journal article·2017-09

Anti-bacterial properties of collagen-coated glass and polydimethylsiloxane substrates

Cheng Li, Yichen Ding, Shreyas Kuddannaya, Yilei Zhang, Liang Yang

Journal of Materials Science· Volume 52· Issue 17
Publisher page

Abstract

Attachments of three bacterial species, Escherichia coli, Staphylococcus aureus, and Pseudomonas aeruginosa on chemically modified glass slides and polydimethylsiloxane substrates were investigated with an attempt to find anti-bacterial materials which can prevent bacterial infections. The results showed that the attachment of the first two species was largely reduced on surfaces treated with self-assembled monolayers plus collagen type 1, whereas attachment of Pseudomonas aeruginosa was not affected on all the treated/untreated surfaces. Gentamicin protection assay showed that the fewest Pseudomonas aeruginosa were engulfed by macrophages when the substrates were coated with (3-aminopropyl)triethoxysilane/(3-aminopropyl)trimethoxysilane plus glutaraldehyde plus collagen type 1. Considering that both Pseudomonas aeruginosa and macrophage adhesion were not influenced very much by the chemical modifications, the decreased engulfment of Pseudomonas aeruginosa was attributed to its decreased ability to invade macrophage cells on the two coated substrates. The results indicate that by employing appropriate chemical modifications, bacterial adhesion could be weakened with a decreased bacterial engulfment response of macrophages to the coated substrates, which shows an interesting and promising direction for applicability of this surface modification strategy for future biomedical research on anti-inflammatory/anti-microbial cell-material interactions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Polymer Surface Interaction Studies · Antimicrobial agents and applications · Dental materials and restorations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Angelina JTT, Ganesan S, Panicker TMR et al (2016) Pulsed laser deposition of silver nanoparticles on prosthetic heart valve material to prevent bacterial infection. Mater Technol. doi: 10.1080/10667857.2016.116050310.1080/10667857.2016.1160503 ↗
2. Miller JD (2013) Cardiovascular calcification: orbicular origins. Nat Mater 12:476–478. doi: 10.1038/nmat366310.1038/nmat3663 ↗
3. Wang B, Takahashi S, Du X, Anzai JI (2014) Electrochemical biosensors based on ferroceneboronic acid and its derivatives: a review. Biosensors 4:243–256. doi: 10.3390/bios403024310.3390/bios4030243 ↗
4. Vigneshvar S, Sudhakumari CC, Senthilkumaran B, Prakash H (2016) Recent advances in biosensor technology for potential applications—an overview. Front Bioeng Biotechnol 4:11. doi: 10.3389/fbioe.2016.0001110.3389/fbioe.2016.00011 ↗
5. Ribeiro M, Monteiro FJ, Ferraz MP (2012) Infection of orthopedic implants with emphasis on bacterial adhesion process and techniques used in studying bacterial-material interactions. Biomatter 2:176–194. doi: 10.4161/biom.2290510.4161/biom.22905 ↗
6. Sousa C, Teixeira P, Bordeira S et al (2008) Staphylococcus epidermidis adhesion to modified polycarbonate surfaces: gold and SAMs coated. J Adhes Sci Technol 22:675–686. doi: 10.1163/156856108X30965710.1163/156856108X309657 ↗
7. Bridges AW, García AJ (2008) Anti-inflammatory polymeric coatings for implantable biomaterials and devices. J Diabetes Sci Technol 2:984–99410.1177/193229680800200628 ↗
