Mechanical behavior of surface-patterned and coated Si or Ge wafers for superhydrophobic and antireflective light transmitting windows
Source abstract
Abstract
International audience ; The compressive resistance of truncated nanocone lattices produced by lithography and etching steps on Si or Ge wafers to get superhydrophobic and antireflective light transmitting windows, as well as the protection efficiency of alumina or diamond coatings are investigated by numerical simulations of elastic buckling, and nano-compression tests. The latter reveal the limits of an elastic analysis, since the stress at the top of the cones is high enough to trigger plastic flow, or phase changes. Ge nano-cones exhibit a large ductility in compression, and even seem to creep at room temperature. Thin alumina or diamond coatings are however shown to provide an effective protection against both buckling and plastic flow. Surface patterning is shown to induce stress concentrations at the foot of the cones, which reduces the fracture resistance of the substrate in biaxial bending.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Modification and Superhydrophobicity · Advanced Surface Polishing Techniques · Optical Coatings and Gratings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Mouterde T, Lehoucq G, Xavier S, Checco A, Black CT, Rahman A, Midavaine T, Clanet C, Quéré D (2017) Antifogging abilities of model nanotextures. Nat Mater 16:658–66410.1038/nmat4868 ↗
2. Park KC, Choi HJ, Chang CH, Cohen RE, McKinley GH, Barbastathis G (2012) Nanotextured Silica Surfaces with Robust Superhydrophobicity and Omnidirectional Broadband Supertransmissivity. ACS Nano 6:3789–379910.1021/nn301112t ↗
3. D. S. Hobbs (2009) Study of the Environmental and Optical Durability of AR Microstructures in Sapphire, ALON, and Diamond, Proc of SPIE, 7302, 73020J1-J1210.1117/12.818335 ↗
4. Infante D, Koch KW, Mazumder P, Tian L, Carrilero A, Tulli D, Baker D, Pruneri V (2013) Durable, superhydrophobic, antireflection, and low haze glass surfaces using scalable metal dewetting nanostructuring. Nano Res 6:429–44010.1007/s12274-013-0320-z ↗
5. P. Lecointre, S Laney, M. Michalska, T. Li, A. Tanguy, I. Papakonstantinou, D. Quéré (2021) Unique and universal dew-repellency of nanocones, Nature Communications, 12, 3458 (9 pages)10.1038/s41467-021-23708-6 ↗
6. M. Banik, P. Chakrabarty, A. Das, S. K. Ray, and R. Mukherjee (2019) Colloidal Transfer Printing–Mediated Fabrication of Zinc Oxide Nanorods for Self-Cleaning Applications, Adv. Mater. Interfaces 6, 1900063 (9 pages)10.1002/admi.201900063 ↗
7. Varughese SM, Bhandaru N (2020) Durability of Submerged Hydrophobic Surfaces. Soft Matter 16:1692–170110.1039/C9SM01942A ↗
8. Ghosh UU, Nair S, Das A, Mukherjee R, DasGupta S (2019) Replicating and resolving wetting and adhesion characteristics of a Rose petal. Colloids Surfaces A 561:9–1710.1016/j.colsurfa.2018.10.028 ↗
9. M. Reza Eslami (2018) Buckling and Postbuckling of Beams, Plates, and Shells (Structural Integrity Book 1), Springer, 1st Ed10.1007/978-3-319-62368-9 ↗
10. V. Beladiya, T. Faraz, W. M. M. Kessels, A. Tünnermann, A. Szeghalmi (2018) Controlling mechanical, structural and optical properties of Al2O3 thin films deposited by plasma-enhanced atomic layer deposition with substrate biasing, Proc. SPIE 10691, Advances in Optical Thin Films VI, 106910E (5 June 2018)10.1117/12.2312516 ↗
