.org/10.1016/j.ijrmhm.2019.10499110.1016/j.ijrmhm.2019.104991 ↗
34. Barthel B, Janas F, Wieland S (2021) Powder condition and spreading parameter impact on green and sintered density in metal binder jetting. Powder Metall 64:378–386. https://doi.org/10.1080/00325899.2021.191292310.1080/00325899.2021.1912923 ↗
35. Prakash L (2014) Fundamentals and General Applications of Hardmetals, Comprehensive Hard Materials. Elsevier, Waltham, p 35
36. Armstrong RW (2011) The Hardness and Strength Properties of WC-Co Composites. Materials 4:1287–1308. https://doi.org/10.3390/ma407128710.3390/ma4071287 ↗
37. IKTS. Fraunhofer IKTS, editor.: Härte und Bindergehalt von Hartmetallen. Accessed 09 May 2023. https://www.ikts.fraunhofer.de/de/abteilungen/werkstoff_prozesscharakterisierung/sintern_charakterisierung/hartmetalle_cermets/materialentwicklung_hartmetalle_cermets.html