8. Kenneth Ward W (2008) A review of the foreign-body response to subcutaneously-implanted devices: the role of macrophages and cytokines in biofouling and fibrosis. J Diabetes Sci Technol 2:768–777. doi: 10.1177/19322968080020050410.1177/193229680800200504 ↗
9. Ferraris S, Spriano S (2016) Antibacterial titanium surfaces for medical implants. Mater Sci Eng C 61:965–978. doi: 10.1016/j.msec.2015.12.06210.1016/j.msec.2015.12.062 ↗
10. Campoccia D, Montanaro L, Arciola CR (2006) The significance of infection related to orthopedic devices and issues of antibiotic resistance. Biomaterials 27:2331–2339. doi: 10.1016/j.biomaterials.2005.11.04410.1016/j.biomaterials.2005.11.044 ↗
11. Papadimitrakopoulos F, Ph D, Burgess DJ, Ph D (2008) A review of the biocompatibility of implantable devices: current challenges to overcome foreign body response. J Diabetes Sci Technol 2:1003–101510.1177/193229680800200610 ↗
12. Morais JM, Papadimitrakopoulos F, Burgess DJ (2010) Biomaterials/tissue interactions: possible solutions to overcome foreign body response. AAPS J 12:188–196. doi: 10.1208/s12248-010-9175-310.1208/s12248-010-9175-3 ↗
13. Ong YL, Razatos A, Georgiou G, Sharma MM (1999) Adhesion forces between E. coli bacteria and biomaterial surfaces. Langmuir 15:2719–272510.1021/la981104e ↗
14. Song F, Ren D (2014) Stiffness of cross-linked poly(dimethylsiloxane) affects bacterial adhesion and antibiotic susceptibility of attached cells. Langmuir. doi: 10.1021/la502029f10.1021/la502029f ↗
15. Truong VK, Lapovok R, Estrin YS et al (2010) The influence of nano-scale surface roughness on bacterial adhesion to ultrafine-grained titanium. Biomaterials 31:3674–3683. doi: 10.1016/j.biomaterials.2010.01.07110.1016/j.biomaterials.2010.01.071 ↗
16. Ivanova EP, Truong VK, Wang JY et al (2010) Impact of nanoscale roughness of titanium thin film surfaces on bacterial retention. Langmuir 26:1973–1982. doi: 10.1021/la902623c10.1021/la902623c ↗
17. Chen S, Li L, Zhao C, Zheng J (2010) Surface hydration: principles and applications toward low-fouling/nonfouling biomaterials. Polymer (Guildf) 51:5283–5293. doi: 10.1016/j.polymer.2010.08.02210.1016/j.polymer.2010.08.022 ↗
18. Tan HML, Fukuda H, Akagi T, Ichiki T (2007) Surface modification of poly(dimethylsiloxane) for controlling biological cells’ adhesion using a scanning radical microjet. Thin Solid Films 515:5172–5178. doi: 10.1016/j.tsf.2006.10.02610.1016/j.tsf.2006.10.026 ↗
19. Trentin DS, Silva DB, Frasson AP et al (2015) Natural green coating inhibits adhesion of clinically important bacteria. Sci Rep 5:8287. doi: 10.1038/srep0828710.1038/srep08287 ↗
20. Chen M, Yu Q, Sun H (2013) Novel strategies for the prevention and treatment of biofilm related infections. Int J Mol Sci 14:18488–18501. doi: 10.3390/ijms14091848810.3390/ijms140918488 ↗
21. Eichler M, Katzur V, Scheideler L et al (2011) The impact of dendrimer-grafted modifications to model silicon surfaces on protein adsorption and bacterial adhesion. Biomaterials 32:9168–9179. doi: 10.1016/j.biomaterials.2011.08.06310.1016/j.biomaterials.2011.08.063 ↗
22. Kuddannaya S, Chuah YJY, Lee MHA et al (2013) Surface chemical modification of poly(dimethylsiloxane) for the enhanced adhesion and proliferation of mesenchymal stem cells. ACS Appl Mater Interfaces 5:9777–9784. doi: 10.1021/am402903e10.1021/am402903e ↗
23. Chuah YJ, Kuddannaya S, Lee MHA et al (2015) The effects of poly(dimethylsiloxane) surface silanization on the mesenchymal stem cell fate. Biomater Sci 3:383–390. doi: 10.1039/C4BM00268G10.1039/C4BM00268G ↗
