In situ reactive hot press sintering and mechanical properties of Al2O3–TiB2–B4C composites
Source abstract
Abstract
Dense Al2O3–TiB2–B4C composites are synthesized by in situ reactive hot press sintering of B4C with 20 wt% TiAl2 and TiAl3 at 1700 °C, respectively. The sinterability of B4C is improved by the intermetallic compounds due to the formation of Al2O3 and TiB2. The sizes of Al2O3, TiB2, and B4C grains are less than 2.5 μm. The agglomerates of Al2O3 and TiB2 particles tend to orientationally align in the direction perpendicular to the pressure axis. By incorporation of TiAl2, the flexural strength and fracture toughness reach 482 MPa and 3.6 MPa m1/2, respectively. When TiAl3 is added, the flexural strength is reduced to 408 MPa because of the thermal residual stress, while the fracture toughness is increased to 4.2 MPa·m1/2. The increase of Al2O3 in the composite can reduce the strength and enhance the toughness of the composite due to the thermal residual stress originated from the thermal expansion mismatch between B4C and Al2O3.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Jollivet D (1996) Specific and genetic diversity at deep-sea hydrothermal vents: an overview. Biol Conserv 5(12):1619–1653
2. Lutz RZ, Kennish MJ (1993) Ecology of deep-sea hydrothermal vent communities: a review. Rev Geophys 31(3):211–24210.1029/93RG01280 ↗
3. Deng JX, Sun JL (2009) Microstructure and mechanical properties of hot-pressed B4C/TiC/Mo ceramic composites. Ceram Inter 35(2):771–77810.1016/j.ceramint.2008.02.014 ↗
4. Mondal S, Banthia AK (2005) Low-temperature synthetic route for boron carbide. J Eur Ceram Soc 25(2–3):287–29110.1016/j.jeurceramsoc.2004.08.011 ↗
5. Thévenot F (1990) Boron carbide—a comprehensive review. J Eur Ceram Soc 6(4):205–22510.1016/0955-2219(90)90048-K ↗
6. Pei LZ, Xiao HN (2009) B4C/TiB2 composite powders prepared by carbothermal reduction method. J Mater Proc Technol 209(4):2122–212710.1016/j.jmatprotec.2008.05.003 ↗
7. Deng JX, Sun JL (2008) Sand erosion performance of B4C based ceramic nozzles. Inter J Refract Met & Hard Mater 26(3):128–13410.1016/j.ijrmhm.2007.06.001 ↗
8. Sigl LS, Kleebe HJ (1995) Microcracking in B4C-TiB2 composites. J Am Ceram Soc 78(9):2374–238010.1111/j.1151-2916.1995.tb08671.x ↗
9. Dole SL, Prochazka S, Doremus RH (1989) Microstructural coarsening during sintering of boron carbide. J Am Ceram Soc 72(6):958–96610.1111/j.1151-2916.1989.tb06252.x ↗
10. Bougoin M, Thevenot F (1990) Pressureless sintering of boron carbide with an addition of polycarbosilane. J Mater Sci 22(1):109–114. doi: 10.1007/BF0116055810.1007/BF01160558 ↗
11. Levin L, Frage N, Dariel MP (2000) Novel approach for the preparation of B4C-based cermets. Inter J Refract Met Hard Mater 18(2–3):131–13510.1016/S0263-4368(00)00012-3 ↗
12. Goldstein A, Geffen Y, Goldenberg A (2001) Boron carbide-zirconium boride in situ composites by the reactive pressureless sintering of boron carbide zirconia mixtures. J Am Ceram Soc 84(3):642–64410.1111/j.1151-2916.2001.tb00714.x ↗
13. Sigl LS (1998) Processing and mechanical properties of boron carbide sintered with TiC. J Eur Ceram Soc 18(11):1521–152910.1016/S0955-2219(98)00071-5 ↗
14. Roy TK, Subramanian C, Suri AK (2006) Pressureless sintering of boron carbide. Cerami Inter 32(3):227–23310.1016/j.ceramint.2005.02.008 ↗
15. Yang YF, Wang HY, Liang YH, Zhao RY, Jiang QC (2007) Effect of nickel addition on the exothermic reaction of titanium and boron carbide. J Mater Res 22(1):169–17410.1557/jmr.2007.0010 ↗
16. Mashhadi M, Taheri-assaj E, Sglavo VM (2010) Pressureless sintering of boron carbide. Cerami Inter 36(1):151–15910.1016/j.ceramint.2009.07.034 ↗
17. Kang ES, Kim CH (1990) Improvements in mechanical properties of TiB2 by the dispersion of B4C particles. J Mater Sci 25(1):580–584. doi: 10.1007/BF0071407810.1007/BF00714078 ↗
