journal article·2018-12

The response of yttrium aluminum garnet (YAG) grains and grain boundaries to nanoindentation

Wen Jiang, Xingwang Cheng, Hongnian Cai, Tayyeb Ali, Jian Zhang

Journal of Materials Science· Volume 53· Issue 24
Publisher page

Abstract

A systematic investigation on the mechanical response of the interior grain and grain boundary of yttrium aluminum garnet is carried out using nanoindentation and microstructure characterization. The nano-hardness is calculated, while the residual indent is analyzed in terms of surface profiles, plastic deformation and elastic recovery. The results show that the nano-hardness at the center of grain is higher than that in the grain boundary region. All indents display an anisotropic elastic recovery, mainly occurring in the loading direction. The grain boundary has a better plasticity than the center of grain, which is probably due to a weaker inter-atomic bonding force at the grain boundary rather than the formation of glassy phase at intergranular region. In addition, indentation size effect in the center of grain and at grain boundary region are determined by the analysis of nano-hardness using Meyer’s law. A weaker indentation size effect in the grain boundary region is observed due to a smaller elastic recovery.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Ahmad K, Pan W (2015) Microstructure-toughening relation in alumina based multiwall carbon nanotube ceramic composites. J Eur Ceram Soc 35:663–67110.1016/j.jeurceramsoc.2014.08.044 ↗
2. Yamamoto G, Hashida T, Omori M, Kimura H (2009) Preparation and microstructure of carbon nanotube-toughened alumina composites. J Solid Mech Mater Eng 3:85–9510.1299/jmmp.3.85 ↗
3. Becher PF (1986) Toughening behavior in ceramics associated with the transformation of tetragonal ZrO2. Acta Metall 34:1885–189110.1016/0001-6160(86)90246-4 ↗
4. Wang SF, Zhang J, Luo DW, Gu F, Tang DY, Dong ZL, Tan GE, Que WX et al (2013) Transparent ceramics: processing, materials and applications. Prog Solid State Chem 41:20–5410.1016/j.progsolidstchem.2012.12.002 ↗
5. Sokol M, Kalabukhov S, Shneck R, Zaretsky E, Frage N (2017) Effect of grain size on the static and dynamic mechanical properties of magnesium aluminate spinel (MgAl2O4). J Eur Ceram Soc 37:3417–342410.1016/j.jeurceramsoc.2017.04.025 ↗
6. Wang HM, Huang ZY, Jiang JS, Liu K, Duan MY, Lu ZW, Cedelle J, Guan ZW et al (2016) Unique mechanical properties of nano-grained YAG transparent ceramics compared with coarse-grained partners. Mater Des 105:9–1510.1016/j.matdes.2016.04.094 ↗
7. Kimberley J, Ramesh KT (2011) Dynamic response of transparent ceramic MgAl2O4 spinel. Scripta Mater 65:830–83310.1016/j.scriptamat.2011.07.044 ↗
8. Sokol M, Kalabukhov S, Dariel MP, Frage N (2014) High-pressure spark plasma sintering (SPS) of transparent polycrystalline magnesium aluminate spinel (PMAS). J Eur Ceram Soc 34:4305–431010.1016/j.jeurceramsoc.2014.07.022 ↗
9. Moshe Drezner H, Shilo D, Dorogoy A, Zolotoyabko E (2010) Nanometer-scale mapping of elastic modules in biogenic composites: the nacre of mollusk shells. Adv Funct Mater 20:2723–272810.1002/adfm.200902165 ↗
10. Raichman Y, Kazakevich M, Rabkin E, Tsur Y (2010) Inter-nanoparticle bonds in agglomerates studied by nanoindentation. Adv Mater 18:2028–203010.1002/adma.200600538 ↗
11. Xue F, Wang F, Huang P, Lu TJ, Xu KW (2015) Structural inhomogeneity and strain rate dependent indentation size effect in Zr-based metallic glass. Mater Sci Eng A 655:373–37810.1016/j.msea.2015.12.083 ↗
12. Dey A, Bhattacharya M, Mukhopadhyay AK (2015) Grain boundary nanohardness of coarse grain alumina. Int J Appl Ceram Technol 12:1199–120910.1111/ijac.12351 ↗
13. Ikesue A, Yan LA, Taira T, Kamimura T, Yoshida K, Messing GL (2006) Progress in ceramic lasers. Annu Rev Mater Res 17:397–42910.1146/annurev.matsci.36.011205.152926 ↗
14. Ikesue A, Furusato I, Kamata K (2010) Fabrication of polycrystalline, transparent YAG ceramics by a solid-state reaction method. J Am Ceram Soc 78:225–22810.1111/j.1151-2916.1995.tb08389.x ↗
15. Oliver CW, Pharr MG (1992) An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J Mater Res 7:1564–158310.1557/JMR.1992.1564 ↗
16. Rohrer GS (2011) Grain boundary energy anisotropy: a review. J Mater Sci 46:5881–5895. https://doi.org/10.1007/s10853-011-5677-310.1007/s10853-011-5677-3 ↗
17. Dao M, Lu L, Asaro RJ, Hosson JTMD, Ma E (2007) Toward a quantitative understanding of mechanical behavior of nanocrystalline metals. Acta Mater 55:4041–406510.1016/j.actamat.2007.01.038 ↗
18. Jiang B, Weng GJ (2004) A theory of compressive yield strength of nano-grained ceramics. Int J Plast 20:2007–202610.1016/j.ijplas.2003.10.010 ↗
19. Donnelly E, Baker SP (2006) Effects of surface roughness and maximum load on the mechanical properties of cancellous bone measured by nanoindentation. J Biomed Mater Res A 77:42610.1002/jbm.a.30633 ↗
20. Taljat B, Pharr GM (2004) Development of pile-up during spherical indentation of elastic-plastic solids. Int J Solids Struct 41:3891–390410.1016/j.ijsolstr.2004.02.033 ↗
21. Muller AM, Green DJ (2011) Elastic-plastic indentation response of two transparent fine-grained polycrystalline spinels. J Am Ceram Soc 94:3967–397510.1111/j.1551-2916.2011.04770.x ↗
22. Chaim R (2016) On densification mechanisms of ceramic particles during spark plasma sintering. Scr Mater 115:84–8610.1016/j.scriptamat.2016.01.010 ↗
23. Tabor D (1951) The hardness of metals. Oxford University Press, Oxford
24. Peng Z, Gong J, Miao H (2004) On the description of indentation size effect in hardness testing for ceramics: analysis of the nanoindentation data. J Eur Ceram Soc 24:2193–220110.1016/S0955-2219(03)00641-1 ↗
25. Patel PJ, Swab JJ, Staley M, Quinn GD (2006) Indentation size effect (ISE) of transparent AlON and MgAl2O4. ARL Report ARL-TR-3852
26. Haney EJ, Subhash G (2011) Rate sensitive indentation response of a coarse-grained magnesium aluminate spinel. J Am Ceram Soc 94:3960–396610.1111/j.1551-2916.2011.04756.x ↗
27. Chakraborty R, Dey A, Mukhopadhyay AK, Joshi KD, Rav A, Mandal AK, Bysakh S, Biswas SK et al (2012) Indentation size effect of alumina ceramic shocked at 12 GPa. Int J Refract Met Hard Mater 33:22–3210.1016/j.ijrmhm.2012.02.003 ↗
28. Bull SJ, Page TF, Yoffe EH (1989) An explanation of the indentation size effect in ceramics. Philos Mag Lett 59:281–28810.1080/09500838908206356 ↗