24. Webster TJ, Patel AA, Rahaman MN, Sonny Bal B (2012) Anti-infective and osteointegration properties of silicon nitride, poly(ether ether ketone), and titanium implants. Acta Biomater 8:4447–4454. doi: 10.1016/j.actbio.2012.07.03810.1016/j.actbio.2012.07.038 ↗
25. Toth JM, Wang M, Estes BT et al (2006) Polyetheretherketone as a biomaterial for spinal applications. Biomaterials 27:324–334. doi: 10.1016/j.biomaterials.2005.07.01110.1016/j.biomaterials.2005.07.011 ↗
26. Busscher HJ, Van Der Mei HC, Subbiahdoss G et al (2012) Biomaterial-associated infection: locating the finish line in the race for the surface. Sci Transl Med. doi: 10.1126/scitranslmed.300452810.1126/scitranslmed.3004528 ↗
27. Tegoulia VA, Cooper SL (2002) Staphylococcus aureus adhesion to self-assembled monolayers: effect of surface chemistry and fibrinogen presence. Coll Surf B Biointerfaces 24:217–228. doi: 10.1016/S0927-7765(01)00240-510.1016/S0927-7765(01)00240-5 ↗
28. Johnson JR (1991) Virulence factors in Escherichia coli urinary tract infection. Clin Microbiol Rev 4:80–128. doi: 10.1128/CMR.4.1.8010.1128/CMR.4.1.80 ↗
29. Oliver A, Canton R, Campo P et al (2000) High frequency of hypermutable Pseudomonas aeruginosa in cystic fibrosis lung infection. Science 288:1251–1254. doi: 10.1126/science.288.5469.125110.1126/science.288.5469.1251 ↗
30. Gillaspy AF, Lee CY, Sau S et al (1998) Factors affecting the collagen binding capacity of Staphylococcus aureus. Infect Immun 66:3170–317810.1128/IAI.66.7.3170-3178.1998 ↗
31. Smeltzer MS, Gillaspy AF, Pratt FL et al (1997) Prevalence and chromosomal map location of Staphylococcus aureus adhesin genes. Gene 196:249–259. doi: 10.1016/S0378-1119(97)00237-010.1016/S0378-1119(97)00237-0 ↗
32. Elasri MO, Thomas JR, Skinner RA et al (2002) Staphylococcus aureus collagen adhesin contributes to the pathogenesis of osteomyelitis. Bone 30:275–280. doi: 10.1016/S8756-3282(01)00632-910.1016/S8756-3282(01)00632-9 ↗
33. Stepinska M, Trafny EA (1995) Modulation of Pseudomonas aeruginosa adherence to collagen type I and type II by carbohydrates. FEMS Immunol Med Microbiol 12:187–194. doi: 10.1016/0928-8244(95)00066-610.1016/0928-8244(95)00066-6 ↗
34. Shen W, Ljungh A (1993) Microbiology collagen binding to Escherichia coli strain NG7C. Curr Microbiol 27:311–31610.1007/BF01568953 ↗
35. Wells TJ, McNeilly TN, Totsika M et al (2009) The Escherichia coli O157:h7 EhaB autotransporter protein binds to laminin and collagen i and induces a serum IgA response in O157:H7 challenged cattle. Environ Microbiol 11:1803–1814. doi: 10.1111/j.1462-2920.2009.01905.x10.1111/j.1462-2920.2009.01905.x ↗
36. Medina MB (2001) Binding of collagen I to Escherichia coli O157:H7 and inhibition by carrageenans. Int J Food Microbiol 69:199–208. doi: 10.1016/S0168-1605(01)00497-410.1016/S0168-1605(01)00497-4 ↗
37. Shahara S, White JD, Ross T, Tamplin ML (2012) Bacterial attachment to immobilized extracellular matrix proteins in vitro. Int J Food Microbiol 157:210–217. doi: 10.1016/j.ijfoodmicro.2012.05.00710.1016/j.ijfoodmicro.2012.05.007 ↗
38. Edwards AM, Massey RC (2011) Invasion of human cells by a bacterial pathogen. J Vis Exp. doi: 10.3791/269310.3791/2693 ↗
39. Lavalle P, Stoltz JF, Senger B et al (1996) Red blood cell adhesion on a solid/liquid interface. Proc Natl Acad Sci USA 93:15136–15140. doi: 10.1073/pnas.93.26.1513610.1073/pnas.93.26.15136 ↗
40. Zhang X, Jones P, Haswell SJ (2007) Attachment and detachment of living cells on modified microchannel surfaces in a microfluidic-based lab-on-a-chip system. Chem Eng J 135:82–88. doi: 10.1016/j.cej.2007.07.05410.1016/j.cej.2007.07.054 ↗