11. M. Cottance, S. Nazeer, L. Rousseau, G. Lissorgues, A. Bongrain, et al. (2013) Diamond micro-electrode arrays (MEAs) : A new route for in-vitro applications. 2013 Symposium on Design, Test, Integration and Packaging of MEMS/MOEMS (DTIP), Apr 2013, Barcelona, Spain. https://hal-cea.archives-ouvertes.fr/cea-01842332
12. Ankit K, Varade A, Niranjan Reddy K, Dhan S, Chellamalai M, Balashanmugam N, Krishna P (2017) Synthesis of high hardness IR optical coating using diamond-like carbon by PECVD at room temperature. Diam Relat Mater 78:39–4310.1016/j.diamond.2017.07.008 ↗
13. A.S. Grenadyorov, A.A. Solovyev, K.V. Oskomov, V.O. Oskirko, V.A. Semenov (2020) Thermal stability of anti-reflective and protective a-C:H:SiOx coating for infrared Optics, Applied Surface Science, 510, 145433 (9 pages)10.1016/j.apsusc.2020.145433 ↗
14. Craig JV, Pugh EN (1967) Fracture of germanium at room temperature. Acta Met. 15:1309–131510.1016/0001-6160(67)90006-5 ↗
15. Barnat S (2012) Evaluation by three-point-bend and ball-on-ring tests of thinning process on Silicon die strength. Microelectronics Reliability 52:2278–228210.1016/j.microrel.2012.06.093 ↗
16. McLaughlin JC, Willoughby AFW (1987) Fracture of silicon wafers. J Crystal Growth 85:83–9010.1016/0022-0248(87)90207-7 ↗
17. Wortman JJ, Evans RA (1965) Young’s modulus, Shear modulus, and Poisson’s ratio in silicon and germanium. J Appl Phys 36:153–15610.1063/1.1713863 ↗
18. Oliver WC, Pharr GM (1992) An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J Mater Res 7:1564–158310.1557/JMR.1992.1564 ↗
19. Gong MF, Qiao SR, Mei F (2014) Determining Young’s modulus and Poisson’s ratio of thin hard films. Surf Eng 30:589–59310.1179/1743294414Y.0000000288 ↗
20. M. Yang, S. Bai, Q. Xu, J. Li, T. Shimada, Q. Li, T. Goto, R. Tu, S. Zhang (2020) Mechanical properties of high-crystalline diamond films grown via laser MPCVD, Diamond Related Mater. 109, 108094 (8 pages)10.1016/j.diamond.2020.108094 ↗
21. Domnich V, Gogotsi Y (2002) Phase transformations in silicon under contact loading. Rev Adv Mater 3:1–3610.1016/S1468-6996(01)00150-4 ↗
22. Lee WS, Chang SL (2015) Nanoindentation behaviour and microstructural evolution of annealed single-crystal silicon Int. J Mater Metal Engng 9:799–803
23. J. Jang, M. J. Lance, S. Wen, G. M. Pharr. (2005), Evidence for nanoindentation-induced phase transformations in germanium, Appl Phys Lett, 86, 131907 (3 pages)10.1063/1.1894588 ↗
24. Ostlund F, Rzepiejewska-Malyska K, Leifer K, Hale LM, Tang Y, Ballarini R, Gerberich WW, Michler J (1987) Brittle-to-ductile transition in uniaxial compression of silicon pillars at room temperature. Adv funct Mater 19:2439–244410.1002/adfm.200900418 ↗
25. Wagner AJ, Hintsala ED, Kumar P, Gerberich WW, Mkhoyan KA (2015) Mechanisms of plasticity in near-theoretical strength sub-100 nm Si Nanocubes. Acta Mater 100:256–26510.1016/j.actamat.2015.08.029 ↗
26. Chrobak D, Tymiak N, Beaber A, Ugurlu O, Gerberich WW, Nowak R (2011) Deconfinement leads to changes in the nanoscale plasticity of silicon. Nat Nanotechnol 6:480–48410.1038/nnano.2011.118 ↗
27. Guenole J, Brochard S, Godet J (2011) Unexpected slip mechanism induced by the reduced dimensions in silicon nanostructures: atomistic study. Acta Mater 59:7464–747210.1016/j.actamat.2011.08.039 ↗