18. Srivatsan TS, Guruprasad G, Black D, Petraroli M, Radhakrishnan R, Sudarshan TS (2006) Microstructural development and hardness of TiB2–B4C composite samples: influence of consolidation temperature. J Alloys Compd 413(1–2):63–7210.1016/j.jallcom.2005.04.209 ↗
19. Zhao H, Cheng YB (1999) Formation of TiB2-TiC composites by reactive sintering. Ceram Inter 25(4):353–35810.1016/S0272-8842(98)00048-0 ↗
20. Skorokhod V, Krstic VD (2000) High strength-high toughness B4C-TiB2 composites. J Mater Sci Lett 19(3):237–23910.1023/A:1006766910536 ↗
21. Yamada S, Hirao K, Yamauchi Y, Kanzaki S (2003) High strength B4C-TiB2 composites fabricated by reaction hot-pressing. J Eur Ceram Soc 23(7):1123–113010.1016/S0955-2219(02)00274-1 ↗
22. Lavrenko VA, Panasyuk AD, Firstov SA, Prima SB, Kochubei VO, Adeev VM (2003) Corrosion of titanium-aluminum intermetallides. II. Electrolytic oxidation of γ-TiAl, TiAl3, AND α2-Ti3Al in sea water. Powder Metall Met Ceram 42(5–6):291–29610.1023/A:1025727814582 ↗
23. Zhang WK, Gao LZ, Li J, Yang BJ, Yin YS (2011) TiAl/B4C marine material—fabrication, mechanical and corrosion properties. Ceram Inter 37(3):783–78910.1016/j.ceramint.2010.10.019 ↗
24. Kumazawa T, Honda T, Zhou Y, Miyazaki H, Hyuga H, Yoshizawa Y (2008) Pressureless sintering of boron carbide ceramics. J Ceram Soc Jap 116(12):1319–132110.2109/jcersj2.116.1319 ↗
25. Huang SG, Vanmeensel K, Malek OJA, Van der Biest O, Vleugels J (2011) Microstructure and mechanical properties of pulsed electric current sintered B4C–TiB2 composites. Mater Sci Eng A 528(3):1302–130910.1016/j.msea.2010.10.022 ↗
26. Huang SG, Vanmeensel K, Malek OJA, Van der Biest O, Vleugels J (2011) In situ synthesis and densification of submicrometer-grained B4C-TiB2 composites by pulsed electric current sintering. J Eur Ceram Soc 31(4):637–64410.1016/j.jeurceramsoc.2010.10.028 ↗
27. Ma ZY, Tjong SC (1997) In situ ceramic particle-reinforced aluminum matrix composites fabricated by reaction pressing in the TiO2 (Ti)-Al-B (B2O3) systems. Metall Mater Trans A 28(9):1931–194210.1007/s11661-997-0123-5 ↗
28. Chu MS, Wu SK (2003) The improvement of high temperature oxidation of Ti-50Al by sputtering Al film and subsequent interdiffusion treatment. Acta Mater 51(11):3109–312010.1016/S1359-6454(03)00123-X ↗
29. Braun J, Ellner M (2001) Phase equilibria investigations on the aluminum-rich part of the binary system Ti-Al. Metall Mater Trans A 32(5):1037–104710.1007/s11661-001-0114-x ↗
30. Levin L, Frage N, Dariel MP (1999) The effect of Ti and TiO2 additions on the pressureless sintering of B4C. Metall Mater Trans A 30(12):3201–321010.1007/s11661-999-0230-6 ↗
31. Mashhadi M, Taheri-Nassaj E, Sglavo VM, Sarpoolaky H, Ehsani N (2009) Effect of Al addition on pressureless sintering of B4C. Ceram Inter 35:831–83710.1016/j.ceramint.2008.03.003 ↗
32. Halverson DC (1989) Processing of boron carbide-aluminum composites. J Am Ceram Soc 72(5):775–78010.1111/j.1151-2916.1989.tb06216.x ↗
33. Zhang Z, Chen XG, Charette A (2009) Fluidity and microstructure of an Al–10% B4C composite. J Mater Sci 44:492–501. doi: 10.1007/s10853-008-3097-910.1007/s10853-008-3097-9 ↗
34. Kim HW, Koh YH, Kim HE (2000) Densification and mechanical properties of B4C with Al2O3 as a sintering aid. J Am Ceram Soc 83(11):2863–286510.1111/j.1151-2916.2000.tb01647.x ↗
35. Zhang WK, Gao LZ, Lei Y, Yang BJ, Li J, Xiao L et al (2010) TiAl/B4C composite fabricated by high energy ball milling and hot press sintering processes and its mechanical properties. Mater Sci Eng A 527:7436–744110.1016/j.msea.2010.08.041 ↗
36. Ye F, Hou ZP, Zhang HJ, Liu LM (2010) Densification and mechanical properties of spark plasma sintered with Si as a sintering aid. J Am Ceram Soc 93(10):2956–295910.1111/j.1551-2916.2010.03931.x ↗