41. Bucior I, Pielage JF, Engel JN (2012) Pseudomonas aeruginosa pili and flagella mediate distinct binding and signaling events at the apical and basolateral surface of airway epithelium. PLoS Pathog. doi: 10.1371/journal.ppat.100261610.1371/journal.ppat.1002616 ↗
42. Petrova OE, Sauer K (2012) Sticky situations: key components that control bacterial surface attachment. J Bacteriol 194:2413–2425. doi: 10.1128/JB.00003-1210.1128/JB.00003-12 ↗
43. Yang M, Ding Y, Ge X, Leng Y (2015) Control of bacterial adhesion and growth on honeycomb-like patterned surfaces. Coll Surf B Biointerfaces 135:549–555. doi: 10.1016/j.colsurfb.2015.08.01010.1016/j.colsurfb.2015.08.010 ↗
44. Crawford RJ, Webb HK, Truong VK et al (2012) Surface topographical factors influencing bacterial attachment. Adv Colloid Interface Sci 179–182:142–149. doi: 10.1016/j.cis.2012.06.01510.1016/j.cis.2012.06.015 ↗
45. Bohinc K, Dražić G, Abram A et al (2016) Metal surface characteristics dictate bacterial adhesion capacity. Int J Adhes Adhes 68:39–46. doi: 10.1016/j.ijadhadh.2016.01.00810.1016/j.ijadhadh.2016.01.008 ↗
46. Xu LC, Siedlecki CA (2012) Submicron-textured biomaterial surface reduces staphylococcal bacterial adhesion and biofilm formation. Acta Biomater 8:72–81. doi: 10.1016/j.actbio.2011.08.00910.1016/j.actbio.2011.08.009 ↗
47. Maillard JY (2002) Bacterial target sites for biocide action. Symp Ser Soc Appl Microbiol 16S–27S. doi: 1622 [pii]10.1046/j.1365-2672.92.5s1.3.x ↗
48. Sehmi SK, Allan E, MacRobert AJ, Parkin I (2016) The bactericidal activity of glutaraldehyde-impregnated polyurethane. Microbiologyopen 5:891–897. doi: 10.1002/mbo3.37810.1002/mbo3.378 ↗
49. Bernstein R, Freger V, Lee J-HJ et al (2014) Should I stay or should I go? Bacterial attachment vs biofilm formation on surface-modified membranes. Biofouling 30:367–376. doi: 10.1080/08927014.2013.87601110.1080/08927014.2013.876011 ↗
50. Mansouri J, Harrisson S, Chen V (2010) Strategies for controlling biofouling in membrane filtration systems: challenges and opportunities. J Mater Chem 20:4567. doi: 10.1039/b926440j10.1039/b926440j ↗
51. Cheng G, Zhang Z, Chen S et al (2007) Inhibition of bacterial adhesion and biofilm formation on zwitterionic surfaces. Biomaterials 28:4192–4199. doi: 10.1016/j.biomaterials.2007.05.04110.1016/j.biomaterials.2007.05.041 ↗
52. Davies DG, Parsek MR, Pearson JP et al (1998) The involvement of cell-to-cell signals in the development of a bacterial biofilm. Science 280:295–298. doi: 10.1126/science.280.5361.29510.1126/science.280.5361.295 ↗
53. Miller MB, Bassler BL (2001) Quorum sensing in bacteria. Annu Rev Microbiol 55:165–199. doi: 10.1146/annurev.micro.55.1.16510.1146/annurev.micro.55.1.165 ↗
54. Kim JH, Choi DC, Yeon KM et al (2011) Enzyme-immobilized nanofiltration membrane to mitigate biofouling based on quorum quenching. Environ Sci Technol 45:1601–1607. doi: 10.1021/es103483j10.1021/es103483j ↗
55. Tang L, Eaton JW (1993) Fibrin(ogen) mediates acute inflammatory responses to biomaterials. J Exp Med 178:2147–2156. doi: 10.1084/jem.178.6.214710.1084/jem.178.6.2147 ↗
56. Wilson CJ, Clegg RE et al (2005) Mediation of biomaterial–cell interactions by adsorbed proteins: a review. Tissue Eng 11:1–1810.1089/ten.2005.11.1 ↗
57. Greelhood SJ, Horbett TA, Ward WK et al (2007) Passivating protein coatings for implantable glucose sensors: evaluation of protein retention. J Biomed Mater Res B Appl Biomater 83:340–344. doi: 10.1002/jbmb10.1002/jbmb ↗